Morphology Study of TiC Ceramic Particles Generated In-situ by Laser Cladding AITranslate
Abstract AITranslate
Based on Materials Studio software,a simulation analysis of the growth mechanism of TiC cera-mic particles was conducted and the morphology of the particles was reasonably predicted.To verify the accuracy of simulation results,(Ti+C)/Ni60 laser cladding layer was prepared on H13 steel substrate.The morphology of TiC and the phase and hardness of the coating were analyzed by scanning electron microscope(SEM),energy dispersive spectroscope(EDS),X-ray diffractometer(XRD),and micro-hardness tester.The results show that the morphology of TiC particles obtained by simulation prediction has high consistency with the one obtained by experiments.The plane shapes of TiC particles are usually quadrila-teral,such as square and rhombus.In the cladding process,the main causes for the inconsistency between the predicted and actual morphologies include the cladding environment,phase growth inhibition,and solid-liquid phase interaction.The TiC ceramic particles prepared in-situ are evenly distributed in the coating,and the microhardness of the coating is significantly improved.
KeyWords AITranslate
1任鑫明,马北越,张博文,张亚然,于景坤.钛合金及钢表面激光熔覆涂层的研究进展[J].材料研究与应用,2017,11(3):141-145. 被引量:8
2喻文新,闫忠琳,刘承鑫,叶宏,毛双,裴清泉.热作模具钢激光表面改性研究现状[J].热加工工艺,2015,44(24):25-29. 被引量:6
3刘立君,冯梦奎,王晓陆,崔元彪,贾志欣,李继强.超声辅助H13模具钢表面激光熔覆强化层组织分析[J].焊接学报,2021,42(6):85-90. 被引量:4
4陈菊芳,陈国炎,孙凌燕,王江涛,李兴成.H13钢表面激光熔覆层稀释率及强化效果研究[J].激光技术,2017,41(4):596-601. 被引量:13
5郝玲慧,曹雅彬.碳化物增强金属基激光熔覆层制备技术现状研究[J].热加工工艺,2022,51(2):17-20. 被引量:4
6刘全民.激光熔覆陶瓷增强金属基复合涂层研究现状[J].热喷涂技术,2014,6(2):1-5. 被引量:6
7姚芳萍,房立金,李金华,靳继波.激光功率对激光熔覆Ni基涂层温度场和应力场的影响[J].塑性工程学报,2021,28(11):87-94. 被引量:6
8牛薪,晁明举,王文丽,袁斌,梁二军.原位生成NbC颗粒增强镍基激光熔覆层[J].中国激光,2006,33(7):987-992. 被引量:26
9陈翔,张德强,李金华,孙文强,朴若华.激光辐照区中心温度对高速钢刀具熔覆WC/Co陶瓷层裂纹与组织的影响[J].表面技术,2021,50(4):113-124. 被引量:4
10张晓东,揭晓华,罗松,郑琼彬.WC/Co-Cr复合涂层激光熔覆工艺优化与表征[J].表面技术,2015,44(6):11-16. 被引量:11
1姚冰川,谢洋洋.自装卸式垃圾车装料机构的技术现状与发展趋势探讨[J].专用汽车,2022(11):28-31.
2王开放,姜瑛,陈威伟.云计算环境下虚拟机故障预测[J].现代电子技术,2022,45(24):30-36. 被引量:1
3赵朋飞,马月香,张诺,赵姗,纪硕,姜申德,刘春艳.基于网络药理学和分子对接探讨半边莲治疗新型冠状病毒肺炎的潜力[J].华北理工大学学报:自然科学版,2023,45(1):109-118.
4郭红丽,李勇.激光熔覆制备Ni60-WC-Co复合涂层工艺与性能研究[J].精密成形工程,2022,14(12):184-190. 被引量:1
5范祺,蔡玉强,贾思楠.基于RobotStudio的机器人焊接工作站仿真[J].华北理工大学学报:自然科学版,2023,45(1):81-88. 被引量:1
6史倩,樊小哲,叶蔚甄.芳烃分子最小分子尺寸研究[J].石油化工,2022,51(11):1306-1311.
7吴宪吉,宋元元,杨志荣,闫德胜,姜海昌,胡小锋.淬火温度对Fe-Cr-B-C合金涂层组织及硬度的影响[J].金属热处理,2022,47(10):224-227.
8王磊.石墨烯对氩弧熔覆镍基涂层组织与性能的影响[J].黑龙江科技大学学报,2022,32(6):759-764. 被引量:1
9白韡,曹昊敏,燕子腾,陈伟,刘恒恒,丁国良.管排结构不规则的空调器用翅片管换热器性能仿真[J].暖通空调,2022,52(12):52-58. 被引量:1
10徐伟玮.系统增量评价法在输变电项目经济评价中的应用研究[J].能源研究与利用,2022(5):35-38.
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Based on Materials Studio software,a simulation analysis of the growth mechanism of TiC cera-mic particles was conducted and the morphology of the particles was reasonably predicted.To verify the accuracy of simulation results,(Ti+C)/Ni60 laser cladding layer was prepared on H13 steel substrate.The morphology of TiC and the phase and hardness of the coating were analyzed by scanning electron microscope(SEM),energy dispersive spectroscope(EDS),X-ray diffractometer(XRD),and micro-hardness tester.The results show that the morphology of TiC particles obtained by simulation prediction has high consistency with the one obtained by experiments.The plane shapes of TiC particles are usually quadrila-teral,such as square and rhombus.In the cladding process,the main causes for the inconsistency between the predicted and actual morphologies include the cladding environment,phase growth inhibition,and solid-liquid phase interaction.The TiC ceramic particles prepared in-situ are evenly distributed in the coating,and the microhardness of the coating is significantly improved.
quote
| GB/T 7714-2015 | [1] YAO Fang-ping, WANG Ying-xiao, LI Jin-hua, et al. Morphology Study of TiC Ceramic Particles Generated In-situ by Laser Cladding[J]. Rare Metals and Cemented Carbides, 2022(5): 75-81. |
| MLA | [1] YAO Fang-ping, et al., "Morphology Study of TiC Ceramic Particles Generated In-situ by Laser Cladding." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 75-81. |
| APA | [1] YAO Fang-ping, WANG Ying-xiao, LI Jin-hua, & GAO Feng. (2022). Morphology Study of TiC Ceramic Particles Generated In-situ by Laser Cladding. Rare Metals and Cemented Carbides(5), 75-81. |
| IEEE | [1] YAO Fang-ping, WANG Ying-xiao, LI Jin-hua, and GAO Feng, "Morphology Study of TiC Ceramic Particles Generated In-situ by Laser Cladding," Rare Metals and Cemented Carbides, no. 5, pp. 75-81, 2022. keywords: {TiC ceramic particle;laser cladding;growth mechanism;morphology;in-situ generation;microhardness;simulation analysis} |