Derivatives of 2-Pyridone Exhibiting Hot-Exciton TADF for Sky-Blue and White OLEDs Derivatives of 2-Pyridone Exhibiting Hot-Exciton TADF for Sky-Blue and White OLEDs AITranslate

Lviv Polytechnic National University;Lviv Polytechnic National University;Lviv Polytechnic National University;Lviv Polytechnic National University; Kaunas University of Technology; Kaunas University of Technology;Lviv Polytechnic National University; Bohdan Khmelnytsky National University; Kaunas University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Development of emissive materials for utilization in organic light-emitting diodes (OLEDs) remains a highly relevant research field. One of the most important aspects in the development of efficient emitters for OLEDs is the efficiency of triplet-to-singlet exciton conversion. There are many concepts proposed for the transformation of triplet excitons to singlet excitons, among which thermally activated delayed fluorescence (TADF) is the most efficient and widespread. One of the variations of the TADF concept is the hot exciton approach according to which the process of exciton relaxation into the lowest energy electronic state (internal conversion as usual) is slower than intersystem crossing between high-lying singlets and triplets. In this paper, we present the donor–acceptor materials based on 2-pyridone acceptor coupled to the different donor moieties through the phenyl linker demonstrating good performance as components of sky-blue, green-yellow, and white OLEDs. Despite relatively low photoluminescence quantum yields, the compound containing 9,9-dimethyl-9,10-dihydroacridine donor demonstrated very good efficiency in sky-blue OLED with the single emissive layer, which showed an external quantum efficiency (EQE) of 3.7%. It also forms a green-yellow-emitting exciplex with 4,4′,4″-tris[phenyl(m-tolyl)amino]triphenylamine. The corresponding OLED showed an EQE of 6.9%. The white OLED combining both exciplex and single emitter layers demonstrated an EQE of 9.8% together with excellent current and power efficiencies of 16.1 cd A–1 and 6.9 lm W–1, respectively. Quantum-chemical calculations together with the analysis of photoluminescence decay curves confirm the ability of all of the studied compounds to exhibit TADF through the hot exciton pathway, but the limiting factor reducing the efficiency of OLEDs is the low photoluminescence quantum yields caused mainly by nonradiative intersystem crossing dominating over the radiative fluorescence pathway.

KeyWords AITranslate

pyridone hot exciton delayed fluorescence exciplex OLED
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00443

Chinese Library Classification Number:

Citation Information:

Development of emissive materials for utilization in organic light-emitting diodes (OLEDs) remains a highly relevant research field. One of the most important aspects in the development of efficient emitters for OLEDs is the efficiency of triplet-to-singlet exciton conversion. There are many concepts proposed for the transformation of triplet excitons to singlet excitons, among which thermally activated delayed fluorescence (TADF) is the most efficient and widespread. One of the variations of the TADF concept is the hot exciton approach according to which the process of exciton relaxation into the lowest energy electronic state (internal conversion as usual) is slower than intersystem crossing between high-lying singlets and triplets. In this paper, we present the donor–acceptor materials based on 2-pyridone acceptor coupled to the different donor moieties through the phenyl linker demonstrating good performance as components of sky-blue, green-yellow, and white OLEDs. Despite relatively low photoluminescence quantum yields, the compound containing 9,9-dimethyl-9,10-dihydroacridine donor demonstrated very good efficiency in sky-blue OLED with the single emissive layer, which showed an external quantum efficiency (EQE) of 3.7%. It also forms a green-yellow-emitting exciplex with 4,4′,4″-tris[phenyl(m-tolyl)amino]triphenylamine. The corresponding OLED showed an EQE of 6.9%. The white OLED combining both exciplex and single emitter layers demonstrated an EQE of 9.8% together with excellent current and power efficiencies of 16.1 cd A–1 and 6.9 lm W–1, respectively. Quantum-chemical calculations together with the analysis of photoluminescence decay curves confirm the ability of all of the studied compounds to exhibit TADF through the hot exciton pathway, but the limiting factor reducing the efficiency of OLEDs is the low photoluminescence quantum yields caused mainly by nonradiative intersystem crossing dominating over the radiative fluorescence pathway.

quote

GB/T 7714-2015 [1] Iryna Danyliv, Khrystyna Ivaniuk, Yan Danyliv, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00443.
MLA [1] Iryna Danyliv, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00443.
APA [1] Iryna Danyliv, Khrystyna Ivaniuk, Yan Danyliv, Igor Helzhynskyy, Viktorija Andruleviciene, Dmytro Volyniuk, Pavlo Stakhira, Glib V. Baryshnikov, & Juozas V. Grazulevicius. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00443
IEEE [1] Iryna Danyliv, Khrystyna Ivaniuk, Yan Danyliv, Igor Helzhynskyy, Viktorija Andruleviciene, Dmytro Volyniuk, Pavlo Stakhira, Glib V. Baryshnikov, and Juozas V. Grazulevicius, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00443. keywords: {pyridone hot exciton delayed fluorescence exciplex OLED}