daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Floating and Mass Transfer of Bottom-blown Nitrogen Bubbles in Sm-Fe Melt AITranslate

College of Metallurgy and Energy,North China University of Science and Technology,Tangshan 063000,Chin;College of Metallurgy and Energy,North China University of Science and Technology,Tangshan 063000,Chin;College of Metallurgy and Energy,North China University of Science and Technology,Tangshan 063000,Chin;College of Metallurgy and Energy,North China University of Science and Technology,Tangshan 063000,Chin;College of Metallurgy and Energy,North China University of Science and Technology,Tangshan 063000,Chin
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the general rule of gas-liquid two-phase flow,the floating and mass transfer of bottom- blown nitrogen bubbles in the Sm-Fe melt were studied. The relationship between the radius of nitrogen bubbles in liquid Sm-Fe alloy and time in the process of floatation was discussed, and the mass transfer rate was also analyzed. The results show that the radius of nitrogen bubbles in the Sm-Fe melt increases with the increase of time at atmospheric pressure, and the air pressure has a significant inhibition effect on the growth of nitrogen bubbles. At atmospheric pressure, the mass transfer rate of bubbles increases at first and then decreases with time increasing in the floating process of nitrogen bubbles. When the floating time equals to 7.8 s,the mass transfer rate reaches the maximum value of 6.2×10^-11mol/(m^3·s). When the floating time is less than 7.8 s, the bubble radius plays a leading role in the mass transfer of bubbles. When the floating time is more than 7.8 s,the concentration of bubbles plays a leading role. Meanwhile,with the increase of air pressure the maximum mass transfer rate is reduced and the time to achieve the maximum mass transfer rate is increased.

KeyWords AITranslate

Sm-Fe melt nitrogen bubble floating mass transfer

1王冰,范承恩.世界最强的最大磁能积的各向同性Sm-Zr-Fe-N系粘结磁粉[J].国外金属热处理,2002,23(2):6-7. 被引量:6

2车得福,林宗虎,陈学俊.气泡在液体中形成的试验研究[J].钢铁研究学报,1994,6(1):9-14. 被引量:18

3朱江江,陈伯义.水面舰船尾流气泡半径变化规律的研究[J].热科学与技术,2005,4(2):146-149. 被引量:14

4闫雪飞,王桂军,王涌,金良安.水溶液中气泡聚并的研究进展[J].化学工业与工程,2013,30(6):49-55. 被引量:5

1刘小超.小学科学课堂自主探究教学策略[J].教育(周刊),2018,0(8):73-73.

2郭瑞华,郭乐乐,张捷宇,周国治,安胜利.双钙钛矿结构固体氧化物燃料电池阴极SmBaFe_(2-x)Co_xO_(5+δ)的制备与性能研究[J].化工新型材料,2018,46(3):183-186.

3李青,王世岚,周波,王丽红.无碱高铝硼硅酸盐玻璃澄清工艺研究[J].现代化工,2017,37(9):155-158. 被引量:4

4朱信尧,宋保维,王鹏.锚泊式驻留水下航行器着陆锚链冲击力分析[J].西北工业大学学报,2017,35(5):922-927. 被引量:2

5陈桥.阜南县洪河洼地受灾原因分析及治理思路[J].治淮,2018(3):18-19.

6陈磊磊,黄永红,袁野,林文威.单绕组磁悬浮开关磁阻电机低铜耗发电研究[J].信息技术,2017,41(12):1-5. 被引量:1

7薛珺予,朱宗涛,江柱中.脉冲光纤激光-MIG复合焊接A7N01铝合金接头组织及力学性能[J].热加工工艺,2017,46(21):43-46.

8孙坤,陈琛.人工心脏泵用磁轴承系统的起浮特性研究[J].机床与液压,2017,45(23):101-104. 被引量:2

9艾旭鹏,倪宝玉.流体黏性及表面张力对气泡运动特性的影响[J].物理学报,2017,66(23):227-236. 被引量:9

10冯凇,饶国宁,彭金华.含铝炸药深水爆炸冲击波和气泡脉动的数值模拟[J].爆破器材,2017,46(5):1-7. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]

Citation Information:

Based on the general rule of gas-liquid two-phase flow,the floating and mass transfer of bottom- blown nitrogen bubbles in the Sm-Fe melt were studied. The relationship between the radius of nitrogen bubbles in liquid Sm-Fe alloy and time in the process of floatation was discussed, and the mass transfer rate was also analyzed. The results show that the radius of nitrogen bubbles in the Sm-Fe melt increases with the increase of time at atmospheric pressure, and the air pressure has a significant inhibition effect on the growth of nitrogen bubbles. At atmospheric pressure, the mass transfer rate of bubbles increases at first and then decreases with time increasing in the floating process of nitrogen bubbles. When the floating time equals to 7.8 s,the mass transfer rate reaches the maximum value of 6.2×10^-11mol/(m^3·s). When the floating time is less than 7.8 s, the bubble radius plays a leading role in the mass transfer of bubbles. When the floating time is more than 7.8 s,the concentration of bubbles plays a leading role. Meanwhile,with the increase of air pressure the maximum mass transfer rate is reduced and the time to achieve the maximum mass transfer rate is increased.

quote

GB/T 7714-2015 [1] YUAN Liang-liang, GAO Ai-min, MA Hai-tao, et al. Floating and Mass Transfer of Bottom-blown Nitrogen Bubbles in Sm-Fe Melt[J]. Rare Metals and Cemented Carbides, 2018(2): 32-36.
MLA [1] YUAN Liang-liang, et al., "Floating and Mass Transfer of Bottom-blown Nitrogen Bubbles in Sm-Fe Melt." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 32-36.
APA [1] YUAN Liang-liang, GAO Ai-min, MA Hai-tao, WANG Shu-huan, & ZHAO Ding-guo. (2018). Floating and Mass Transfer of Bottom-blown Nitrogen Bubbles in Sm-Fe Melt. Rare Metals and Cemented Carbides(2), 32-36.
IEEE [1] YUAN Liang-liang, GAO Ai-min, MA Hai-tao, WANG Shu-huan, and ZHAO Ding-guo, "Floating and Mass Transfer of Bottom-blown Nitrogen Bubbles in Sm-Fe Melt," Rare Metals and Cemented Carbides, no. 2, pp. 32-36, 2018. keywords: {Sm-Fe melt;nitrogen bubble;floating;mass transfer}