Effect of Different PrPO_4 Coating Methods on the Electrochemical Performance of Li-rich Manganese-based Cathode Materials AITranslate
Abstract AITranslate
Li-rich manganese-based material Li1.2[Mn0.54Ni0.13Co0.13]O2, was synthesized with co-precipitati- on and high temperature solid state method,and then coated with PrPO4 by simple wet chemical precipita- tion and PVP-assisted wet chemical deposition. The results show that with PVP-assisted coating,the coat- ing layer is more uniform,and the electrochemical properties are obviously improved. The 3 %-PVP coated sample shows an initial discharge capacity of 286.7 mA·h/g with Coulombie efficiency of 89.60~, and more excellent cycling stability with discharge specific capacity of 254 mA·h/g after 50 cycles at 0.1C discharge rate, and the capacity retention increases from 88.5% of the blank sample to 95%. Thus,it turns out that the uniform PrPO4 coating layer can effectively improve the comprehensive electrochemical performance of Li-rieh manganese-based cathode material.
KeyWords AITranslate
1殷春梅,郭忻,周春仙,夏朝阳,廖达前,习小明,肖可颂,陈晓青.表面包覆对富锂锰基材料循环稳定性影响研究[J].矿冶工程,2016,36(3):94-97. 被引量:5
2王旭阳,叶学海,郅晓科,何爱珍,赵桢,章甦,时洁.AlF_3包覆对Li_(1.2)Mn_(0.534)Ni_(0.133)Co_(0.133)O_2正极材料电化学性能的影响[J].无机化学学报,2013,29(4):774-778. 被引量:8
1耿萌萌,杨凯,毛洪星,高运兴,钟健健.表面修饰MnMoO4用于提高富锂锰基正极材料的电化学性能的研究[J].稀有金属与硬质合金,2020(1):61-67. 被引量:2
1黄鹏,邹大中,牛棒棒,陈浩舟,李勋.高能量密度富锂锰基正极材料结构调控与性能研究[J].稀有金属与硬质合金,2022,50(1):63-69. 被引量:3
2冯婷,王睿,王京玥,王磊营,石沁灵,王立帆,詹纯.压电材料K_(0.5)Na_(0.5)NbO_(3)表面修饰高镍正极材料LiNi_(0.83)Co_(0.12)Mn_(0.05)O_(2)的电化学性能研究[J].稀有金属与硬质合金,2022,50(5):89-95. 被引量:1
1张建峰,赵春龙,童晶,涂溶.二氧化硅包覆的微纳米材料的制备与应用[J].硅酸盐学报,2017,45(10):1410-1420. 被引量:4
2澳大利亚稀土生产商Lynas 2017年销售额上涨[J].稀土信息,2018,0(3):19-19.
3时志权,王惠,陆德炜.PEDOT/RDX复合粒子的制备与性能研究[J].推进技术,2017,38(11):2628-2633. 被引量:2
4姚建华,韩鹏献,韩晓琪,崔光磊.硬炭用于锂离子电容器的研究及其低温性能[J].电源技术,2018,42(1):87-89.
5张露,韩勇.电动汽车电池管理系统SOC算法优化研究分析[J].南方农机,2018,49(5):146-146. 被引量:3
6张鹏,杜飞,栗茹,潘尚可,潘建国,陈红兵.Pr3+、Ce3+共掺LiYSiO4闪烁体的发光性能[J].硅酸盐学报,2018,46(4):524-528.
7张大鹏,范瑞娟,曹国林,田占元,邓增社.混合电容器负极材料钛铬酸锂/钛酸锂复合材料合成及性能研究[J].矿冶工程,2018,38(1):123-126. 被引量:2
8刘宝禄,谢志鹏.多重氧化的石墨毡作为Zn/Fe液流电池电极[J].有色金属科学与工程,2018,9(1):39-44. 被引量:2
9周佳,吴鹏超,田晓.充放电对LaMgNi系储氢合金电化学性能的影响[J].内蒙古师范大学学报:自然科学汉文版,2017,46(6):814-817. 被引量:2
10王彦斌,张紫朋,张德华,苏琼,王宏刚.SiO_2/酚醛树脂核壳纳米颗粒制备研究[J].化工新型材料,2018,46(3):172-174.
Basic Information:
DOI:
Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]
Citation Information:
Li-rich manganese-based material Li1.2[Mn0.54Ni0.13Co0.13]O2, was synthesized with co-precipitati- on and high temperature solid state method,and then coated with PrPO4 by simple wet chemical precipita- tion and PVP-assisted wet chemical deposition. The results show that with PVP-assisted coating,the coat- ing layer is more uniform,and the electrochemical properties are obviously improved. The 3 %-PVP coated sample shows an initial discharge capacity of 286.7 mA·h/g with Coulombie efficiency of 89.60~, and more excellent cycling stability with discharge specific capacity of 254 mA·h/g after 50 cycles at 0.1C discharge rate, and the capacity retention increases from 88.5% of the blank sample to 95%. Thus,it turns out that the uniform PrPO4 coating layer can effectively improve the comprehensive electrochemical performance of Li-rieh manganese-based cathode material.
quote
| GB/T 7714-2015 | [1] DING Fei-xiang, LI dian-ling, DENG Fu-hai, et al. Effect of Different PrPO_4 Coating Methods on the Electrochemical Performance of Li-rich Manganese-based Cathode Materials[J]. Rare Metals and Cemented Carbides, 2018(2): 27-31. |
| MLA | [1] DING Fei-xiang, et al., "Effect of Different PrPO_4 Coating Methods on the Electrochemical Performance of Li-rich Manganese-based Cathode Materials." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 27-31. |
| APA | [1] DING Fei-xiang, LI dian-ling, DENG Fu-hai, XU Ouo-feng, LI Zhan-yu, & LIU Yan-ying. (2018). Effect of Different PrPO_4 Coating Methods on the Electrochemical Performance of Li-rich Manganese-based Cathode Materials. Rare Metals and Cemented Carbides(2), 27-31. |
| IEEE | [1] DING Fei-xiang, LI dian-ling, DENG Fu-hai, XU Ouo-feng, LI Zhan-yu, and LIU Yan-ying, "Effect of Different PrPO_4 Coating Methods on the Electrochemical Performance of Li-rich Manganese-based Cathode Materials," Rare Metals and Cemented Carbides, no. 2, pp. 27-31, 2018. keywords: {lithiumion battery + Lirich manganese- based cathode material;PVP;PrPO4;electrochemical performance} |