Study on Preparation Technology of LiNbO3 Polycrystal Powder AITranslate

Guangdong Guangsheng Rare Metal Photoelectric New Material Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

LiNbOpolycrystal powder was prepared from high-purity niobium pentoxide and high-purity lithium carbonate by proportionally mixing,charging and sintering.And the control of the preparation process was reflected by the decrement rate of the components.The results show that the increase of sintering temperature and holding time can promote the increase of particle size of LiNbOpolycrystal powder.The particle size distribution of LiNbOpolycrystal powder prepared by two-stage sintering of 790~850℃×3.5 h and 1050~1100℃×4 h is uniform with D50 of 18.10μm,which is suitable for LiNbOsingle crystal production.

KeyWords AITranslate

LiNbO3 polycrystal powder high-purity niobium pentoxide sintering decrement rate particle size

1吁霁,刘兴泉.铌酸锂多晶粉体的水热合成及表征[J].高等学校化学学报,2005,26(4):595-598. 被引量:4

2鲁东,喻文斌,王诗海,张伟宁,郭洪范.结晶法和萃取法制备高纯氧化铌的研究[J].广州化工,2020,48(20):53-54. 被引量:1

1吴呈祥,李付明.氧化铝粉粒度及粒度分布的工艺控制[J].世界有色金属,2021,46(22):32-33.

2何晋丰,杨威,乔健,王琨,陈赟,张翀,林俊,尹立,张进.高导热环氧/Al_(2)O_(3)复合材料制备工艺研究[J].绝缘材料,2022,55(12):20-26.

3李建新,赵婉君,闫石,乐威,马晓航,刘大志,焦清介.镁含量对离心雾化铝镁合金粉反应性能的影响[J].含能材料,2021,29(10):888-896. 被引量:1

4李波,卢森,龚艺松,聂远洋,高真真,李胜利,芦菲.金针菇豆腐制备工艺研究[J].食用菌,2022,44(5):68-70.

5劳海晴,蔡学军,谢仁亮,钱程.乌拉草提取液上染纯棉非织造布的制备工艺研究[J].产业用纺织品,2022,40(7):46-51.

6列静怡,曾靖敏,赵炳权,王岩,王婴.羟基喜树碱脂质体的制备工艺研究[J].广东药科大学学报,2022,38(6):1-6.

7李成,李一兵,方丽丽,李婷,潘杰,陈连剑.复方苦参蛇床子止痒乳膏剂制备工艺研究[J].中国药业,2022,31(23):44-47. 被引量:1

8邸学,田盛,魏巍,李万敏,裴帅龙,王海波.响应面法优化磁性壳状固定化脂肪酶制备工艺研究[J].食品安全质量检测学报,2022,13(19):6238-6246.

9李松洋,邓妍,杨放,雷诗懿,高天赐,杨敏,徐玉玲.秦艽喷膜剂的制备工艺研究及其质量标准建立[J].中草药,2022,53(20):6462-6471.

10赵立杰,张芳,彭军,明守禄,朱瑞宗.多孔金属材料的制备工艺研究进展及应用[J].粉末冶金工业,2022,32(5):110-116. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TM22.5[一般工业技术—材料科学与工程]

Citation Information:

LiNbOpolycrystal powder was prepared from high-purity niobium pentoxide and high-purity lithium carbonate by proportionally mixing,charging and sintering.And the control of the preparation process was reflected by the decrement rate of the components.The results show that the increase of sintering temperature and holding time can promote the increase of particle size of LiNbOpolycrystal powder.The particle size distribution of LiNbOpolycrystal powder prepared by two-stage sintering of 790~850℃×3.5 h and 1050~1100℃×4 h is uniform with D50 of 18.10μm,which is suitable for LiNbOsingle crystal production.

quote

GB/T 7714-2015 [1] LIU Zi-xi. Study on Preparation Technology of LiNbO3 Polycrystal Powder[J]. Rare Metals and Cemented Carbides, 2022(5): 66-69.
MLA [1] LIU Zi-xi. "Study on Preparation Technology of LiNbO3 Polycrystal Powder." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 66-69.
APA [1] LIU Zi-xi. (2022). Study on Preparation Technology of LiNbO3 Polycrystal Powder. Rare Metals and Cemented Carbides(5), 66-69.
IEEE [1] LIU Zi-xi, "Study on Preparation Technology of LiNbO3 Polycrystal Powder," Rare Metals and Cemented Carbides, no. 5, pp. 66-69, 2022. keywords: {LiNbO3 polycrystal powder;high-purity niobium pentoxide;sintering;decrement rate;particle size}