Abstract AITranslate

We proposed a strategy to transform a cell shape from convex to concave via viscoelastic compression in order to reverse the Poisson’s ratio of biomass foam to be negative and improve its properties in compression and shockproof. The poly(butylene succinate) (PBS) foam with a negative Poisson’s ratio (NPR) was prepared; the Poisson’s ratio reached −0.7, and the compressive modulus increased by 359%. In the shockproof field, the storage and loss modulus could increase by ca. 270% and 350%, respectively. Such a method of viscoelastic compression can be universal for the reinforcement of biomass foam materials.

KeyWords AITranslate

negative Poisson’s ratio metamaterials biomass polymers mechanical properties shockproof
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01232

Chinese Library Classification Number:

Citation Information:

We proposed a strategy to transform a cell shape from convex to concave via viscoelastic compression in order to reverse the Poisson’s ratio of biomass foam to be negative and improve its properties in compression and shockproof. The poly(butylene succinate) (PBS) foam with a negative Poisson’s ratio (NPR) was prepared; the Poisson’s ratio reached −0.7, and the compressive modulus increased by 359%. In the shockproof field, the storage and loss modulus could increase by ca. 270% and 350%, respectively. Such a method of viscoelastic compression can be universal for the reinforcement of biomass foam materials.

quote

GB/T 7714-2015 [1] Yi He, Dong Li, Na Zhou, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01232.
MLA [1] Yi He, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01232.
APA [1] Yi He, Dong Li, Na Zhou, Lin Gan, & Jin Huang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01232
IEEE [1] Yi He, Dong Li, Na Zhou, Lin Gan, and Jin Huang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01232. keywords: {negative Poisson’s ratio;metamaterials;biomass polymers;mechanical properties;shockproof}