daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of ATO(Antimony- doped Tin Oxide) Nanometer Powder with Ultrasonic Hydrolysis AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

ATO nanometer powder was prepared respectively by ultrasonic hydrolysis and conventional electromagnetic agitation hydrolysis.The powder was tested with XRD,SEM,TEM and the resistivity of powder was measured.Comparison is made between the aggregation factor of the nanometer powders prepared by the said two methods and the mechanism of agglomerate phenomena was discussed.The results showed that ultrasonic can inhibit the aggregation of ATO nanometer powder prepared by alkoxide hydrolysis,whose resistivity is slightly higher than that prepared by conventional electromagnetic agitation hydrolysis.

KeyWords AITranslate

ultrasonic hydrolysis of alkoxide ATO nanometer powder aggregation-resistance

1陈少贞,陈森凤.湿化学法制备ZrO_2超细粉的团聚机理、表征及控制[J].材料导报,1996,10(3):39-45. 被引量:17

2张宗涛,胡黎明.无团聚Al_2O_3-ZrO_2复合纳米粉末的制备及机理[J].华东理工大学学报:自然科学版,1996,22(4):439-444. 被引量:11

3Youshaw R A,et al.Compction of spray-dried powders[J].American Ceramic Society Bulletin,1982,62(2):227.

4Marsumoto R L K.Analysis of powder compaction using a compaction rate diagram[J].Journal of the American Ceramic Society,1990,73(2):465.

5李树棠.晶体X射线衍射学基础[M].北京:冶金工业出版社,1994.171.

6黄培云.粉末冶金原理[M].北京:冶金工业出版社,1981..

7王剑华,郭玉忠.超细粉制备方法及其团聚问题[J].昆明理工大学学报:理工版,1997,22(1):71-77. 被引量:30

8李青山,张金朝,宋鹂.共沉淀条件对纳米级Sb/SnO_2粒度和电性能的影响[J].应用化学,2002,19(2):163-167. 被引量:27

1曹瑞军,林晨光,孙兰,赵诣林,刘总,贾成厂.超细粉末的团聚及其消除方法[J].粉末冶金技术,2006,24(6):460-466. 被引量:21

2李宁,孟庆林.建筑玻璃涂膜技术研究进展[J].玻璃与搪瓷,2008,36(4):36-38.

3许爱忠,张荣华.液相法制备锑掺杂二氧化锡(ATO)材料研究进展[J].化工新型材料,2009,37(9):8-10. 被引量:2

1陈杰,林晨光,胡学晟,贾成厂,曹瑞军.超细WC粉末中团聚体的强度[J].粉末冶金工业,2008,18(5):25-29. 被引量:6

2梁滔,魏绪玲,丛日新,郑红兵.粉末橡胶的开发与研究进展 Ⅱ.研究及应用[J].合成橡胶工业,2009,32(6):527-531.

3韦相忠,岳丽,秦松梅,劳深,冯军,陆秋凡,李耀华.HPLC测定广西莪术不同炮制品超微细粉中牻牛儿酮的含量[J].中国实验方剂学杂志,2010,16(12):45-47. 被引量:2

