Highly Efficient Antifouling Coating of Star-Shaped Block Copolymers with Variable Sizes of Hydrophobic Cores and Charge-Neutral Hydrophilic Arms AITranslate

University of Alberta;Nanotechnology Research Centre, National Research Council Canada;Nanotechnology Research Centre, National Research Council Canada; University of Alberta; University of Alberta; University of Alberta;Nanotechnology Research Centre, National Research Council Canada;IBM Almaden Research Center, 650 Harry Road; University of Alberta
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Star-shaped block copolymers (SPs) have shown promise as antifouling coating materials on water purification membranes. The unique architectural design of these SPs, composed of covalently linked hydrophobic core and hydrophilic arms, offers the flexibility of tailoring the core and/or arm compositions to achieve properties on demand. Here, variable sizes of SPs with increasingly hydrophobic polystyrene cores (PSCs) and longer hydrophilic poly(ethylene glycol) (PEG) arms were synthesized to evaluate their coatability on polysulfone ultrafiltration (PSF UF) membranes and to study the effect of the hydrophilic PEG arm lengths on the antifouling properties of SP-coated membranes. The oleophobicity evaluated from underwater hexadecane contact angle (CA) measurements of SP-coated membranes increased by approximately 3 times, leading to almost 7 times improvement in permeation flux during oil emulsion filtration. No flux recovery was observed for the pristine PSF membrane, whereas 100% flux recovery ratio (FRR) was achieved for SP-coated membranes. The filtration of bovine serum albumin (BSA) protein solution exhibited an improvement in the permeation flux by 2.7–8.9 times for SP-coated membranes. The FRR was only 64% for the pristine PSF membrane, as opposed to nearly 100% FRR for all SP-coated membranes. The stability of the SP coating was tested by rigorous washing with Tween 80 surfactant and three-cycle oil emulsion filtrations. Surfactant washing only removed the loosely bound extra layers of SP coating, leaving the surface-bound and pore-entrapped stable SP coating with remarkable antifouling properties. Since SP3 with the largest hydrophobic PSC showed much better performance, the effect of increasing its PEG arm length on the antifouling properties was studied further, and the largest size SP3 with the longest PEG arm was the optimum antifouling coating. This study provides insights into the design of block copolymer nanoarchitecture to develop antifouling surfaces of interest ranging from water purification to biomedical applications.

KeyWords AITranslate

starshaped block copolymers polystyrene cores poly(ethylene glycol) arms antifouling coating oil emulsion filtration BSA Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01334

Chinese Library Classification Number:

Citation Information:

Star-shaped block copolymers (SPs) have shown promise as antifouling coating materials on water purification membranes. The unique architectural design of these SPs, composed of covalently linked hydrophobic core and hydrophilic arms, offers the flexibility of tailoring the core and/or arm compositions to achieve properties on demand. Here, variable sizes of SPs with increasingly hydrophobic polystyrene cores (PSCs) and longer hydrophilic poly(ethylene glycol) (PEG) arms were synthesized to evaluate their coatability on polysulfone ultrafiltration (PSF UF) membranes and to study the effect of the hydrophilic PEG arm lengths on the antifouling properties of SP-coated membranes. The oleophobicity evaluated from underwater hexadecane contact angle (CA) measurements of SP-coated membranes increased by approximately 3 times, leading to almost 7 times improvement in permeation flux during oil emulsion filtration. No flux recovery was observed for the pristine PSF membrane, whereas 100% flux recovery ratio (FRR) was achieved for SP-coated membranes. The filtration of bovine serum albumin (BSA) protein solution exhibited an improvement in the permeation flux by 2.7–8.9 times for SP-coated membranes. The FRR was only 64% for the pristine PSF membrane, as opposed to nearly 100% FRR for all SP-coated membranes. The stability of the SP coating was tested by rigorous washing with Tween 80 surfactant and three-cycle oil emulsion filtrations. Surfactant washing only removed the loosely bound extra layers of SP coating, leaving the surface-bound and pore-entrapped stable SP coating with remarkable antifouling properties. Since SP3 with the largest hydrophobic PSC showed much better performance, the effect of increasing its PEG arm length on the antifouling properties was studied further, and the largest size SP3 with the longest PEG arm was the optimum antifouling coating. This study provides insights into the design of block copolymer nanoarchitecture to develop antifouling surfaces of interest ranging from water purification to biomedical applications.

quote

GB/T 7714-2015 [1] Muhammad Amirul Islam, JaeYoung Cho, Khalid Azyat, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01334.
MLA [1] Muhammad Amirul Islam, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01334.
APA [1] Muhammad Amirul Islam, JaeYoung Cho, Khalid Azyat, Farshad Mohammadtabar, Feng Gao, Michael J. Serpe, Andrew J. Myles, YoungHye La, & Mohtada Sadrzadeh. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01334
IEEE [1] Muhammad Amirul Islam, JaeYoung Cho, Khalid Azyat, Farshad Mohammadtabar, Feng Gao, Michael J. Serpe, Andrew J. Myles, YoungHye La, and Mohtada Sadrzadeh, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01334. keywords: {starshaped block copolymers;polystyrene cores;poly(ethylene glycol) arms;antifouling coating;oil emulsion filtration;BSA;Show More}