Research on Fluorine Content Control in Ta_2O_5 and Nb_2O_5 AITranslate
Abstract AITranslate
Ta2O5 and Nb2 O5 powders are prepared with tantalum solution and niobium solution as the raw material and by ammonia neutralization precipitation-washing-drying-calcination. Influences of wash water amount and calcining time on fluorine content of the product were studied. The results show that fluorine content in tantalum and niobium oxides increases after they are placed in hydrofluoric acid atmosphere for some time,and therefore their fluorine content can be controlled at 0.07% -0.12 %, meeting the application requirements of foreign fiber field for tantalum and niobium oxides.
KeyWords AITranslate
1屈乃琴,陈久录.Nb铌的应用现状与展望[J].世界有色金属,1998(11):16-19. 被引量:21
2王永跃.铌的应用与发展[J].稀有金属与硬质合金,1996,24(1):41-43. 被引量:10
3屈乃琴.钽铌及其合金与应用[J].稀有金属与硬质合金,1998,26(2):48-54. 被引量:29
4YS/T547-2007.高纯五氧化二钽[S].
5YS/T548-2007.高纯五氧化二铌[s].
6辛良佐.等.钽铌冶金[M].北京:冶金工业出版社,1982.
1Krumm.,N,阎道全.生产钽铌氧化物的一种新工艺[J].南方冶院科技,1991(1):58-63.
2潘万成.溶剂萃取法从钽铌废料中回收钽、铌[J].化学世界,1991,32(6):249-251. 被引量:1
3何季林,张宗国,徐忠亭.中国钽铌湿法冶金[J].稀有金属材料与工程,1998,27(1):9-14. 被引量:30
4王太伟,张学珍,王启滨.重铀酸铵产品除氟工艺研究[J].科技与生活,2010(24):117-117.
5普锐特冶金技术提供的两台板坯连铸机在宝钢湛江投入运行[J].冶金自动化,2016,40(1):81-81.
6谢中华,陈树茂,王文华,张秋和,赵会团,刘斌.球形钨粉的制备工艺研究[J].中国钨业,2009,24(4):40-42. 被引量:12
7张波,李春龙,姜茂发.熔分过程中铌、磷在渣铁两相间的分配比[J].东北大学学报:自然科学版,2014,35(7):983-986. 被引量:4
8李涛,李培玉,孙顺义.振动钢包下渣检测技术的应用[J].首钢科技,2006(4):32-33.
9陈宏.直接还原法在铌提取上的应用[J].宝钢技术,1998(5):26-29. 被引量:12
10穆林,丁智敏,姜鑫,魏国,沈峰满.含铌尾矿的直接还原研究[J].中国冶金,2010,20(4):41-45. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
Ta2O5 and Nb2 O5 powders are prepared with tantalum solution and niobium solution as the raw material and by ammonia neutralization precipitation-washing-drying-calcination. Influences of wash water amount and calcining time on fluorine content of the product were studied. The results show that fluorine content in tantalum and niobium oxides increases after they are placed in hydrofluoric acid atmosphere for some time,and therefore their fluorine content can be controlled at 0.07% -0.12 %, meeting the application requirements of foreign fiber field for tantalum and niobium oxides.
quote
| GB/T 7714-2015 | [1] YANG Ji-hong, KUANG Guo-zhen. Research on Fluorine Content Control in Ta_2O_5 and Nb_2O_5[J]. Rare Metals and Cemented Carbides, 2012(4): 10-12. |
| MLA | [1] YANG Ji-hong, and KUANG Guo-zhen. "Research on Fluorine Content Control in Ta_2O_5 and Nb_2O_5." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 10-12. |
| APA | [1] YANG Ji-hong, & KUANG Guo-zhen. (2012). Research on Fluorine Content Control in Ta_2O_5 and Nb_2O_5. Rare Metals and Cemented Carbides(4), 10-12. |
| IEEE | [1] YANG Ji-hong and KUANG Guo-zhen, "Research on Fluorine Content Control in Ta_2O_5 and Nb_2O_5," Rare Metals and Cemented Carbides, no. 4, pp. 10-12, 2012. keywords: {Ta2O5;Nb2O5;fluorine content control;fluorine absorption;HF} |