Postmodification of Polymer Networks via the Freezing-Induced Generation of Radicals AITranslate

Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report polymer reactions triggered by freezing, in which pink radicals with yellow fluorescence, generated by the cleavage of the mechanophore tetraarylsuccinonitrile (TASN), act not only as reactive species but also as indicators of radical generation. The driving force of this reaction is the mechanical stress that TASN moieties in the cross-linkers of the polymer network experience due to solvent freezing; this stress leads to the homolytic cleavage of the TASN moieties to form carbon-centered radicals that react with the vinyl monomers. Electron paramagnetic resonance measurements revealed that the amount of radicals remains constant, providing a consistent reaction field.

KeyWords AITranslate

polymer mechanochemistry mechanochromism dynamic covalent chemistry gels monomer insertion Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01195

Chinese Library Classification Number:

Citation Information:

We report polymer reactions triggered by freezing, in which pink radicals with yellow fluorescence, generated by the cleavage of the mechanophore tetraarylsuccinonitrile (TASN), act not only as reactive species but also as indicators of radical generation. The driving force of this reaction is the mechanical stress that TASN moieties in the cross-linkers of the polymer network experience due to solvent freezing; this stress leads to the homolytic cleavage of the TASN moieties to form carbon-centered radicals that react with the vinyl monomers. Electron paramagnetic resonance measurements revealed that the amount of radicals remains constant, providing a consistent reaction field.

quote

GB/T 7714-2015 [1] Sota Kato, Daisuke Aoki, Hideyuki Otsuka. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01195.
MLA [1] Sota Kato, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01195.
APA [1] Sota Kato, Daisuke Aoki, & Hideyuki Otsuka. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01195
IEEE [1] Sota Kato, Daisuke Aoki, and Hideyuki Otsuka, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01195. keywords: {polymer mechanochemistry;mechanochromism;dynamic covalent chemistry;gels;monomer insertion;Show More}