Cholate Conjugated Polymeric Amphiphiles as Efficient Artificial Ionophores AITranslate
Abstract AITranslate
A family of amphiphilic copolymers containing hydrophobic cholate pendants has been prepared by copolymerization of cholic acid-based monomer 2-(methacryloxy)-ethyl cholate (MAECA) with polyethylene glycol methyl ether methacrylate (PEGMA). The polymers differ for the content of MAECA that increases from 0 to 35%. The copolymers partition within liposomes and display potent ionophoric activity forming large pores in the membrane and allowing the leakage of small inorganic ions (H+, Na+) and of large polar organic molecules (calcein). Their activity is strictly correlated to the content of cholic acid subunits, increasing as the fraction of cholate moiety increases.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01182
Chinese Library Classification Number:
Citation Information:
A family of amphiphilic copolymers containing hydrophobic cholate pendants has been prepared by copolymerization of cholic acid-based monomer 2-(methacryloxy)-ethyl cholate (MAECA) with polyethylene glycol methyl ether methacrylate (PEGMA). The polymers differ for the content of MAECA that increases from 0 to 35%. The copolymers partition within liposomes and display potent ionophoric activity forming large pores in the membrane and allowing the leakage of small inorganic ions (H+, Na+) and of large polar organic molecules (calcein). Their activity is strictly correlated to the content of cholic acid subunits, increasing as the fraction of cholate moiety increases.
quote
| GB/T 7714-2015 | [1] Subhasish Sahoo, Jawad ur Rehman, Muhammad Raza Shah, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01182. |
| MLA | [1] Subhasish Sahoo, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01182. |
| APA | [1] Subhasish Sahoo, Jawad ur Rehman, Muhammad Raza Shah, Priyadarsi De, & Paolo Tecilla. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01182 |