daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Calculation and Analysis of Macroscopic Residual Stress in Polycrystalline Diamond Compacts with Finite Element Method AITranslate

Department of Materials Science and Engineering, Chongqing Jiaotong University;Department of Materials Science and Engineering, Chongqing Jiaotong University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Macroscopic residual stress distribution in polycrystalline diamond compacts was calculated with finite element method. The results show that both radial residual stress and axial residual stress are tensile stress in the polycrystalline diamond layer along cylindrical edge of the compact,and therefore the edge of the compact is easily broken off in the form of large pieces during operation. Decreasing the thickness of polyerystalline diamond layer can effectively reduce its tensile stress at the edge.

KeyWords AITranslate

polycrystalline diamond compact cemented carbide residual stress finite element method

1A.D. Krawitz,R. Andrew Winholtz,E.F. Drake,N.D. Griffin.Residual stresses in polycrystalline diamond compacts[J].International Journal of Refractory Metals and Hard Materials.1999(1)

2Tomlinsin, P.N.,Pipkin, N.J.,Lammer, A.,Burnand, R.P.HIGH PERFORMANCE DRILLING - SYNDAX 3 SHOWS VERSATILITY[].Industrial Diamond Review.1985

3Sneddon, M.V.,Hall, D.R.Polycrystalline diamond: Manufacture, wear mechanisms, and implications for bit design[].JPT Journal of Petroleum Technology.1988

4Lin, Tze-Pin,Hood, Michael,Cooper, George A.,Smith, Redd H.Residual stresses in polycrystalline diamond compacts[].Journal of the American Ceramic Society.1994

5Lin, Tze-Pin,Cooper, George A,Hood, Michael.Fatigue test on polycrystalline diamond compacts[].Journal of Materials Science.1993

1牛凯强,刘备,宋双路,平志峰.基于有限元的多孔结构金刚石圆锯片模态分析[J].机械工程与自动化,2022(3):73-74. 被引量:3

1孙坤鹏,李吉成.基于DEM-FEA的圆盘开沟机刀盘的力学特性分析[J].机电产品开发与创新,2023,36(1):68-70. 被引量:1

2周好斌,唐帅,刘泽强.基于医学实验的多自由度可调节人体复合训练设备研究[J].机电工程技术,2023,52(1):102-106.

3陈杰,卢玉斌,侯玉波.基于ABAQUS的圆锯片切削竹筒仿真试验研究[J].林产工业,2023,60(3):38-43. 被引量:1

1张秀林,宋德玉.宏观残余应力与金属构件疲劳强度的关系[J].冶金设备,2000(5):54-55. 被引量:2

2孙方遒.宏观残余应力X射线测定[J].煤炭技术,2012,31(12):11-12. 被引量:1

3高玉周,史雅琴,林国强,严立.(Ti,Zr)N复合薄膜的微观结构及性能[J].大连海事大学学报,2002,28(2):81-84. 被引量:8

4罗治平,宋德玉,杨玉荣,张少卿.GH169合金孔内表面层的挤压强化对孔边疲劳性能的影响[J].材料工程,1994,22(8):24-25. 被引量:1

5朱平,刘萍,张力宁.宏观残余应力对微塑性变形行为的影响[J].东南大学学报:自然科学版,1991,21(1):25-27.

6窦剑琳,贾惠玲.短应力线轧机轧辊的有限元计算及分析[J].包钢科技,2008,34(3):39-41. 被引量:1

7贾强,刘艳,张志昌.SAF2205双相不锈钢焊接工艺及耐蚀性的研究[J].科技信息,2013(23):23-24. 被引量:3

8芦亚萍,马振宇,贾权仕,顾荣荣.振动时效机理研究[J].机械科学与技术,2001,20(4):587-589. 被引量:29

9刘燕燕,张庆瑜,林国强.电弧离子镀制备(TiCr)N薄膜的微观结构及性能[J].真空科学与技术,2002,22(4):299-302. 被引量:17

10宋小放,周志明,王祥,范红山,张宝亮.强流脉冲电子束表面改性1.2344钢的显微组织和性能[J].表面技术,2014,43(6):75-78. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

Macroscopic residual stress distribution in polycrystalline diamond compacts was calculated with finite element method. The results show that both radial residual stress and axial residual stress are tensile stress in the polycrystalline diamond layer along cylindrical edge of the compact,and therefore the edge of the compact is easily broken off in the form of large pieces during operation. Decreasing the thickness of polyerystalline diamond layer can effectively reduce its tensile stress at the edge.

quote

GB/T 7714-2015 [1] LI Li, ZHOU Chao. Calculation and Analysis of Macroscopic Residual Stress in Polycrystalline Diamond Compacts with Finite Element Method[J]. Rare Metals and Cemented Carbides, 2013(6): 63-66.
MLA [1] LI Li, and ZHOU Chao. "Calculation and Analysis of Macroscopic Residual Stress in Polycrystalline Diamond Compacts with Finite Element Method." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 63-66.
APA [1] LI Li, & ZHOU Chao. (2013). Calculation and Analysis of Macroscopic Residual Stress in Polycrystalline Diamond Compacts with Finite Element Method. Rare Metals and Cemented Carbides(6), 63-66.
IEEE [1] LI Li and ZHOU Chao, "Calculation and Analysis of Macroscopic Residual Stress in Polycrystalline Diamond Compacts with Finite Element Method," Rare Metals and Cemented Carbides, no. 6, pp. 63-66, 2013. keywords: {polycrystalline diamond compact;cemented carbide;residual stress;finite element method}