Research on Acid Separation by Diffusion Dialysis from Se-extracted Waste Liquor of Ni-Mo Ore Smelter Dust AITranslate
Abstract AITranslate
The mechanism was discussed of acid separation from Se-extracted waste liquor of Ni-Mo ore smelter dust with anion exchange membrane.Static diffusion dialysis tests were carried out,and the average diffusion velocity was investigated of H^+ and Na^+ with the selected 1^# or 3^# anion exchange membrane.Acid to salt separation coefficient of 1^# and 3^# anion exchange membrane was calculated,and then the type was determined of the anion exchange membrane suitable for acid separation from Se-extracted waste liquor.Meanwhile,the change law was studied of H^+concentration with time in diffusion chamber and dialysis chamber during diffusion dialysis.
KeyWords AITranslate
1王国青,焦怀金,高鹏杰.MBR技术在城市湖泊水华治理工程中的应用[J].水利规划与设计,2013(3):41-43. 被引量:2
2吴新祥,司海娟.顺丁橡胶装置溶剂油纤维液膜脱酸技术应用[J].石油化工设备,2013,42(2):90-92. 被引量:6
3KestingRS.SymthetiePolymericMembrane[M].北京:化学工业出版社,1992,2-13.
4罗爱平,张启修,石崇光,曾奇才.电渗析处理赤泥回水流程研究[J].中南工业大学学报,1997,28(5):440-443. 被引量:3
5罗爱平,张启修.改性金属膜膜萃取萃铜速度影响因素考察[J].中南工业大学学报,1998,29(5):442-445. 被引量:8
6龚柏凡,罗爱平,张启修.钨离子交换尾液电渗析脱盐研究[J].中南矿冶学院学报,1994,24(钨专辑):147-150.
7付丹,徐静.酸回收的扩散渗析技术及其发展现状[J].污染防治技术,2008,21(1):59-61. 被引量:19
8周国平,杨建男,罗士平.阴离子交换膜渗析法回收含硫酸钠的高浓度硫酸废水[J].膜科学与技术,2002,22(6):24-27. 被引量:7
1熊庆丰,范兴祥,余宇楠,刘琼,刘振楠,姚春玲.用氢氧化钠从银渣中浸出硒碲试验研究[J].湿法冶金,2017,36(4):281-284. 被引量:2
2王尔东.基于中和反渗透方法对云式除尘系统中主要杂质为硝酸根,硫酸根的酸性废水处理方法[J].科学技术创新,2022(28):167-170.
1谢刚,杨妮,田林.2017年云南冶金年评[J].云南冶金,2018,47(2):39-50. 被引量:1
2宋旭俊,施辉献.浮选渣中碲的浸出研究[J].有色金属设计,2022,49(2):18-22.
1卓晓军,侯晓川,杨润德,李贺.采用阴离子交换膜从镍钼矿冶炼烟尘提硒废液中分离酸的实验研究[J].矿冶工程,2016,0(6):61-63. 被引量:1
2含铜冶炼烟尘的处理方法[J].有色冶金设计与研究,1995,16(3):61-63.
3倪如宝,沈志伟.从废杂铜冶炼烟尘中简易回收铜的实践[J].江苏冶金,1997,25(6):71-71. 被引量:1
4侯晓川,高丛堦,肖连生,张启修,曾理,曹佐英.在H_2SO_4-HCl-H_2O复合体系中氧化浸出镍钼矿冶炼烟尘中的硒[J].中国有色金属学报,2011,21(5):1178-1185. 被引量:6
5欧阳岚.氯化法处理冶炼烟尘[J].有色冶炼,1994,23(3):30-34.
6王魁,张一敏,黄晶,刘涛,汪劲鹏.扩散渗析法应用于石煤提钒酸浸液预处理研究[J].有色金属:冶炼部分,2017(4):39-44.
7罗爱平,王晓春,刘军,张启修.离子交换膜扩散渗析分离碱钨的可行性研究[J].五邑大学学报:自然科学版,2000,14(2):29-32. 被引量:2
8张启修,张传福.离子交换膜分离技术在冶金中的应用[J].膜科学与技术,2001,21(2):37-43. 被引量:18
9侯晓川,肖连生,张启修,沈裕军,彭俊.从镍钼矿冶炼烟尘中浸出硒的体系选择[J].中南大学学报:自然科学版,2012,43(12):4626-4632. 被引量:1
10郑先君,周春山,吴鹏程,周建.从锌冶炼烟尘中回收银及有价金属的工艺研究[J].黄金,2000,21(11):40-44. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]
Citation Information:
The mechanism was discussed of acid separation from Se-extracted waste liquor of Ni-Mo ore smelter dust with anion exchange membrane.Static diffusion dialysis tests were carried out,and the average diffusion velocity was investigated of H^+ and Na^+ with the selected 1^# or 3^# anion exchange membrane.Acid to salt separation coefficient of 1^# and 3^# anion exchange membrane was calculated,and then the type was determined of the anion exchange membrane suitable for acid separation from Se-extracted waste liquor.Meanwhile,the change law was studied of H^+concentration with time in diffusion chamber and dialysis chamber during diffusion dialysis.
quote
| GB/T 7714-2015 | [1] HOU Xiao-chuan, YANG Run-de, LI He. Research on Acid Separation by Diffusion Dialysis from Se-extracted Waste Liquor of Ni-Mo Ore Smelter Dust[J]. Rare Metals and Cemented Carbides, 2014(3): 15-18. |
| MLA | [1] HOU Xiao-chuan, et al., "Research on Acid Separation by Diffusion Dialysis from Se-extracted Waste Liquor of Ni-Mo Ore Smelter Dust." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 15-18. |
| APA | [1] HOU Xiao-chuan, YANG Run-de, & LI He. (2014). Research on Acid Separation by Diffusion Dialysis from Se-extracted Waste Liquor of Ni-Mo Ore Smelter Dust. Rare Metals and Cemented Carbides(3), 15-18. |
| IEEE | [1] HOU Xiao-chuan, YANG Run-de, and LI He, "Research on Acid Separation by Diffusion Dialysis from Se-extracted Waste Liquor of Ni-Mo Ore Smelter Dust," Rare Metals and Cemented Carbides, no. 3, pp. 15-18, 2014. keywords: {acid separation;diffusion dialysis;ion exchange membrane;Se-extracted waste liquor;Ni-Mo ore smelter dust;H+ concentration} |