daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Confined Pyrolysis within a Nanochannel to Form a Highly Efficient Single Iron Site Catalyst for Zn–Air Batteries AITranslate

University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Structural engineering of atomic-scaled metal/N–C catalysts is crucial yet challenging in enhancing their performance for the oxygen reduction reaction (ORR). Herein, we demonstrate exclusive single iron sites in periodic mesoporous nitrogen-doped carbon through an efficient template-directed pyrolysis strategy. The channel in SBA-15 was introduced to give a large specific area and uniform mesopore, providing abundant exposed active sites for the ORR. As a result, the optimal single-atom Fe catalyst exhibits a more positive onset potential (1.03 V vs RHE) and half-wave potential (0.902 V vs RHE) than those of a commercial Pt/C catalyst in an alkaline medium. For the single-atom Fe catalyst after 20000 s, 93.6% of the current at 0.8 V vs RHE can be retained, demonstrating its good stability. Additionally, when utilized to assemble the air electrode of a primary zinc–air battery, the obtained Fe single-atoms catalyst provides high voltage and durability, indicating its practical applicability.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01508

Chinese Library Classification Number:

Citation Information:

Structural engineering of atomic-scaled metal/N–C catalysts is crucial yet challenging in enhancing their performance for the oxygen reduction reaction (ORR). Herein, we demonstrate exclusive single iron sites in periodic mesoporous nitrogen-doped carbon through an efficient template-directed pyrolysis strategy. The channel in SBA-15 was introduced to give a large specific area and uniform mesopore, providing abundant exposed active sites for the ORR. As a result, the optimal single-atom Fe catalyst exhibits a more positive onset potential (1.03 V vs RHE) and half-wave potential (0.902 V vs RHE) than those of a commercial Pt/C catalyst in an alkaline medium. For the single-atom Fe catalyst after 20000 s, 93.6% of the current at 0.8 V vs RHE can be retained, demonstrating its good stability. Additionally, when utilized to assemble the air electrode of a primary zinc–air battery, the obtained Fe single-atoms catalyst provides high voltage and durability, indicating its practical applicability.

quote

GB/T 7714-2015 [1] Zheng Kun Yang, ChengZong Yuan, AnWu Xu. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01508.
MLA [1] Zheng Kun Yang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01508.
APA [1] Zheng Kun Yang, ChengZong Yuan, & AnWu Xu. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01508
IEEE [1] Zheng Kun Yang, ChengZong Yuan, and AnWu Xu, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01508.