Study on Microstructure and Electrochemical Corrosion Behavior of Al2O3 Doped Molybdenum Alloys AITranslate

School of Materials Science and Engineering,Henan University of Science and Technology;School of Materials Science and Engineering,Henan University of Science and Technology;School of Materials Science and Engineering,Henan University of Science and Technology;School of Materials Science and Engineering,Henan University of Science and Technology;School of Materials Science and Engineering,Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of Al2O3doping on the electrochemical corrosion resistance of molybdenum alloys in 3.5%NaCl solution was studied,and the corrosion mechanism of the alloys was analyzed.The results show that the corrosion resistance of Mo-Al2O3alloys is significantly better than that of pure molybdenum,and it increases at first and then decreases with the increase of Al2O3content.During the corrosion process,Cl-is preferentially adsorbed on the defect positions of the molybdenum alloy oxide film to form pitting.With the increase of potential,the pitting expands along the grain boundary to become corrosion grooves.Al2O3can refine the molybdenum grains to promote the formation of a dense oxide film of molybdenum alloys which is less easily prone to pitting,thereby improving the corrosion resistance of the molybdenum alloys.However,when the volume fraction of Al2O3in molybdenum alloys reaches 1.6%,the Al2O3particles agglomerate and grow larger,which destroys the integrity of the oxide film of the molybdenum alloy and weakens their protection of the alloy matrix,resulting in a decrease in the corrosion resis-tance of the molybdenum alloy.

KeyWords AITranslate

molybdenum alloy Al2O3doping electrochemical corrosion corrosion mechanism oxide film microstructure

1居炎鹏,王爱琴.钼合金研究现状[J].粉末冶金工业,2015,25(4):58-62. 被引量:29

2刘辉,巨建辉,张军良,崔顺,夏明星.钼合金的强韧化与发展趋势[J].中国钼业,2011,35(2):26-28. 被引量:10

3李洲,徐流杰,魏世忠,潘昆明,肖方闹.水热法制备ZrO_2掺杂钨合金粉末的工艺研究及表征[J].稀有金属与硬质合金,2017,45(1):31-35. 被引量:4

4朱向炜,张国赏,崔超鹏,魏世忠,郭松亮.Zr元素添加量对钼合金组织和性能的影响研究[J].稀有金属与硬质合金,2014,42(4):31-34. 被引量:2

5康蓉,颜建辉,李茂键.溶胶凝胶/高温氢还原法制备纳米Mo-ZrO_(2)(Y_(2)O_(3))复合粉末[J].稀有金属,2021,45(3):288-296. 被引量:4

6代宝珠,魏世忠,徐流杰,彭光辉,李继文,张国赏.Al_2O_3对钼合金组织与性能的影响[J].河南科技大学学报:自然科学版,2010,31(1):1-4. 被引量:4

7侯风亮,倪峰,崔延遂,侯麦珍,魏世忠,流杰.Al2O3/Mo复合材料的制备与性能[J].稀有金属材料与工程,2011,40(12):2175-2178. 被引量:7

8胡亚杰,徐流杰,周玉成,李继文,刘伟,魏世忠.水热法制备Al_2O_3掺杂钼合金[J].材料热处理学报,2015,36(6):15-20. 被引量:7

9孙铁龙,徐流杰,魏世忠,潘昆明,李武会,周玉成,黄志民.Al2O3颗粒弥散强化钼合金的显微组织与压缩性能[J].中国有色金属学报:英文版,2020,30(12):3307-3321. 被引量:3

10田文明,巢昺轩,李智勇,郭楠,韩凤鸣.晶粒尺寸影响金属钝化行为的研究进展[J].失效分析与预防,2018,13(2):130-136. 被引量:6

1张昌青,王树文,罗德春,师文辰,刘晓,崔国胜,陈波阳,辛舟,芮执元.热电耦合对铝/钢连续驱动摩擦焊接头组织的影响机理[J].材料工程,2022,50(5):35-42. 被引量:1

2温家浩,杨中桂,白洁,王自强.海上风电设备防腐技术与展望[J].船舶工程,2022,44(S01):57-60. 被引量:3

3郭星.铁器文物腐蚀与保护的几个问题[J].收藏与投资,2022,13(11):110-112.

