Modeling and simulation of percussive impact for robotic riveting system AITranslate

Shanghai University; Shanghai University; Ryerson University; Shanghai University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Riveting is one of the major joining methods used in assembly, and the robotic riveting has been gradually introduced into aircraft industry. In this paper, a method is presented for modeling and simulation of percussive robotic riveting. In percussive riveting, vibration always exists. When an impact force is employed, a forced vibration will be induced. If it resonates with a robot natural frequency, the vibration will cause damage to the robot. The main content of this paper is divided into three parts. Firstly, a robot dynamic model is established to compute the driving torque for each joint. Secondly, vibration responses under impact are analyzed for the percussive riveting process. Thirdly, the effect of riveting on robot vibration is studied over the robot workspace. The purpose of this paper is to discuss the suitable regions for riveting where the robot vibration is very minimal. It is shown that based on the presented method an appropriate trajectory can be planned for robotic riveting.

KeyWords AITranslate

Robotic dynamics Analysis Vibration response Impact force Riveting
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-014-0091-0

Chinese Library Classification Number:

Citation Information:

Riveting is one of the major joining methods used in assembly, and the robotic riveting has been gradually introduced into aircraft industry. In this paper, a method is presented for modeling and simulation of percussive robotic riveting. In percussive riveting, vibration always exists. When an impact force is employed, a forced vibration will be induced. If it resonates with a robot natural frequency, the vibration will cause damage to the robot. The main content of this paper is divided into three parts. Firstly, a robot dynamic model is established to compute the driving torque for each joint. Secondly, vibration responses under impact are analyzed for the percussive riveting process. Thirdly, the effect of riveting on robot vibration is studied over the robot workspace. The purpose of this paper is to discuss the suitable regions for riveting where the robot vibration is very minimal. It is shown that based on the presented method an appropriate trajectory can be planned for robotic riveting.

quote

GB/T 7714-2015 [1] Shuai Guo, SongLiang Nie, FengFeng Xi, et al. Advances in Manufacturing, 2014(2). DOI:10.1007/s40436-014-0091-0.
MLA [1] Shuai Guo, et al., Advances in Manufacturing, no. 2, 2014, https://doi.org/10.1007/s40436-014-0091-0.
APA [1] Shuai Guo, SongLiang Nie, FengFeng Xi, & Tao Song. (2014). Advances in Manufacturing(2). https://doi.org/10.1007/s40436-014-0091-0
IEEE [1] Shuai Guo, SongLiang Nie, FengFeng Xi, and Tao Song, Advances in Manufacturing, no. 2, 2014, doi: 10.1007/s40436-014-0091-0. keywords: {Robotic dynamics;Analysis;Vibration response;Impact force;Riveting}