Effect of Heat Treatment on High-temperature Wearing Character of WC/Steel Composite Material AITranslate

School of Materials Science and Engineering, Anhui University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study and analysis is made of the transformation of the microstructure and the hardness of WC/steel composite material under different heat-treatment conditions.And effect of the heat-treatment temperature on high-temperature wearing character is also investigated.The results showed WC/steel composites material has good high-temperature wearing character when quenching at 1 050 ℃ and tempering at 480 ℃ and 640 ℃.

KeyWords AITranslate

WC/steel composite material heat treatment high-temperature wearing character

1株州硬质合金厂.钢结硬质合金[M].北京:冶金工业出版社,1982..

2李沐山.国外钢结硬质合金新进展[J].硬质合金,1994,11(2):105-114. 被引量:50

3高彩桥.金属的摩擦磨损与热处理[M].北京:机械工业出版社,1988..

4游兴河.WC系钢结硬质合金在烧结和热处理过程中相成分及组织结构的变化[J].金属热处理学报,1984,5(2):35-35.

1田四光,尤显卿,钟成山,黄曼平,马建国.金属基复合材料热磨损性能的研究现状[J].五金科技,2007,35(5):18-23.

1陈其伟.高温磨损试验参数对WC/钢复合材料高温磨损特性的影响[J].稀有金属与硬质合金,2005,33(1):22-25. 被引量:1

2马建国,叶劲,尤显卿,刘宝.离心铸造WC/钢复合材料显微组织[J].材料热处理学报,2009,30(6):130-134. 被引量:1

3陈九磅,刘少光,束德林,郭新成.5CrMnMo钢膏剂硼铝共渗层的高温磨损特性[J].金属热处理,2001,26(2):8-10. 被引量:5

4尤显卿.热处理条件对WC/钢复合材料热疲劳性能的影响[J].兵器材料科学与工程,2004,27(6):23-26. 被引量:3

5任祥,陈其伟.采用WC/钢复合材料作导卫辊的应用研究[J].稀有金属与硬质合金,2005,33(4):4-7. 被引量:1

6陈九磅,束德林,刘少光,郭新成.5CrMnMo钢渗硼层的高温磨损特性[J].热处理,2000,15(3):32-35. 被引量:3

7黄曼平,尤显卿,张成军,马建国.电冶熔铸WC/钢复合材料表面激光重熔工艺[J].金属热处理,2008,33(9):19-24. 被引量:1

8尤显卿,马建国,宋雪峰,任昊,黄曼平.电冶熔铸WC/钢复合材料中WC的溶解行为[J].中国有色金属学报,2005,15(9):1363-1368. 被引量:17

9尤显卿,任昊,郑玉春,斯廷智.电渣熔铸WC/钢复合材料的磨损性能研究[J].特种铸造及有色合金,2003(6):19-21. 被引量:9

10尤显卿,王基才,郑玉春,黄漫平,袁根福.铸造WC/钢复合材料的锻造研究[J].热加工工艺,2002,31(6):40-42. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG166.9[金属学及工艺—热处理]

Citation Information:

Study and analysis is made of the transformation of the microstructure and the hardness of WC/steel composite material under different heat-treatment conditions.And effect of the heat-treatment temperature on high-temperature wearing character is also investigated.The results showed WC/steel composites material has good high-temperature wearing character when quenching at 1 050 ℃ and tempering at 480 ℃ and 640 ℃.

quote

GB/T 7714-2015 [1] CHEN Qi-wei. Effect of Heat Treatment on High-temperature Wearing Character of WC/Steel Composite Material[J]. Rare Metals and Cemented Carbides, 2004(4): 10-13.
MLA [1] CHEN Qi-wei. "Effect of Heat Treatment on High-temperature Wearing Character of WC/Steel Composite Material." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 10-13.
APA [1] CHEN Qi-wei. (2004). Effect of Heat Treatment on High-temperature Wearing Character of WC/Steel Composite Material. Rare Metals and Cemented Carbides(4), 10-13.
IEEE [1] CHEN Qi-wei, "Effect of Heat Treatment on High-temperature Wearing Character of WC/Steel Composite Material," Rare Metals and Cemented Carbides, no. 4, pp. 10-13, 2004. keywords: {WC/steel composite material;heat treatment;high-temperature wearing;character}