4戴军,徐超,李冀.卤水对矿山充填体中钢筋腐蚀的机理及防护研究[J].采矿技术,2022,22(6):110-113.

5黄玉林,邢佳颖,王春波,张月.Mn-Fe复合氧化物脱除燃煤烟气中砷、硒的实验研究[J].燃料化学学报,2022,50(11):1517-1523.

6何成,王欣欣,李富天,刘光明,何华林,杨海涛.304不锈钢在不同pH的库尔勒土壤浸出液中的腐蚀电化学行为[J].电镀与涂饰,2022,41(22):1595-1600. 被引量:1

7张明,付冬梅,张达威,马菱薇,邵立珍.基于综合智能模型的碳钢大气腐蚀重要变量提取和依赖关系挖掘[J].工程科学学报,2023,45(3):407-418.

8淳道勇,詹中伟,葛玉麟,孙志华.GH909合金热盐腐蚀行为及力学性能衰减研究[J].电镀与精饰,2022,44(12):11-16.

9马麒,蔡景顺,穆松,刘凯,刘建忠,刘加平.羧酸胺阻锈剂在模拟孔隙液和混凝土中对钢筋的阻锈作用[J].材料导报,2022,36(23):149-156.

10张逸哲,张天遂,万辉海,李广芳,刘宏芳.应力条件下埋地输油管线菌致开裂行为研究进展[J].化学工程与技术,2022,12(6):353-364.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]

Citation Information:

The effect of Al2O3doping on the electrochemical corrosion resistance of molybdenum alloys in 3.5%NaCl solution was studied,and the corrosion mechanism of the alloys was analyzed.The results show that the corrosion resistance of Mo-Al2O3alloys is significantly better than that of pure molybdenum,and it increases at first and then decreases with the increase of Al2O3content.During the corrosion process,Cl-is preferentially adsorbed on the defect positions of the molybdenum alloy oxide film to form pitting.With the increase of potential,the pitting expands along the grain boundary to become corrosion grooves.Al2O3can refine the molybdenum grains to promote the formation of a dense oxide film of molybdenum alloys which is less easily prone to pitting,thereby improving the corrosion resistance of the molybdenum alloys.However,when the volume fraction of Al2O3in molybdenum alloys reaches 1.6%,the Al2O3particles agglomerate and grow larger,which destroys the integrity of the oxide film of the molybdenum alloy and weakens their protection of the alloy matrix,resulting in a decrease in the corrosion resis-tance of the molybdenum alloy.

quote

GB/T 7714-2015 [1] JIAO Zhao-lin, XU Liu-jie, XU Zhao-ning, et al. Study on Microstructure and Electrochemical Corrosion Behavior of Al2O3 Doped Molybdenum Alloys[J]. Rare Metals and Cemented Carbides, 2022(5): 59-65.
MLA [1] JIAO Zhao-lin, et al., "Study on Microstructure and Electrochemical Corrosion Behavior of Al2O3 Doped Molybdenum Alloys." Rare Metals and Cemented Carbides, no. 5, 2022, pp. 59-65.
APA [1] JIAO Zhao-lin, XU Liu-jie, XU Zhao-ning, ZHOU Yu-cheng, & YANG Lu. (2022). Study on Microstructure and Electrochemical Corrosion Behavior of Al2O3 Doped Molybdenum Alloys. Rare Metals and Cemented Carbides(5), 59-65.
IEEE [1] JIAO Zhao-lin, XU Liu-jie, XU Zhao-ning, ZHOU Yu-cheng, and YANG Lu, "Study on Microstructure and Electrochemical Corrosion Behavior of Al2O3 Doped Molybdenum Alloys," Rare Metals and Cemented Carbides, no. 5, pp. 59-65, 2022. keywords: {molybdenum alloy;AlOdoping;electrochemical corrosion;corrosion mechanism;oxide film;microstructure}