Effect of Rare Earth La on High Temperature Oxidation of High Carbon Alloy Tool Steel AITranslate
Abstract AITranslate
The effect of La addition on high temperature oxidation of high carbon alloy tool steel was stud- ied. The high-temperature oxidation behavior of high carbon alloy tool steel without and with rare earth La was analyzed with thermal analyzer and weight gain method. The morphology of oxide film was observed by scanning electron microscopy. The structure of the oxide layer and its layering were analyzed by observing the cross-sectional morphology of the oxide layer. The results show that all the kinetic curves of iso- thermal oxidation at 900 ℃, 1 000 ℃, 1 100 ℃ and 1 200 ℃ of high carbon alloy tool steels with and without La are in accordance with the parabolic law,and the oxide films of the two alloy tool steels are protective. The oxidation reaction activation energy of high carbon alloy tool steel with rare earth La is 23% higher than that without La addition, and its oxidation rate constant is also lower. The adhesion of the oxide film on the high carbon alloy tool steel with rare earth La is stronger,and its oxide layer is more solid. The addition of rare earth La refines oxide film grains on high carbon alloy tool steel surface, and reduces the interspace among oxide film grains, resulting in the oxide films not easy to peel off.
KeyWords AITranslate
1杨吉春,杨昌桥,贾利涛.铈对IF钢冲击韧性的影响[J].稀土,2014,35(3):19-22. 被引量:13
2苏勇,张顺科,付广艳,刘群,朱鹤.铈对铜硅合金高温氧化性能的影响[J].稀土,2016,37(4):60-66. 被引量:1
3白力静,梁戈,李虹燕,李均明.常用中碳钢氧化特性研究[J].西安工业学院学报,2005,25(5):460-464. 被引量:20
4陈伟鹏,李光卫,张欢,谢智辉,计云萍.稀土对低合金钢抗高温氧化性能的影响[J].稀土,2016,37(6):52-57. 被引量:3
5杨吉春,杨昌桥,周莉,王明超.Ce对IF钢显微组织和力学性能的影响[J].稀土,2014,35(5):25-29. 被引量:17
6张辉,崔文芳,王建军,刘春明.铈对00Cr17铁素体不锈钢高温抗氧化性的影响[J].中国稀土学报,2010,28(3):366-371. 被引量:6
7林勤,宋波,郭兴敏,张梅.钢中稀土微合金化作用与应用前景[J].稀土,2001,22(4):31-36. 被引量:103
8王龙妹,杜挺,卢先利,乐可襄.微量稀土元素在钢中的作用机理及应用研究[J].稀土,2001,22(4):37-40. 被引量:144
9张建,朱兆顺.稀土在钢中的应用[J].金属材料与冶金工程,2008,36(5):56-60. 被引量:14
10于萍,王文,王福会.Influence of cyclic frequency on oxidation behavior of K38 superalloy with yttrium additions at 1273 K[J].稀土学报:英文版,2011,29(2):119-123. 被引量:13
1白公民.20CrMnTi钢表面稀土硼碳共渗层组织及性能[J].金属加工:热加工,2021(1):73-76. 被引量:1
2屠兴圹,左锦中,赵赟,苏振伟.加热和冷却条件对合金工具钢S2表面氧化与脱碳的影响[J].金属热处理,2023,48(8):124-131.
3郭克星,夏鹏举.稀土镁变质对金属型铸造高铬铸铁Cr26耐磨性的影响[J].稀有金属与硬质合金,2019,47(2):39-44. 被引量:3
1王松,张卫红,周啸颖,王建刚.淬火回火工艺对高碳热磨片显微组织及耐磨性的影响[J].河北科技大学学报,2020,41(6):537-543. 被引量:5
2宋延沛,陈丹萍,周汉,林小丽,李丽.热处理工艺对Cr15Ni2MnMoCuNbRE铸钢组织及性能的影响[J].金属热处理,2022,47(2):178-182. 被引量:1
3郭克星.高铬铸铁耐磨性研究的进展[J].热处理,2023,38(1):1-5.
4于庆萍,张光胜,夏莲森,方慧敏.CeO_(2)添加量对铁基粉末冶金材料表面渗硼层组织与摩擦磨损性能的影响[J].机械工程材料,2023,47(4):18-22.
