Unexpectedly Slow Yet Efficient Picosecond to Nanosecond Photoinduced Hole-Transfer Occurs in a Polymer/Nonfullerene Acceptor Organic Photovoltaic Blend AITranslate

University of Washington; University of Washington; University of Washington; City University of Hong Kong; University of Washington
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We study photoinduced charge generation in a model polymer/nonfullerene acceptor (NFA) organic photovoltaic (OPV) blend. Specifically, we focus on hole-transfer kinetics from the photoexcited NFA thiophene-thieno[3,2-b]thiophene-thiophene-3-(dicyanomethylidene)indan-1-one (4TIC) to the conjugated polymer donor poly[(4,4′-bis(2-butyloctoxycarbonyl-[2,2′-bithiophene]-5,5-diyl)-alt-(2,2′-bithiophene-5,5′-diyl)] (PDCBT) using ultrafast transient absorption spectroscopy by selectively exciting the 4TIC electron acceptor and monitoring the bleach of the PDCBT ground-state population. In the blend, the 4TIC excitons decay with an average lifetime of 7 ps, accompanied by a concomitant rise in the ground-state bleach of the polymer with a comparable average lifetime that is 60% complete by 8 ps and 95% complete by 100 ps, occurring roughly an order of magnitude slower than that in most previously reported polymer/NFA blends. Notably, the ground-state bleach of the polymer continues to grow, not reaching its maximum until ∼1 ns. To explain this slow ground-state bleach rise, we propose that some 4TIC charge-transfer-like excitons are generated, which undergo hole transfer to the polymer on the 100 ps–1 ns time scale. Our findings provide new insight into the kinetics of hole transfer in nonfullerene OPV blends in the regime of small driving force and also support the proposal that nonfullerene acceptors may generate long-lived charge species upon direct photoexcitation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01416

Chinese Library Classification Number:

Citation Information:

We study photoinduced charge generation in a model polymer/nonfullerene acceptor (NFA) organic photovoltaic (OPV) blend. Specifically, we focus on hole-transfer kinetics from the photoexcited NFA thiophene-thieno[3,2-b]thiophene-thiophene-3-(dicyanomethylidene)indan-1-one (4TIC) to the conjugated polymer donor poly[(4,4′-bis(2-butyloctoxycarbonyl-[2,2′-bithiophene]-5,5-diyl)-alt-(2,2′-bithiophene-5,5′-diyl)] (PDCBT) using ultrafast transient absorption spectroscopy by selectively exciting the 4TIC electron acceptor and monitoring the bleach of the PDCBT ground-state population. In the blend, the 4TIC excitons decay with an average lifetime of 7 ps, accompanied by a concomitant rise in the ground-state bleach of the polymer with a comparable average lifetime that is 60% complete by 8 ps and 95% complete by 100 ps, occurring roughly an order of magnitude slower than that in most previously reported polymer/NFA blends. Notably, the ground-state bleach of the polymer continues to grow, not reaching its maximum until ∼1 ns. To explain this slow ground-state bleach rise, we propose that some 4TIC charge-transfer-like excitons are generated, which undergo hole transfer to the polymer on the 100 ps–1 ns time scale. Our findings provide new insight into the kinetics of hole transfer in nonfullerene OPV blends in the regime of small driving force and also support the proposal that nonfullerene acceptors may generate long-lived charge species upon direct photoexcitation.

quote

GB/T 7714-2015 [1] Yun Liu, Lijian Zuo, Xueliang Shi, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01416.
MLA [1] Yun Liu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01416.
APA [1] Yun Liu, Lijian Zuo, Xueliang Shi, Alex K.Y. Jen, & David S. Ginger. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01416
IEEE [1] Yun Liu, Lijian Zuo, Xueliang Shi, Alex K.Y. Jen, and David S. Ginger, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01416.