Biobased, Biodegradable, Self-Healing Boronic Ester Vitrimers from Epoxidized Soybean Oil Acrylate AITranslate

Smart Materials, Istituto Italiano di Tecnologia; Université Côte d’Azur CNRS;Smart Materials, Istituto Italiano di Tecnologia;Materials Characterization Facility, Istituto Italiano di Tecnologia;Smart Materials, Istituto Italiano di Tecnologia;Smart Materials, Istituto Italiano di Tecnologia;Smart Materials, Istituto Italiano di Tecnologia
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The global production of thermosets has been increasing in recent years causing rapid consumption of fossil-based feedstocks and contributing to the plastic waste accumulation in the environment, especially because they cannot be easily reprocessed or recycled at the end of their lifetime. These drawbacks can only be overcome with the development of environmentally friendly, recyclable thermosets from renewable resources. For this reason, we present a facile way to produce a biobased reprocessable thermoset, a vitrimer, by thiol-acrylate coupling between epoxidized soybean oil acrylate and a diboronic ester dithiol dynamic cross-linker. The synthesis of the cross-linker and all the processes for the production of the vitrimer has been done following green chemistry principles. The developed vitrimer material can be reprocessed multiple times like a thermoplastic, without compromising its mechanical properties. Moreover, it can be conveniently recycled by reversible hydrolysis in 90% ethanol and subsequent solvent evaporation, regenerating the original vitrimer. An important advantage of the developed material, especially regarding its applications, is that it is able to self-repair mechanical abrasion-related defects, like scratches and cuts, at room temperature, thanks to the low glass transition temperature and rapid boronic ester exchange, which enables it to demonstrate great potential as a self-healing coating. In case of an accidental release into the environment, it is able to biodegrade, solving the problem of waste accumulation.

KeyWords AITranslate

biobased biodegradable vitrimers reprocessable thermoset dynamic crosslinks selfhealing boronic esters epoxidized Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01335

Chinese Library Classification Number:

Citation Information:

The global production of thermosets has been increasing in recent years causing rapid consumption of fossil-based feedstocks and contributing to the plastic waste accumulation in the environment, especially because they cannot be easily reprocessed or recycled at the end of their lifetime. These drawbacks can only be overcome with the development of environmentally friendly, recyclable thermosets from renewable resources. For this reason, we present a facile way to produce a biobased reprocessable thermoset, a vitrimer, by thiol-acrylate coupling between epoxidized soybean oil acrylate and a diboronic ester dithiol dynamic cross-linker. The synthesis of the cross-linker and all the processes for the production of the vitrimer has been done following green chemistry principles. The developed vitrimer material can be reprocessed multiple times like a thermoplastic, without compromising its mechanical properties. Moreover, it can be conveniently recycled by reversible hydrolysis in 90% ethanol and subsequent solvent evaporation, regenerating the original vitrimer. An important advantage of the developed material, especially regarding its applications, is that it is able to self-repair mechanical abrasion-related defects, like scratches and cuts, at room temperature, thanks to the low glass transition temperature and rapid boronic ester exchange, which enables it to demonstrate great potential as a self-healing coating. In case of an accidental release into the environment, it is able to biodegrade, solving the problem of waste accumulation.

quote

GB/T 7714-2015 [1] Arkadiusz Zych, Jonathan Tellers, Laura Bertolacci, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01335.
MLA [1] Arkadiusz Zych, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01335.
APA [1] Arkadiusz Zych, Jonathan Tellers, Laura Bertolacci, Luca Ceseracciu, Lara Marini, Giorgio Mancini, & Athanassia Athanassiou. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01335
IEEE [1] Arkadiusz Zych, Jonathan Tellers, Laura Bertolacci, Luca Ceseracciu, Lara Marini, Giorgio Mancini, and Athanassia Athanassiou, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01335. keywords: {biobased;biodegradable vitrimers;reprocessable thermoset;dynamic crosslinks;selfhealing;boronic esters;epoxidized;Show More}