Abstract AITranslate

The concentration of nucleating agent (NA) and flow fields are both important factors affecting the crystalline behavior and final properties of semicrystalline polymers. In this work, the concentration effect of N,N′-dicyclohexylterephthalamide (DCHT), an effective β-NA for isotactic polypropylene (iPP), on the shear-induced crystallization of iPP was investigated by comparing the crystallization temperatures (Tcs) of iPP/DCHT under unsheared, shear-unrelaxed, and relaxed conditions via rheological measurement. For iPP with an extremely low concentration of 0.01 wt %, Tc greatly improved after shearing and distinctly reduced after relaxation of 30 min, which was similar to that of pure iPP. For iPP with moderate concentrations of 0.05–0.3 wt %, the Tc could still increase after shearing but remained nearly constant after relaxation. In this concentration range, the increment in Tc induced by shear gradually decreased with increasing concentration. Interestingly, for iPP with high concentrations of 0.5 and 1 wt %, the Tc hardly changed regardless of applying shear or relaxation. The results of Fourier transform infrared suggested that DCHT existed in different forms including “free” molecules only and the coexistence of “free” DCHT and the associated assembly in various iPP/DCHT samples, and polarized optical microscopy observation showed that the DCHT assembly exhibited diverse morphologies at different concentrations. Combining the roles of “free” DCHT molecules and the associated assembly with diverse morphology in the shear-induced crystallization of iPP, a possible mechanism explaining the effect of DCHT concentration was proposed and experimentally verified.

KeyWords AITranslate

isotactic polypropylene shearinduced crystallization concentration nucleating agent N N′dicyclohexylterephthalamide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01345

Chinese Library Classification Number:

Citation Information:

The concentration of nucleating agent (NA) and flow fields are both important factors affecting the crystalline behavior and final properties of semicrystalline polymers. In this work, the concentration effect of N,N′-dicyclohexylterephthalamide (DCHT), an effective β-NA for isotactic polypropylene (iPP), on the shear-induced crystallization of iPP was investigated by comparing the crystallization temperatures (Tcs) of iPP/DCHT under unsheared, shear-unrelaxed, and relaxed conditions via rheological measurement. For iPP with an extremely low concentration of 0.01 wt %, Tc greatly improved after shearing and distinctly reduced after relaxation of 30 min, which was similar to that of pure iPP. For iPP with moderate concentrations of 0.05–0.3 wt %, the Tc could still increase after shearing but remained nearly constant after relaxation. In this concentration range, the increment in Tc induced by shear gradually decreased with increasing concentration. Interestingly, for iPP with high concentrations of 0.5 and 1 wt %, the Tc hardly changed regardless of applying shear or relaxation. The results of Fourier transform infrared suggested that DCHT existed in different forms including “free” molecules only and the coexistence of “free” DCHT and the associated assembly in various iPP/DCHT samples, and polarized optical microscopy observation showed that the DCHT assembly exhibited diverse morphologies at different concentrations. Combining the roles of “free” DCHT molecules and the associated assembly with diverse morphology in the shear-induced crystallization of iPP, a possible mechanism explaining the effect of DCHT concentration was proposed and experimentally verified.

quote

GB/T 7714-2015 [1] Yang Yue, Xinxin Wang, Jiachun Feng. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01345.
MLA [1] Yang Yue, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01345.
APA [1] Yang Yue, Xinxin Wang, & Jiachun Feng. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01345
IEEE [1] Yang Yue, Xinxin Wang, and Jiachun Feng, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01345. keywords: {isotactic polypropylene;shearinduced crystallization;concentration;nucleating agent;N;N′dicyclohexylterephthalamide}