Effects of La Addition on Microstructure of NdFeB and Magnetic Properties of the Melt-spun Ribbons AITranslate
Abstract AITranslate
The study was carried out on the microstructure of Nd2.28 Fe13.58B1.11 alloy with different content of rare earth La and the magnetic properties of the melt-spun ribbons. The experimental results show that the main phase of the alloy is still Nd2 Fe14 B phase after La addition. With the increase of La addition, the crystal cell volume of Nd2Fe14B phase slightly increases,both the coercivity and remanence of the meltspun ribbons decreases,and the Curie temperature also decreases.
KeyWords AITranslate
1周怀营,顾正飞,庄应烘.Nd-Fe-B磁性能的改善[J].广西大学学报:自然科学版,1991,16(3):33-37. 被引量:2
2魏成富,唐杰,杨梨容,赵导文,林红,邓盛贤.烧结钕铁硼的研究与应用进展[J].稀有金属与硬质合金,2010,38(1):47-49. 被引量:22
3姚茂海,王川,刘宇晖,陈云志,苏正夫.Ho对烧结钕铁硼永磁体性能的影响[J].稀有金属与硬质合金,2016,44(3):51-55. 被引量:8
4李智,刘卫强,查善顺,李玉卿,王云峤,张东涛,岳明,张久兴.Effects of lanthanum substitution on microstructures and intrinsic magnetic properties of Nd-Fe-B alloy[J].稀土学报:英文版,2015,33(9):961-964. 被引量:11
5李红英,郝壮志,刘宇晖,朱望伟,陈云志.烧结NdFeB永磁体磁控溅射镀Al的制备工艺及性能研究[J].稀有金属与硬质合金,2016,44(5):48-54. 被引量:1
6周晓庆,刘盛业,吕向科,张民,丁勇.La取代对烧结NdFeB磁体微观结构和性能的影响[J].磁性材料及器件,2013,44(6):17-20. 被引量:9
1许磊,柯庆进,李莎,戎茂华,王江.La-Fe-B合金的微观组织及物相转变研究[J].稀有金属与硬质合金,2020(1):31-34. 被引量:2
2张佳彬,李莎,程祥,戎茂华,王江.Pr-Fe-B合金的相转变及微观组织研究[J].稀有金属与硬质合金,2020,48(4):37-41.
3刘春,高励珍,张翼明,刘晓杰.电感耦合等离子体发射光谱法测定镨钕钆合金中稀土杂质量[J].金属功能材料,2021,28(4):59-63. 被引量:2
1李佳,朱悦然,赵文怡,周凯红.质量法测定稀土萃取回收物中有价金属的含量[J].金属功能材料,2021,28(6):100-104. 被引量:1
2张建华,李永峰,刘艳丽.晶界添加Pr-Cu对烧结Nd-La-Ce-Fe-B磁体磁性能和微观结构的影响[J].稀有金属与硬质合金,2022,50(1):57-62.
3马才伏,袁川来,赵雪琪.球磨时间对石墨烯复合材料电化学性能的影响[J].无机盐工业,2022,54(12):68-73.
4李佳,吴文琪,朱悦然,王振江.高频红外吸收法测定稀土铁合金中碳硫[J].金属功能材料,2022,29(6):113-118.
1马冬冬,顾正飞,徐成福,刘涛,成林一.SPS烧结双主相Nd_2Fe_(14)B-Ce_2Fe_(14)B稀土永磁材料微观结构的研究[J].稀有金属与硬质合金,2017,45(5):42-45.
2杜帅龙,张磊,杜杰杰,步绍静,杨薇,孙继兵.铌铁原料成分对Finemet型薄带结构及性能影响[J].功能材料,2017,48(9):9197-9203.
3张国清,黄有林,侯育花,李志浩,石志强.Ce掺杂对Nd-Fe-B快淬薄带结构及磁性能影响[J].南昌航空大学学报:自然科学版,2017,31(3):67-72.
4官钰洁.烧结温度对钛酸钡陶瓷铁电性能的影响[J].陶瓷,2018(3):24-28.
5周燕.高丰度稀土添加对NdFeB微观结构及性能影响[J].福建冶金,2017,46(5):44-46. 被引量:1
6郭沛音,杨亚,曹世勋.Cr掺杂BaTiO_3几何结构、电子结构和磁性的第一性原理研究[J].低温物理学报,2017,39(6):5-9.
7罗国仕,郑兴华,骆统领,刘洋,肖腾.退火对Ba4Sm2Fe2Nb8O30铁电体结构和性能的影响[J].金属热处理,2018,43(3):151-154.
8吕蒙,孔拓,朱明原,胡业旻,金红明,李文献,李瑛.非稀土金属及合金化合物改性烧结NdFeB磁体的研究进展[J].上海师范大学学报:自然科学版,2017,46(6):899-911.
9Bin Fu,Jun He,Jie Han,Jie Hu,Li-Wei Pang.Flow hydrogen absorption of LaFe_(10.9)Co_(0.8)Si_(1.3) compound under constant low hydrogen gas pressure[J].稀有金属:英文版,2018,37(3):243-248. 被引量:2
10王娜娜,张娜,闫景辉,姚爽.以S-中心Preyssler型多酸为模板构筑有机-无机杂化材料[J].分子科学学报,2018,34(1):45-48. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.454[金属学及工艺—金属材料]
Citation Information:
The study was carried out on the microstructure of Nd2.28 Fe13.58B1.11 alloy with different content of rare earth La and the magnetic properties of the melt-spun ribbons. The experimental results show that the main phase of the alloy is still Nd2 Fe14 B phase after La addition. With the increase of La addition, the crystal cell volume of Nd2Fe14B phase slightly increases,both the coercivity and remanence of the meltspun ribbons decreases,and the Curie temperature also decreases.
quote
| GB/T 7714-2015 | [1] CHEN Xiao-long, MA Jie, RONG Mao-hua, et al. Effects of La Addition on Microstructure of NdFeB and Magnetic Properties of the Melt-spun Ribbons[J]. Rare Metals and Cemented Carbides, 2018(2): 16-20. |
| MLA | [1] CHEN Xiao-long, et al., "Effects of La Addition on Microstructure of NdFeB and Magnetic Properties of the Melt-spun Ribbons." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 16-20. |
| APA | [1] CHEN Xiao-long, MA Jie, RONG Mao-hua, & WANG Jiang. (2018). Effects of La Addition on Microstructure of NdFeB and Magnetic Properties of the Melt-spun Ribbons. Rare Metals and Cemented Carbides(2), 16-20. |
| IEEE | [1] CHEN Xiao-long, MA Jie, RONG Mao-hua, and WANG Jiang, "Effects of La Addition on Microstructure of NdFeB and Magnetic Properties of the Melt-spun Ribbons," Rare Metals and Cemented Carbides, no. 2, pp. 16-20, 2018. keywords: {NdFeB;La;phase composition;crystal cell volume;melt-spun ribbon;magnetic property} |