The microstructure and mechanical properties of B2-type as-cast Zr46Co46Cu8,Zr45Co45Cu10and Zr44Co44Cu12alloys were studied by X-ray diffractometer,optical microscope,electro-mechanical universal testing machine,and scanning electron microscope.The results show that the Zr-Co-Cu alloys are mainly composed of the B2-ZrCo phase and the secondary phase Co2Zr,and the content of the Co2Zr phase increases with the increase of Cu content.Part of the Co2Zr phase precipitates along the grain boundary or inside the equiaxed B2 phase particles.Also with the increase of Cu content,both the yield strength and elastic limit of the material increase.The higher strength of Zr45Co45Cu10and Zr44Co44Cu12alloys is attributed to the grain refinement of the B2 phase and the strengthening effect of the secondary phase Co2Zr.The larger toughness values of Zr46Co46Cu8and Zr45Co45Cu10alloys indicate that these two alloys are safe and reliable in practical application.The fracture mechanism of Zr46Co46Cu8and Zr45Co45Cu10alloys is mainly ductile fracture,while the fracture mechanism of Zr44Co44Cu12alloy is mainly ductile fracture supplemented by intergranular fracture.
KeyWords AITranslate
1黄斌,武俊霞,孟凡莹,何叶,高亮明,李培友.快速凝固制备铸态B2型Zr-Co-Al合金的微观结构和力学性能[J].机械工程材料,2020,44(10):67-71. 被引量:4
2李培友.热处理温度对B2型Zr56Co44合金显微组织及力学性能影响[J].材料热处理学报,2019,40(7):53-59. 被引量:4
3李培友,童婷,王永善,唐玲.热处理温度对B2型Zr54Co46合金微观组织及力学性能的影响[J].有色金属工程,2019,9(10):29-35. 被引量:5
4李培友,王永善.热处理温度对Zr_(44)Co_(56)合金显微组织和力学性能影响[J].中国有色金属学报,2017,27(11):68-69. 被引量:5
5李培友,童婷,王永善.热处理温度对Zr_(49)Co_(49)Ti_2合金微观组织和力学性能的影响[J].金属热处理,2017,42(9):90-93. 被引量:4
6李培友,童婷,王永善.热处理温度对Zr_(48)Co_(52)合金微观组织和力学性能的影响[J].材料热处理学报,2017,38(3):83-88. 被引量:6
1程剑文,饶群力,李金富,姚婷婷.Ti_(2)AlNb基合金中的组织转变及其动力学研究进展[J].航空材料学报,2022,42(6):1-8.
2李文超,景媛.一种改进的Xue-Wierzbicki延性断裂模型[J].塑性工程学报,2022,29(11):127-137.
3袁希金,许用会.42CrMo传动半轴断裂失效分析[J].山西冶金,2022,45(7):53-55.
4张林,刘海,官跃辉,蒋楠,陆长河,张剑锋.高碳铬轴承钢碳化物带状评定方法探究[J].特殊钢,2022,43(6):42-45. 被引量:2
5李晓宇,马永泉,赵永宁,张华恺,田利.输电线路金具直角挂板断裂原因分析[J].山东电力技术,2022,49(11):25-31.
6周万清,覃意,赵帅,刘冬梅,王斌,李东升.磷石膏自蒸养法制备α半水石膏[J].化工环保,2022,42(6):721-727.
7罗子相,刘克,杨兵,吴焕芬,张灵,廖蓓蕾.深冷处理对18Cr2Ni2MoNbA钢耐磨性的影响[J].金属热处理,2022,47(10):164-168.
8吴章平,关春龙,赵志伟,赵小苗,陈倩倩,史丽萍.微波溶剂热法快速合成CoSb_(3)纳米粉体的工艺研究[J].现代化工,2022,42(11):145-149.
9栾玉琦,吴红艳,王琬淇,高秀华,杜林秀.轴类锻件用中锰钢的高温热塑性[J].金属热处理,2022,47(10):52-57.
10王芝秀,章宇豪,陈天宇,李海,孙萌,徐效栋.时效对冷轧Al-Cu-Li合金拉伸性能及晶间腐蚀敏感性的影响[J].中国有色金属学报,2022,32(10):2909-2919.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]
Citation Information:
The microstructure and mechanical properties of B2-type as-cast Zr46Co46Cu8,Zr45Co45Cu10and Zr44Co44Cu12alloys were studied by X-ray diffractometer,optical microscope,electro-mechanical universal testing machine,and scanning electron microscope.The results show that the Zr-Co-Cu alloys are mainly composed of the B2-ZrCo phase and the secondary phase Co2Zr,and the content of the Co2Zr phase increases with the increase of Cu content.Part of the Co2Zr phase precipitates along the grain boundary or inside the equiaxed B2 phase particles.Also with the increase of Cu content,both the yield strength and elastic limit of the material increase.The higher strength of Zr45Co45Cu10and Zr44Co44Cu12alloys is attributed to the grain refinement of the B2 phase and the strengthening effect of the secondary phase Co2Zr.The larger toughness values of Zr46Co46Cu8and Zr45Co45Cu10alloys indicate that these two alloys are safe and reliable in practical application.The fracture mechanism of Zr46Co46Cu8and Zr45Co45Cu10alloys is mainly ductile fracture,while the fracture mechanism of Zr44Co44Cu12alloy is mainly ductile fracture supplemented by intergranular fracture.
quote
| GB/T 7714-2015 | [1] DONG Hong-feng, MENG Fan-ying, LIU Ya-ling, et al. Study on Microstructure and Mechanical Properties of B2-type As-cast Zr-Co-Cu Alloys[J]. Rare Metals and Cemented Carbides, 2022(5): 82-88. |
| MLA | [1] DONG Hong-feng, et al., "Study on Microstructure and Mechanical Properties of B2-type As-cast Zr-Co-Cu Alloys." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 82-88. |
| APA | [1] DONG Hong-feng, MENG Fan-ying, LIU Ya-ling, ZHANG Wei, WANG Lin, WU Jun-xia, & LI Pei-you. (2022). Study on Microstructure and Mechanical Properties of B2-type As-cast Zr-Co-Cu Alloys. Rare Metals and Cemented Carbides(5), 82-88. |
| IEEE | [1] DONG Hong-feng, MENG Fan-ying, LIU Ya-ling, ZHANG Wei, WANG Lin, WU Jun-xia, and LI Pei-you, "Study on Microstructure and Mechanical Properties of B2-type As-cast Zr-Co-Cu Alloys," Rare Metals and Cemented Carbides, no. 5, pp. 82-88, 2022. keywords: {Zr-Co-Cu alloy;microstructure;mechanical property;work hardening} |