1陈海军,陈云帅,胡宇浩,袁正浩.冷却方式对Cr26Ni14Nb2钢抗氧化性能的影响[J].热加工工艺,2017,46(24):115-118.
2王建泽,钱张信,惠恺,纪显彬.铁素体不锈钢罩式退火表面铬氧化物富积机理[J].金属热处理,2017,42(9):202-205. 被引量:2
3田筱维,王伯健,刘世锋,黄炳喜.310S奥氏体不锈钢丝高温氧化行为[J].热加工工艺,2018,47(4):51-53. 被引量:4
4孙利,阎维平.超临界水工况下铁素体马氏体钢氧化速率常数的计算方法与分析[J].动力工程学报,2018,38(2):156-162.
5王宇,隋小波,金松哲.Cr18Mn18高氮奥氏体不锈钢高温氧化特性[J].长春工业大学学报,2017,38(4):381-385. 被引量:4
6汪家梅,Farzin Arjmand,杜东海,陈凯,赖平,高文华,张浩,郭相龙,张乐福.压水堆一回路主管道316L不锈钢的电化学腐蚀行为[J].工程科学学报,2017,39(9):1355-1363. 被引量:10
7Yan-wei Yang,Yun-lu Wang,Jia-kai Lu,Lei Tian,Mu Jin,Wei-ping Cheng.Delayed xenon post-conditioning mitigates spinal cord ischemia/reperfusion injury in rabbits by regulating microglial activation and inflammatory factors[J].中国神经再生研究:英文版,2018,13(3):510-517. 被引量:4
8杨雪春.合金工具钢9SiCr的球化组织分析[J].通化师范学院学报,2017,38(10):55-58. 被引量:1
9赵艳妮,何亮.应用脉冲电流改善合金工具钢9CrSi基体组织的研究[J].机电信息,2017(33):114-115.
10任英广.高强度冲压件产品制造模具表面改性研究[J].煤矿机电,2018,39(1):64-67. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.454[金属学及工艺—金属材料]
Citation Information:
The effect of La addition on high temperature oxidation of high carbon alloy tool steel was stud- ied. The high-temperature oxidation behavior of high carbon alloy tool steel without and with rare earth La was analyzed with thermal analyzer and weight gain method. The morphology of oxide film was observed by scanning electron microscopy. The structure of the oxide layer and its layering were analyzed by observing the cross-sectional morphology of the oxide layer. The results show that all the kinetic curves of iso- thermal oxidation at 900 ℃, 1 000 ℃, 1 100 ℃ and 1 200 ℃ of high carbon alloy tool steels with and without La are in accordance with the parabolic law,and the oxide films of the two alloy tool steels are protective. The oxidation reaction activation energy of high carbon alloy tool steel with rare earth La is 23% higher than that without La addition, and its oxidation rate constant is also lower. The adhesion of the oxide film on the high carbon alloy tool steel with rare earth La is stronger,and its oxide layer is more solid. The addition of rare earth La refines oxide film grains on high carbon alloy tool steel surface, and reduces the interspace among oxide film grains, resulting in the oxide films not easy to peel off.
quote
| GB/T 7714-2015 | [1] CHEN Wei-peng, WANG qiang, JIANG Meng-qing, et al. Effect of Rare Earth La on High Temperature Oxidation of High Carbon Alloy Tool Steel[J]. Rare Metals and Cemented Carbides, 2018(2): 21-26. |
| MLA | [1] CHEN Wei-peng, et al., "Effect of Rare Earth La on High Temperature Oxidation of High Carbon Alloy Tool Steel." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 21-26. |
| APA | [1] CHEN Wei-peng, WANG qiang, JIANG Meng-qing, TANG Wei-dong, & LI Bao-wei. (2018). Effect of Rare Earth La on High Temperature Oxidation of High Carbon Alloy Tool Steel. Rare Metals and Cemented Carbides(2), 21-26. |
| IEEE | [1] CHEN Wei-peng, WANG qiang, JIANG Meng-qing, TANG Wei-dong, and LI Bao-wei, "Effect of Rare Earth La on High Temperature Oxidation of High Carbon Alloy Tool Steel," Rare Metals and Cemented Carbides, no. 2, pp. 21-26, 2018. keywords: {rare earth La;high carbon alloy tool steel;high temperature oxidation;oxide film;kinetics} |