Preparation of LiFePO_4 Anode Materials for Lithium-ion Battery AITranslate
Abstract AITranslate
Test is made on olivine LiFePO_4 anode material for lithium-ion battery.LiFePO_4 and carbon-doped LiFePO_4 were prepared by solid-phase synthesization. Test results showed that carbon-doped LiFePO_4 had good electrochemical performance.Discharging at 0.1 C rate,the initial discharge capacity was 130 mA·h/g with little capacity decrease after 10 circles at room temperature.
KeyWords AITranslate
1汪继强.第二十届国际原电池和蓄电池会议评述[J].电源技术,2003,27(3):322-328. 被引量:8
2Cho Jaephil,et al.Effect of preparation methods of LiNi1-xCoxO2 cathode material on their chemical structure and electrode performance[J].J Electrchem Soc,1999,146 (10):3 571.
3Thackeray M M,et al.Structural characterization of the lithium ion oxides LixFe3O4 and LixFe2O3 (0<x<2)[J].Mat Res Bull,1982,17(6):785.
4Thackeray M M,et al.High-temperature lithiation of α-Fe2O3:a mechanistic study[J].J Solid State Chem,1984,55(3):280.
5Pernet M,et al.Structural and electrochemical study of lithium insertion into γ-Fe2O3[J].Solid State Ionics,1993,66(3):259.
6Yoji Sakurai,et al.Low temperature synthesis and electrochemical characteristics of LiFeO2 cathodes[J].J Power Sources, 1997,68(2):711.
7Padhi A K,et al.Phospho-olivines as positive-electrode materials for rechargeable lithium batteries[J].J Electrchem Soc,1997,144(4):1 188.
8Padhi A K,et al.Effect of structure on the Fe3+/Fe2+ redox couple in iron phosphates[J].J Electrchem Soc,1997,144(5):1 609.
9Yamada A,et al.Optimized LiFePO4 for lithium battery cathodes[J].J Electrchem Soc,2001,148(3):A224.
1于逢婕,杨斌,易惠华,胡成林.锂离子电池正极材料LiFePO_4的研究进展[J].云南化工,2008,35(4):45-49. 被引量:3
1龚国辉,钟辉,赵磊.锂离子电池正极材料LiFePO_4制备工艺研究进展[J].广州化工,2011,39(18):24-26. 被引量:2
2马晓玲,吴田,王梦.纳米尺寸锂离子电池正极材料LiFePO_4/C合成与电性能研究[J].湖北第二师范学院学报,2012,29(2):12-14.
3马晓玲,吴田,淳莉.介孔α-Fe_2O_3的制备及电化学性能研究[J].华中师范大学学报:自然科学版,2012,46(3):318-321.
1熊学,戴永年,陈海清,李碧平.包覆碳对LiFePO_4正极材料性能的影响[J].湖南有色金属,2009,25(1):29-32. 被引量:3
2庞明,甘学锋.掺杂Nd对LiCoO2_的结构和电化学性能的影响[J].安徽化工,2005,31(3):43-44. 被引量:7
3徐庆柏,戴槐生,郭德稳,王山林,张敬沏,刘庆德,张奕麟.霍山橄榄石的性质及其在铸造涂料中的应用[J].安徽工学院学报,1990,9(1):8-14.
4李学良,费新坤.锂离子电池正极材料LiMn_(1.95)Cr_(0.05)O_4的电化学性能[J].稀有金属快报,2005,24(4):24-26. 被引量:1
5黄丽娜,王优,罗四海,何小芳,曹新鑫,孙得翔.纳米金属氧化物制备新进展[J].热加工工艺,2015,44(12):23-26. 被引量:5
6崔舜.热处理对贮氢合金电化学性能的影响[J].稀有金属,1999,23(3):201-204. 被引量:7
7刘杨,吴锋.用BP网络预测AB_5型储氢合金初始放电容量[J].功能材料,2004,35(2):174-176. 被引量:1
8董丽荣,宋健,李长生,唐华,于万秋,华中.Ag/SmBa_2Cu_3O_(7--δ)金属陶瓷的摩擦特性[J].硅酸盐学报,2014,42(12):1543-1547. 被引量:2
9施玲玲,徐用军,李康,姚忠平,姜兆华.Mg-Li合金微弧氧化陶瓷膜的制备及其耐蚀性能[J].材料研究学报,2009,0(2):220-224. 被引量:2
10刘洁群,钟胜奎,伍凌,万康,吕凡.不同方法合成的LiVPO_4F/C的电化学性能(英文)[J].中国有色金属学会会刊:英文版,2012,22(S1):157-161.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.263[金属学及工艺—金属材料]
Citation Information:
Test is made on olivine LiFePO_4 anode material for lithium-ion battery.LiFePO_4 and carbon-doped LiFePO_4 were prepared by solid-phase synthesization. Test results showed that carbon-doped LiFePO_4 had good electrochemical performance.Discharging at 0.1 C rate,the initial discharge capacity was 130 mA·h/g with little capacity decrease after 10 circles at room temperature.
quote
| GB/T 7714-2015 | [1] QU Tao, TIAN Yan-wen, DING Yang, et al. Preparation of LiFePO_4 Anode Materials for Lithium-ion Battery[J]. Rare Metals and Cemented Carbides, 2004(4): 14-16. |
| MLA | [1] QU Tao, et al., "Preparation of LiFePO_4 Anode Materials for Lithium-ion Battery." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 14-16. |
| APA | [1] QU Tao, TIAN Yan-wen, DING Yang, & DI Yu-chun. (2004). Preparation of LiFePO_4 Anode Materials for Lithium-ion Battery. Rare Metals and Cemented Carbides(4), 14-16. |
| IEEE | [1] QU Tao, TIAN Yan-wen, DING Yang, and DI Yu-chun, "Preparation of LiFePO_4 Anode Materials for Lithium-ion Battery," Rare Metals and Cemented Carbides, no. 4, pp. 14-16, 2004. keywords: {Lithium-ion battery;anode material;LiFePO_4;carbon-doped LiFePO_4;solid-phase synthesization} |