Abstract AITranslate

Luminescent hydrogels are of immense importance for various applications; however, they often are severely damaged during long-term storage and transportation, which have been the major barriers impeding their further application in the industrial realm. On the other hand, the emerging self-healable materials also suffer from a high dependence on freshness or require external substance assistance or energy imput. We herein for the first time report spontaneously self-regenerative luminescent hydrogels prepared via copolymerization of an acrylamide–lanthanide complex in the presence of a sodium alginate skeleton. The hydrogel–powder–hydrogel regeneration cycles can be repeated for multiple rounds with both mechanical and luminescence properties restored, even long after being ground into powder. This work highlights a simple strategy that can effectively address the long-term storage and transportation obstacles and thus pushes forward the further practical application of luminescent hydrogels in various fields.

KeyWords AITranslate

regeneration lanthanide luminescence hydrogel longterm storage and transportation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01289

Chinese Library Classification Number:

Citation Information:

Luminescent hydrogels are of immense importance for various applications; however, they often are severely damaged during long-term storage and transportation, which have been the major barriers impeding their further application in the industrial realm. On the other hand, the emerging self-healable materials also suffer from a high dependence on freshness or require external substance assistance or energy imput. We herein for the first time report spontaneously self-regenerative luminescent hydrogels prepared via copolymerization of an acrylamide–lanthanide complex in the presence of a sodium alginate skeleton. The hydrogel–powder–hydrogel regeneration cycles can be repeated for multiple rounds with both mechanical and luminescence properties restored, even long after being ground into powder. This work highlights a simple strategy that can effectively address the long-term storage and transportation obstacles and thus pushes forward the further practical application of luminescent hydrogels in various fields.

quote

GB/T 7714-2015 [1] Tiyun Zhu, Ruyu Liu, Bo Peng, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01289.
MLA [1] Tiyun Zhu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01289.
APA [1] Tiyun Zhu, Ruyu Liu, Bo Peng, Kongyi Zhu, Xiao Liu, Bin Li, Zhiqiang Li, & Huanrong Li. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01289
IEEE [1] Tiyun Zhu, Ruyu Liu, Bo Peng, Kongyi Zhu, Xiao Liu, Bin Li, Zhiqiang Li, and Huanrong Li, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01289. keywords: {regeneration;lanthanide;luminescence;hydrogel;longterm storage and transportation}