Research on Germanium Extraction from High-concentration H_2SO_4 Solution with HBL101 AITranslate

School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the disadvantages of existing germanium extractants,germanium extraction in high-concentration sulfuric acid medium with HBL101was tested.The effects of feed acidity,extractant concentration,time,phase ratio and temperature on the extraction and stripping of germanium were investigated.The extraction and stripping isotherms were plotted.The results show that with 15%(volume fraction)HBL101 and sulphonated kerosene as extractant,the extraction rate of germanium reaches 98.32% in four-stage counter current extraction with O/A ratio of 1∶1 under the optimum conditions.The germanium in loaded organic phase can be stripped using 150g/L NaOH solution and the stripping rate is above 98% in six-stage counter current stripping with O/A ratio of 8∶1.

KeyWords AITranslate

HBL101 germanium sulfuric acid system extraction stripping

1周娟,王吉坤,李勇.富锗硫化锌精矿浸出液萃取回收锗[J].有色金属:冶炼部分,2009(5):25-27. 被引量:13

2许凯,梁杰.几种锗萃取剂的合成原理及萃取性能的比较[J].湿法冶金,2011,30(2):87-90. 被引量:6

3王安亭,潘吉平.用仲辛醇萃取锗的研究[J].中国测试技术,2007,33(1):82-83. 被引量:8

4梁杰,黄琳,唐海龙.用TOA从硫酸体系中萃取Ge^(4+)的机理研究[J].贵州大学学报:自然科学版,2008,25(1):88-91. 被引量:6

5楚广,周兆安,杨天足,吴江华.G8315从湿法炼锌沉矾后液中萃取锗(Ⅳ)的性能研究[J].矿冶工程,2011,31(5):69-72. 被引量:6

6李旭光,梁铎强,覃峰,蒋继波.7815单液滴法萃取锗的动力学研究[J].有色金属:冶炼部分,2011(4):30-32. 被引量:3

7蒋应平,赵磊,王海北,蒋训雄.从高压浸出镓锗液中回收镓锗的试验研究[J].中国资源综合利用,2012,30(6):25-27. 被引量:10

8李世平,余坦,韦国龙,倪常凯.从含锗铟锌铜的硫酸溶液中分离回收有价金属[J].有色金属:冶炼部分,2012(12):36-38. 被引量:5

9林江顺,王海北,高颖剑,赵磊,张磊.一种新镓锗萃取剂的研制与应用[J].有色金属,2009,61(2):84-87. 被引量:11

10汤淑芳,周春山,蒋新宇.锗的氧肟酸HGS98萃取分离研究[J].稀有金属,2000,24(4):247-250. 被引量:12

1陈欢,刘志宏,刘付朋,李玉虎,刘智勇.用N235从低浓度硫酸溶液中萃取锗试验研究[J].湿法冶金,2017,36(5):391-396. 被引量:2

1王振杰,彭伟,刘安荣,刘洪波,钟波.用硫酸从湿法炼锌尾渣中浸出锗[J].湿法冶金,2021,40(4):294-297. 被引量:2

2马帅兵,刘付朋,陈飞雄.改性花生壳吸附分离湿法炼锌溶液中的镓和锗[J].有色金属科学与工程,2022,13(1):18-26. 被引量:1

1从硫酸溶液中萃取锑[J].有色金属技术经济研究,1991(5):36-36.

2李效军,雒佳莉,王凯,孙树娟,贾睿生.2,2'-硫代双对叔辛基苯酚萃取镍的性能[J].有色金属,2009,61(4):65-67.

3高照国,曹耀华,刘红召,王威.从含铟氧化锌烟尘中回收铟[J].有色金属:冶炼部分,2012(11):41-43. 被引量:16

4陈庆根.溶剂萃取法从石煤酸浸液中提取V_2O_5的新工艺研究[J].矿产综合利用,2010(1):19-22.

5肖华利.用氢氧化钠反萃锗的试验与应用[J].湖南冶金,1992(2):18-20.

6朱声逾,戴桂贞.硫脲反萃金的研究[J].贵金属,1989,10(4):51-53. 被引量:4

7车文婷,肖金娥.含铁锡P204有机相处理的研究[J].株冶科技,1994,22(4):23-28.

8黄志军.从锰电解液中去除高浓度锌的研究[J].中国锰业,1991,9(5):48-51. 被引量:1

9冯雪茹,吕国志,张延安,张莹,赵秋月,刘述平.P204萃取硫酸体系中V(Ⅳ)、Fe(Ⅲ)的分离性能研究[J].钢铁钒钛,2017,38(2):23-29. 被引量:13

10吴志华,张丽英.从少铕氯化稀土中提取氧化铈的研究[J].包头钢铁学院学报,1993,12(2):57-60. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF843[冶金工程—有色金属冶金]

Citation Information:

Based on the disadvantages of existing germanium extractants,germanium extraction in high-concentration sulfuric acid medium with HBL101was tested.The effects of feed acidity,extractant concentration,time,phase ratio and temperature on the extraction and stripping of germanium were investigated.The extraction and stripping isotherms were plotted.The results show that with 15%(volume fraction)HBL101 and sulphonated kerosene as extractant,the extraction rate of germanium reaches 98.32% in four-stage counter current extraction with O/A ratio of 1∶1 under the optimum conditions.The germanium in loaded organic phase can be stripped using 150g/L NaOH solution and the stripping rate is above 98% in six-stage counter current stripping with O/A ratio of 8∶1.

quote

GB/T 7714-2015 [1] ZHANG Kui-fang, CAO Zuo-ying, XIAO Lian-sheng, et al. Research on Germanium Extraction from High-concentration H_2SO_4 Solution with HBL101[J]. Rare Metals and Cemented Carbides, 2014(3): 7-11.
MLA [1] ZHANG Kui-fang, et al., "Research on Germanium Extraction from High-concentration H_2SO_4 Solution with HBL101." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 7-11.
APA [1] ZHANG Kui-fang, CAO Zuo-ying, XIAO Lian-sheng, CENG Li, ZHANG Gui-qing, & LI Qing-gang. (2014). Research on Germanium Extraction from High-concentration H_2SO_4 Solution with HBL101. Rare Metals and Cemented Carbides(3), 7-11.
IEEE [1] ZHANG Kui-fang, CAO Zuo-ying, XIAO Lian-sheng, CENG Li, ZHANG Gui-qing, and LI Qing-gang, "Research on Germanium Extraction from High-concentration H_2SO_4 Solution with HBL101," Rare Metals and Cemented Carbides, no. 3, pp. 7-11, 2014. keywords: {HBL101;germanium;sulfuric acid system;extraction;stripping}