One-Pot Preparation of Conducting Melamine/Polypyrrole/Magnetite Ferrosponge AITranslate

Institute of Macromolecular Chemistry; Tomas Bata University in Zlin; Tomas Bata University in Zlin; Tomas Bata University in Zlin;University of Chemistry and Technology Prague; J.E. Purkyně University; Charles University; Charles University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polypyrrole was deposited in situ on the macroporous open-cell melamine sponge by the oxidation of pyrrole with iron(III) chloride. The oxidant was used in excess, and the reaction mixture after the polymerization thus contained both iron(II) and iron(III) chlorides. These subsequently provided magnetite after treatment with ammonia solution. The conducting melamine/polypyrrole produced in the first step thus afforded melamine/polypyrrole/magnetite ferrosponge in the second. The composite sponge was characterized with respect to molecular structure by FTIR spectroscopy. The dependence of conductivity on the sponge compression is provided and magnetic properties have also been determined. The performance of sponge in electromagnetic radiation shielding in GHz region is demonstrated. While conducting polypyrrole afforded the radiation reflection, magnetite added the absorption component.

KeyWords AITranslate

Ferrosponge Melamine sponge Polypyrrole Magnetite Fe3O4 Electromagnetic radiation shielding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01331

Chinese Library Classification Number:

Citation Information:

Polypyrrole was deposited in situ on the macroporous open-cell melamine sponge by the oxidation of pyrrole with iron(III) chloride. The oxidant was used in excess, and the reaction mixture after the polymerization thus contained both iron(II) and iron(III) chlorides. These subsequently provided magnetite after treatment with ammonia solution. The conducting melamine/polypyrrole produced in the first step thus afforded melamine/polypyrrole/magnetite ferrosponge in the second. The composite sponge was characterized with respect to molecular structure by FTIR spectroscopy. The dependence of conductivity on the sponge compression is provided and magnetic properties have also been determined. The performance of sponge in electromagnetic radiation shielding in GHz region is demonstrated. While conducting polypyrrole afforded the radiation reflection, magnetite added the absorption component.

quote

GB/T 7714-2015 [1] Jaroslav Stejskal, Irina Sapurina, Jarmila Vilčáková, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01331.
MLA [1] Jaroslav Stejskal, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01331.
APA [1] Jaroslav Stejskal, Irina Sapurina, Jarmila Vilčáková, Marek Jurča, Miroslava Trchová, Zdeňka Kolská, Jan Prokeš, & Ivo Křivka. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01331
IEEE [1] Jaroslav Stejskal, Irina Sapurina, Jarmila Vilčáková, Marek Jurča, Miroslava Trchová, Zdeňka Kolská, Jan Prokeš, and Ivo Křivka, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01331. keywords: {Ferrosponge;Melamine sponge;Polypyrrole;Magnetite;Fe3O4;Electromagnetic radiation shielding}