daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Quantum-Cutting Ytterbium-Doped CsPb(Cl1–xBrx)3 Perovskite Thin Films with Photoluminescence Quantum Yields over 190% AITranslate

University of Washington; University of Washington; University of Washington; University of Washington; University of Washington
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A two-step solution-deposition method for preparing ytterbium-doped (Yb3+) CsPb(Cl1–xBrx)3 perovskite thin films is described. Yb3+-doped CsPb(Cl1–xBrx)3 films are made that exhibit intense near-infrared photoluminescence with extremely high quantum yields reaching over 190%, stemming from efficient quantum cutting that generates two emitted near-infrared photons for each absorbed visible photon. The near-infrared Yb3+f–f photoluminescence is largely independent of the anion content (x) in CsPb(Cl1–xBrx)3 films with energy gaps above the quantum-cutting threshold of twice the Yb3+f–f transition energy, but it decreases abruptly when the perovskite energy gap becomes too small to generate two Yb3+ excitations. Excitation power dependence measurements show facile saturation of the Yb3+ luminescence intensity, identifying a major challenge for future solar applications of these materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01528

Chinese Library Classification Number:

Citation Information:

A two-step solution-deposition method for preparing ytterbium-doped (Yb3+) CsPb(Cl1–xBrx)3 perovskite thin films is described. Yb3+-doped CsPb(Cl1–xBrx)3 films are made that exhibit intense near-infrared photoluminescence with extremely high quantum yields reaching over 190%, stemming from efficient quantum cutting that generates two emitted near-infrared photons for each absorbed visible photon. The near-infrared Yb3+f–f photoluminescence is largely independent of the anion content (x) in CsPb(Cl1–xBrx)3 films with energy gaps above the quantum-cutting threshold of twice the Yb3+f–f transition energy, but it decreases abruptly when the perovskite energy gap becomes too small to generate two Yb3+ excitations. Excitation power dependence measurements show facile saturation of the Yb3+ luminescence intensity, identifying a major challenge for future solar applications of these materials.

quote

GB/T 7714-2015 [1] Daniel M. Kroupa, Joo Yeon Roh, Tyler J. Milstein, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01528.
MLA [1] Daniel M. Kroupa, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01528.