Grinding with cubic boron nitride (CBN) superabrasive is a widely used method of machining superalloy in aerospace industries. However, there are some issues, such as poor grinding quality and severe tool wear, in grinding of powder metallurgy superalloy FGH96. In addition, abrasive wheel wear is the significant factor that hinders the further application of CBN abrasive wheels. In this case, the experiment of grinding FGH96 with single CBN abrasive grain using different parameters was carried out. The wear characteristics of CBN abrasive grain were analyzed by experiment and simulation. The material removal behavior affected by CBN abrasive wear was also studied by discussing the pile-up ratio during grinding process. It shows that morphological characteristics of CBN abrasive grain and grinding infeed direction affect the CBN abrasive wear seriously by simulation analysis. Attrition wear, micro break, and macro fracture had an important impact on material removal characteristics. Besides, compared with the single cutting edge, higher pile-up ratio was obtained by multiple cutting edges, which reduced the removal efficiency of the material. Therefore, weakening multiple cutting edge grinding on abrasive grains in the industrial production, such as applying suitable dressing strategy, is an available method to improve the grinding quality and efficiency.
Show more
During assembly process, the miniature part needs to be fixed in its assembly position. In some occasions where adhesive is used, the joining force is not established due to the adhesive curing process, in that case the locking of parts is required. Manual locking is difficult to meet the increasing demand for mass production. To solve this problem and realize fully automatic assembly, a novel gripper module was designed and corresponding locking method was proposed. Thanks to the functional integration, the gripper module is capable of manipulating and locking the part. This module is integrated into the assembly system and plays a crucial role in automatic assembly. The locking method for automatic assembly is based on the integration of the part picking up and the locking unit releasing. After being placed accurately at its desired position, the miniature part can be automatically locked by releasing the locking unit. The innovative structure and mechanism of the gripper module convert the spring force into the locking force of the miniature part, ensuring non-rigid locking and suitable small locking force. Locking principle, flexibility and limitations of the proposed method were clarified in detail. Moreover, an effective compensation strategy was used to achieve accurate and stable pickup of the part, which increased the reliability of the assembly process. During automatic locking, the disturbances to the part due to the eccentric load were analyzed. The effectiveness of the gripper module and proposed method was verified by experiment. Experimental results indicated that the modular system integrated with the gripper module could meet the requirements of fully automatic assembly. Manual locking is replaced by automatic locking, and workers are liberated from tedious manual operations. The improvement of automation level enables assembly equipment to be applied to mass production scenarios.
Show more
Abrasive waterjet (AWJ) is widely applied in 2D machining as it offers high machining efficiency and low machining cost. However, machining a 3D surface, especially for a small curvature radius freeform surface (SCRFS), results in over-erosion of the corner, and has been one of the greatest issues of AWJ. To solve this problem, a local smoothing algorithm for SCRFS is developed by the junction of two linear segments at the corner by inserting cubic second-order B-spline to smooth the nozzle path and posture under the setting tolerance error, which is aimed to avoid over-erosion due to the change in dwell time. Analytical solutions of the smooth corner position and orientation of the nozzle path are obtained by evaluating a synchronization algorithm. According to the set tolerance error of the nozzle position and orientation, the interpolation of the smooth path of the corner meets the constraint conditions of the linear feed drive. Path simulation and experimental results show that the proposed method is validated by the experimental results and has been applied to the integral blisk machining of an aero-engine.
Show more
Robotic GMAW forming process with the advantages of high productivity and high bond strength has become an important forming remanufacturing technology. In this paper, our recent research achievements are introduced and our development prospect on robotic GMAW forming remanufacturing is declared.
Cited: 16
Show more
The reliability and real time of industrial wireless sensor networks (IWSNs) are the absolute requirements for industrial systems, which are two foremost obstacles for the large-scale applications of IWSNs. This paper studies the multi-objective node placement problem to guarantee the reliability and real time of IWSNs from the perspective of systems. A novel multi-objective node deployment model is proposed in which the reliability, real time, costs and scalability of IWSNs are addressed. Considering that the optimal node placement is an NP-hard problem, a new multi-objective binary differential evolution harmony search (MOBDEHS) is developed to tackle it, which is inspired by the mechanism of harmony search and differential evolution. Three large-scale node deployment problems are generated as the benCHmarks to verify the proposed model and algorithm. The experimental results demonstrate that the developed model is valid and can be used to design large-scale IWSNs with guaranteed reliability and real-time performance efficiently. Moreover, the comparison results indicate that the proposed MOBDEHS is an effective tool for multi-objective node placement problems and superior to Pareto-based binary differential evolution algorithms, nondominated sorting genetic algorithm II (NSGA-II) and modified NSGA-II.
