Abstract AITranslate

The common problems of EDM equipment in cemented carbides are discussed and the factors in- fluencing processing quality and efficiency of the equipment are presented,and the constructive advices are proposed for future improvement and development of the equipment.

KeyWords AITranslate

cemented carbide EDM digital controlling equipment selection application

1胡黄卿.电火花加工硬质合金模具的研究[J].稀有金属与硬质合金,2000,28(1):9-14. 被引量:4

2杨连文,何云,周锦进.硬质合金的电火花加工特性研究[J].电加工,1993(3):2-7. 被引量:2

1吴海会,王彤,王俊棋,尹洪石.基于Cr12MoV模具钢水雾中电火花线切割工艺研究[J].硬质合金,2017,34(2):120-128.

2吴海会,王彤,王俊棋,尹洪石.超声水雾中电火花线切割精加工特性研究[J].硬质合金,2017,34(3):179-185. 被引量:1

1王彤,张通,吴吉荣,吴林波,马永会,刘盼.基于PNN神经网络电火花线切割中厚度工件放电状态研究[J].硬质合金,2018,35(5):351-357. 被引量:1

1薛永栋,韩静涛.锻造成形有限元模拟的关键技术及实例分析[J].冶金设备,2007(5):28-31. 被引量:2

2金铭.谈机械制造技术电火花加工设备[J].中国科技纵横,2012(19):220-220.

3田甜,张诗昌.Deform在锻造中的应用[J].冶金设备,2009(5):67-70. 被引量:11

4徐英男.我国发电设备用钢材概述[J].特殊钢,1994,15(3):3-5.

5孙一波,刘祎峰.电火花加工设备脉冲电源故障诊断与检修方法[J].设备管理与维修,2009(3):21-23.

6李心平.快走丝线切割机床加工质量分析及工艺参数选择研究[J].中国机械,2014,0(11):57-57. 被引量:1

7陈德志.浅谈提高快走丝线切割机床加工精度的主要途径[J].金属加工:冷加工,2009(14):59-60.

8许达哲,王国庆,陈济轮.五轴联动数控电火花加工装备集成技术[J].航天制造技术,2012(1):1-3.

9窦振荣,高淑英,孙立新.电火花表面热处理实验研究[J].河北工业大学学报,1997,26(2):105-108.

10姚顺东.关于机械加工过程中对数控机床的改进和发展趋势的探讨[J].科技创新与应用,2012,2(06Z):69-69.

Basic Information:

DOI:

Chinese Library Classification Number:TG661[金属学及工艺—金属切削加工及机床]

Citation Information:

The common problems of EDM equipment in cemented carbides are discussed and the factors in- fluencing processing quality and efficiency of the equipment are presented,and the constructive advices are proposed for future improvement and development of the equipment.

quote

GB/T 7714-2015 [1] TANG Hui. Selection and Application of EDM Equipment in Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2013(6): 58-62.
MLA [1] TANG Hui. "Selection and Application of EDM Equipment in Cemented Carbides." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 58-62.
APA [1] TANG Hui. (2013). Selection and Application of EDM Equipment in Cemented Carbides. Rare Metals and Cemented Carbides(6), 58-62.
IEEE [1] TANG Hui, "Selection and Application of EDM Equipment in Cemented Carbides," Rare Metals and Cemented Carbides, no. 6, pp. 58-62, 2013. keywords: {cemented carbide;EDM;digital controlling;equipment selection;application}