Effects of Remelting on Microstructure and Properties of Ti-1Al-8V-5Fe Alloy Prepared by Selective Laser Melting AITranslate
Abstract AITranslate
To eliminate theβspots in Ti-1 Al-8 V-5 Fe(Ti185)alloy produced by conventional casting process,the large-particle-size Ti185 alloy powder was formed by selective laser melting,and the selective laser melting Ti185 alloy was optimized by remelting process.The microstructure and mechanical properties of the top,middle and bottom positions of the formed sample before and after remelting were analyzed.The results show that macroscopic cracks exist in the Ti185 sample formed by selective laser melting,and the remelting process can effectively suppress the initiation of the cracks.The microstructures of the formed samples by selective laser melting and remelting optimization are all composed of equiaxedβphase,and subcrystalline microstructure exists inside the equiaxed grains.The maximum compressive strength of the formed sample by selective laser melting which is optimized by remelting is 2127±120 MPa,and its fracture strain is 21%±5%,which shows a decrease in compression performance compared with the sample before remelting.
KeyWords AITranslate
1石文天,王朋,刘玉德,石学智.选区激光熔化TiAl合金裂纹产生机制及工艺优化试验研究[J].稀有金属,2019,43(4):349-358. 被引量:14
2卞玉超,彭英博,宋凌峰,汤宏伟,蔡广路,仲高艳,杨守峰.基于激光重熔优化工艺的激光选区熔化316L/IN718异质异构研究[J].中国激光,2021,48(18):74-85. 被引量:5
3邓德伟,马云波,马玉山,何涛,黄治冶,孙奇.重熔及退火对316L不锈钢激光熔覆层残余应力的影响[J].金属热处理,2020,45(8):113-118. 被引量:8
4陈帅,陶凤和,贾长治,孙河洋.激光重熔对选区激光熔化成形4Cr5MoSiV1钢组织和性能的影响[J].表面技术,2020,49(12):209-219. 被引量:5
5Zhiyuan Liu,Dandan Zhao,Pei Wang,Ming Yan,Can Yang,Zhangwei Chen,Jian Lu,Zhaoping Lu.Additive manufacturing of metals:Microstructure evolution and multistage control[J].材料科学技术:英文版,2022(5):224-236. 被引量:22
1欧远辉,王迪,刘林青,杨永强,韩昌骏,陶振青,伊浩,邓澄,谭超林,吴光正.激光选区熔化成形CuCrZr合金导电率提升机理研究[J].机械工程学报,2022,58(17):297-308. 被引量:1
2吝冉,杨丽娜,冯运莉,李杰.退火时间对冷轧中碳Cr-Mo钢微观组织的影响[J].金属热处理,2022,47(10):31-35.
3盛永清,王浩军,陈素明.民机用AlSi10Mg合金SLM成形的组织与性能[J].有色金属工程,2022,12(12):8-11. 被引量:1
4邹田春,陈敏英,梅思远,祝贺,杨旭东.激光选区熔化纳米SiC/AlSi7Mg复合材料微观组织及力学性能[J].材料工程,2022,50(12):143-151.
5刘明坤,刘国良,韩振宇,佟文伟,吴才广.航空发动机压气机转子叶片开裂原因分析[J].风机技术,2022,64(5):76-80.
6赵亚东,路尧文,何洋洋,崔红保,王曙光,郭学锋.1060铝/AZ31B镁异种金属FSW接头的组织演化与力学性能[J].中国有色金属学报,2022,32(10):3071-3084. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]
Citation Information:
To eliminate theβspots in Ti-1 Al-8 V-5 Fe(Ti185)alloy produced by conventional casting process,the large-particle-size Ti185 alloy powder was formed by selective laser melting,and the selective laser melting Ti185 alloy was optimized by remelting process.The microstructure and mechanical properties of the top,middle and bottom positions of the formed sample before and after remelting were analyzed.The results show that macroscopic cracks exist in the Ti185 sample formed by selective laser melting,and the remelting process can effectively suppress the initiation of the cracks.The microstructures of the formed samples by selective laser melting and remelting optimization are all composed of equiaxedβphase,and subcrystalline microstructure exists inside the equiaxed grains.The maximum compressive strength of the formed sample by selective laser melting which is optimized by remelting is 2127±120 MPa,and its fracture strain is 21%±5%,which shows a decrease in compression performance compared with the sample before remelting.
quote
| GB/T 7714-2015 | [1] WANG Lei, ZHANG Xue-zhe, ZHOU Quan, et al. Effects of Remelting on Microstructure and Properties of Ti-1Al-8V-5Fe Alloy Prepared by Selective Laser Melting[J]. Rare Metals and Cemented Carbides, 2022(5): 70-74. |
| MLA | [1] WANG Lei, et al., "Effects of Remelting on Microstructure and Properties of Ti-1Al-8V-5Fe Alloy Prepared by Selective Laser Melting." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 70-74. |
| APA | [1] WANG Lei, ZHANG Xue-zhe, ZHOU Quan, & TANG Hui-ping. (2022). Effects of Remelting on Microstructure and Properties of Ti-1Al-8V-5Fe Alloy Prepared by Selective Laser Melting. Rare Metals and Cemented Carbides(5), 70-74. |
| IEEE | [1] WANG Lei, ZHANG Xue-zhe, ZHOU Quan, and TANG Hui-ping, "Effects of Remelting on Microstructure and Properties of Ti-1Al-8V-5Fe Alloy Prepared by Selective Laser Melting," Rare Metals and Cemented Carbides, no. 5, pp. 70-74, 2022. keywords: {remelting;selective laser melting;Ti-1Al-8V-5Fe alloy;microstructure;compression performance} |