Cited: 9
Show more
In inventory financing, asymmetric information between banks and the third party logistics enterprises may incur moral risks, often causing economic losses of banks. To effectively solve this problem, a pure incentive scheme and a regulatory incentive scheme are designed with the principal-agent theory. By comparison, it is found that the pure incentive model is not applicable to practical conditions, and regulatory incentive model can not only solve practical problems substantially but also outbalance pure incentive model under certain conditions. The research results from example analysis given in this paper offer theoretical instruction and a practical method for effective regulation of banks.
Cited: 5
Show more
In order to study the hot melt extrusion process in fused deposition modeling (FDM), this study mainly explores the effects of printing temperature, heated block length, feeding speed on the exit morphology and mechanical properties of FDM printed Polylactic acid (PLA) samples. High-speed camera is used to capture the exit morphology of molten PLA just extruded to the nozzle. According to exit morphology, the outlet states of extruded molten material can be divided into four categories, namely, bubbled state, coherent state, expanding state, and unstable state. Tensile test results show that printing temperature, heated block length and printing speed have significant influence on tensile properties and fracture mode of FDM printed samples. When the heated block length is 15 mm and 30 mm, there is a ductile-brittle transition in fracture mode with the increase of printing speed. The printing process window under different heated block lengths and printing temperatures has been figured out and the distribution of printing process window under different printing speeds has been discussed. There is a maximum printing process window under the heated block length of 30 mm. This finding provides a frame work for performance prediction of FDM printed parts and theoretical guidance for expanding the scope of printing process window.
Download: 0
Show more
Duplex stainless steels are being used on applications that require, especially, high corrosion resistance and overall good mechanical properties, such as the naval and oil-gas exploration industry. The components employed in these industries are usually obtained by machining, however, these alloys have low machinability when compared to conventional stainless steels. In this work, a study of the wear developed when milling duplex stainless-steel, LDX 2101, is going to be presented and evaluated, employing four types of milling tools with different geometries and coatings, while studying the influence of feed rate and cutting length in the wear of these tools. Tools used have been provided with two and four flutes, as well as three different coatings, namely: TiAlN, TiAlSiN and AlCrN. The cutting behavior of these tools was analyzed; data relative to the cutting forces developed during the process were obtained; and roughness measurements of the machined surfaces were executed. The tools were then submitted to scanning electron microscope (SEM) analysis, enabling the identification of the wear mechanisms that tools were subjected to when machining this material, furthermore, the early stages of these mechanisms were also identified. All this work was done with the goal of relating the machining parameters and cutting force values obtained, identifying, and discussing the wear patterns that were observed in the coating and tools after the milling tests, providing further information on the machining of these alloys.
Download: 0
Show more
Keyhole tungsten inert gas (K-TIG) welding is capable of realizing single-sided welding and double-sided forming and has been widely used in medium and thick plate welding. In order to improve the accuracy of automatic weld identification and weld penetration prediction of robot in the process of large workpiece welding, a two-stage model is proposed in this paper, which can monitor the K-TIG welding penetration state in real time on the embedded system, called segmentation-LSTM model. The proposed system extracts 9 weld pool geometric features with segmentation network, and then extracts the weld gap using a traditional algorithm. Then these 10-dimensional features are input into the LSTM model to predict the penetration state, including under penetration, partial penetration, good penetration and over penetration. The recognition accuracy of the proposed system can reach 95.2%. In this system, to solve the difficulty of labeling data and lack of segmentation accuracy, an improved LabelMe capable of live-wire annotation tool and a novel loss function were proposed, respectively. The latter was also called focal dice loss, which enabled the network to achieve a performance of 0.933 mIoU on the testing set. Finally, an improved slimming strategy compresses the network, making the segmentation network achieve real-time on the embedded system (RK3399pro).
Download: 0
Show more