4尹大鹏,朱协彬,汪海涛.ATO粉体的制备工艺及其导电性能的研究[J].安徽工程大学学报,2011,26(2):51-54. 被引量:1

5周玉成,魏世忠,王利敏,徐流杰.自生氧化铝颗粒增强铁基复合材料的制备[J].热加工工艺,2011,40(22):100-102. 被引量:1

6左勇刚,张利波,刘秉国,彭金辉,李健,马爱元.响应曲面法优化微波干燥白炭黑研究[J].材料导报,2013,27(12):91-94. 被引量:4

7刘亚虎,蔡雪原,朱延超,张琳娇,杨建红.纳米碳化硅颗粒的团聚及分散的研究进展[J].材料工程,2013(9):84-90. 被引量:8

8许第发,周玲玲,罗寄希,曹盈,张世英.过氧改性纳米TiO_2溶胶光催化降解苯酚的研究[J].工业水处理,2014,34(2):22-25. 被引量:5

9程进.钼粉颗粒团聚现象及量化方法[J].中国钼业,2016,40(6):50-53. 被引量:5

10孟凡凯,尹少武,张沛,刘传平,王立.高速气流冲击下微细颗粒的输送特性[J].过程工程学报,2017,17(2):231-236. 被引量:1

1戴健,温廷琏,吕之奕.醇盐水解法制备的纳米级稳定氧化锆细粉[J].无机材料学报,1993,8(1):51-56. 被引量:11

2段学臣,张多默,赵天从.超微锑白(Sb_2O_3)的研究[J].中南矿冶学院学报,1990,21(5):485-491. 被引量:11

3段学臣,黄蔚庄,赵天从.高纯超细锑白的研制[J].矿冶工程,1998,18(2):61-63. 被引量:2

4王晶,张文波.晶种加入对水热合成α-Al_2O_3粉体性能影响[J].轻金属,2008(5):19-21.

5李历历,段学臣.第二组元掺杂对ATO纳米粉体电学和光学性能的影响[J].功能材料,2004(z1):2795-2799.

6段学臣,杨向萍,吴湘伟.金属醇盐水解法制备超细粉末过程中醇与苯的回收[J].稀有金属与硬质合金,2001,29(2):41-43. 被引量:1

7张琳,朱广军,罗军,王恒志.醇盐水解法制备纳米级Sb_2O_3粒子[J].化学世界,2003,44(12):619-621. 被引量:1

8赖复兴,李启厚,黄凯,郭学益,艾侃.CdS/AlOOH纳米粉末组装行为的研究(I):载体γ-AIOOH纳米颗粒的制备[J].湿法冶金,2003,22(4):195-199. 被引量:3

9陈振华,严红革,段学臣.超微粉末的研究[J].功能材料,2000,31(1):36-37. 被引量:5

10张多默,刘志宏,陈慧光,葛荣德,张传福,段学臣,姚珍刚,赵天从.特种粉体材料的研制[J].中南矿冶学院学报,1994,25(4):540-542. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]

Citation Information:

ATO nanometer powder was prepared respectively by ultrasonic hydrolysis and conventional electromagnetic agitation hydrolysis.The powder was tested with XRD,SEM,TEM and the resistivity of powder was measured.Comparison is made between the aggregation factor of the nanometer powders prepared by the said two methods and the mechanism of agglomerate phenomena was discussed.The results showed that ultrasonic can inhibit the aggregation of ATO nanometer powder prepared by alkoxide hydrolysis,whose resistivity is slightly higher than that prepared by conventional electromagnetic agitation hydrolysis.

quote

GB/T 7714-2015 [1] LI Li-li, DUAN Xue-chen. Preparation of ATO(Antimony- doped Tin Oxide) Nanometer Powder with Ultrasonic Hydrolysis[J]. Rare Metals and Cemented Carbides, 2004(4): 17-20.
MLA [1] LI Li-li, and DUAN Xue-chen. "Preparation of ATO(Antimony- doped Tin Oxide) Nanometer Powder with Ultrasonic Hydrolysis." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 17-20.
APA [1] LI Li-li, & DUAN Xue-chen. (2004). Preparation of ATO(Antimony- doped Tin Oxide) Nanometer Powder with Ultrasonic Hydrolysis. Rare Metals and Cemented Carbides(4), 17-20.
IEEE [1] LI Li-li and DUAN Xue-chen, "Preparation of ATO(Antimony- doped Tin Oxide) Nanometer Powder with Ultrasonic Hydrolysis," Rare Metals and Cemented Carbides, no. 4, pp. 17-20, 2004. keywords: {ultrasonic;hydrolysis of alkoxide;ATO nanometer powder;aggregation-resistance}