Causes and Solution for Deformation of Low-pressure Sintered Cemented Carbide Products AITranslate
Abstract AITranslate
Based on introduction for working principle of pressure-sintering furnace, factors are summarized causing deformation of low-pressure sintered cemented carbide products, with systematic analysis combined with actual production cases. The results show that the main factor is furnace leakage, resulting in gas entry into the furnace. O2 in the gas influences the carbon balance of the products,and then causes their de- formation.
KeyWords AITranslate
1吴翔,谭千榆.真空烧结产品变形机理及其控制[J].四川有色金属,2012(3):38-39. 被引量:1
2陈跃辉,郭淳,罗毅.ZYS-50/50/130压力烧结炉设备的研制[J].稀有金属与硬质合金,2008,36(1):42-45. 被引量:5
1万军新,刘诗彪.硬质合金烧结变形及控制方法[J].福建冶金,2023,52(3):41-43.
2仇伟.大直径硬质合金圆盘切刀烧结坯的变形控制[J].中国钨业,2023,38(1):58-64.
1杨晓东.回转窑结圈的原因及处理方法[J].烧结球团,1998,23(2):44-45. 被引量:4
2杨晓东.回转窑结圈的危害,原因及处理方法[J].承钢技术,1998(2):5-6.
3卢仁伟,李笃信,赵志刚,李益民.铜粉末注射成形工艺[J].粉末冶金材料科学与工程,2006,11(2):104-108. 被引量:7
4杨志敏,甘燕玲.浅谈带式输送机常见故障[J].南方金属,2005(3):53-55.
5曲选辉,李志林,李益民,黄伯云.钨基重合金注射成形产品变形原因及其控制[J].中南工业大学学报,1999,30(1):49-51. 被引量:6
6刘亚平.试论电解槽破损原因及处理方法[J].有色冶金节能,2000(2):24-27.
7王士平,杨传芳.霉雨季节铁基粉末冶金制品质量的控制[J].粉末冶金工业,2012,22(5):33-36. 被引量:1
8吴国雄.铁的直接还原度γd碳平衡计算法公式的分析和修正[J].包钢科技,1999(3):72-74. 被引量:2
9刘方舟,曹万里,吴翔,史顺亮.涂料对硬质合金烧结变形的影响[J].稀有金属与硬质合金,2015,43(1):68-72. 被引量:3
10何嵩,覃德勇.宝钢1号高炉炉墙结厚的处理[J].中国冶金,2012,22(4):35-39. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF806.1[冶金工程—有色金属冶金]
Citation Information:
Based on introduction for working principle of pressure-sintering furnace, factors are summarized causing deformation of low-pressure sintered cemented carbide products, with systematic analysis combined with actual production cases. The results show that the main factor is furnace leakage, resulting in gas entry into the furnace. O2 in the gas influences the carbon balance of the products,and then causes their de- formation.
quote
| GB/T 7714-2015 | [1] YANG Jin-kun, YANG Fa-wei. Causes and Solution for Deformation of Low-pressure Sintered Cemented Carbide Products[J]. Rare Metals and Cemented Carbides, 2013(6): 55-57. |
| MLA | [1] YANG Jin-kun, and YANG Fa-wei. "Causes and Solution for Deformation of Low-pressure Sintered Cemented Carbide Products." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 55-57. |
| APA | [1] YANG Jin-kun, & YANG Fa-wei. (2013). Causes and Solution for Deformation of Low-pressure Sintered Cemented Carbide Products. Rare Metals and Cemented Carbides(6), 55-57. |
| IEEE | [1] YANG Jin-kun and YANG Fa-wei, "Causes and Solution for Deformation of Low-pressure Sintered Cemented Carbide Products," Rare Metals and Cemented Carbides, no. 6, pp. 55-57, 2013. keywords: {cemented carbide;low-pressure sintering;product deformation;leakage analysis} |