daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Performance Alkaline Organic Redox Flow Batteries Based on 2-Hydroxy-3-carboxy-1,4-naphthoquinone AITranslate

Nanjing University; Nanjing University; Nanjing University; Nanjing University; Nanjing University; Nanjing University; Nanjing University; Nanjing University; Nanjing University; Texas Tech University; Duke University; Nanjing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Aqueous redox flow batteries (ARFBs) based on the electrolyte solutions of redox-active organic molecules are very attractive for the application of large-scale electrochemical energy storage. We propose a high-performance ARFB system utilizing 2-hydroxy-3-carboxy-1,4-naphthoquinone (2,3-HCNQ) and K4Fe(CN)6 as the anolyte and catholyte active species, respectively. The 2,3-HCNQ molecule exhibits high solubility and can carry out a reversible two-electron redox process with rapid redox kinetics. The assembled 2,3-HCNQ/K4Fe(CN)6 ARFB delivered a cell voltage of 1.02 V and realized a peak power density of 0.255 W cm–2. The 2,3-HCNQ/K4Fe(CN)6 ARFB can be stably operated at a current density of 100 mA cm–2 for long-term cycling (with a capacity retention of ∼94.7% after 100 cycles).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01296

Chinese Library Classification Number:

Citation Information:

Aqueous redox flow batteries (ARFBs) based on the electrolyte solutions of redox-active organic molecules are very attractive for the application of large-scale electrochemical energy storage. We propose a high-performance ARFB system utilizing 2-hydroxy-3-carboxy-1,4-naphthoquinone (2,3-HCNQ) and K4Fe(CN)6 as the anolyte and catholyte active species, respectively. The 2,3-HCNQ molecule exhibits high solubility and can carry out a reversible two-electron redox process with rapid redox kinetics. The assembled 2,3-HCNQ/K4Fe(CN)6 ARFB delivered a cell voltage of 1.02 V and realized a peak power density of 0.255 W cm–2. The 2,3-HCNQ/K4Fe(CN)6 ARFB can be stably operated at a current density of 100 mA cm–2 for long-term cycling (with a capacity retention of ∼94.7% after 100 cycles).

quote

GB/T 7714-2015 [1] Caixing Wang, Zhen Yang, Yanrong Wang, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01296.
MLA [1] Caixing Wang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01296.
APA [1] Caixing Wang, Zhen Yang, Yanrong Wang, Peiyang Zhao, Wen Yan, Guoyin Zhu, Lianbo Ma, Bo Yu, Lei Wang, Guigen Li, Jie Liu, & Zhong Jin. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01296
IEEE [1] Caixing Wang, Zhen Yang, Yanrong Wang, Peiyang Zhao, Wen Yan, Guoyin Zhu, Lianbo Ma, Bo Yu, Lei Wang, Guigen Li, Jie Liu, and Zhong Jin, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01296.