The Latest Development of Molten Salt Electrolysis Equipment Structures for Titanium and Ti Alloy Preparation AITranslate
Abstract AITranslate
Domestic and foreign molten-salt electrolysis device structures for preparing titanium and its alloys are introduced,and their latest development is summarized. The advantages and disadvantages of each electrolytic equipment are comparatively reviewed.
KeyWords AITranslate
1Kroll W J. The production of ductile titanium[J]. Trans Am Elec-trochem Soc, 1940,78 (1) : 35-37.
2Ginatta M V. Process for the Electrolytic Production of Metals[P]. US pat: 6074545, 2000-06-13.
3Chen G Z, Far Y D J, Farthing T W. Direct electrochemical reduction of titanium dioxide to titanium in molten calcium chloride[J]. Nature, 2000,407(1) : 361-364.
4Fray D J, Chen G Z. Reduction of titanium and other metal oxides using electrodeoxidation[J]. Materials and Technology, 2002,20(3) : 295-299.
5聂新苗,董凌燕,白晨光,陈登福,邱贵宝.TiO_2电解制取Ti的热力学研究[J].材料导报,2006,20(10):147-150. 被引量:6
6李颖君,王淑兰,钟和香,孙华.电化学还原TiO_2反应机理及电极电势的研究[J].有色金属,2003,55(4):68-70. 被引量:19
7Wang Shulan, Li Yingjun. Reaction mechanism of di rect electro-reduction of titanium dioxide in molten cal cium chloride[J]. Journal of Electroanalytieal Chemis try,2004,571:37-42.
8郭胜惠,彭金辉,张世敏,范兴祥,张利波.熔盐电解还原TiO_2制取海绵钛新技术研究[J].昆明理工大学学报:理工版,2004,29(4):50-52. 被引量:21
9彭金辉,范兴祥,郭胜惠,张利波,张世敏.二氧化钛直接电解提取钛短流程绿色新技术[J].稀有金属,2002,26(4):290-293. 被引量:23
10杜继红,奚正平,李晴宇,李争显,唐勇.电化学还原TiO_2制备金属钛及反应过程的研究[J].稀有金属材料与工程,2006,35(7):1045-1049. 被引量:22
1杨钢,田卫平,闫洪.2012年云南金属材料与加工年评[J].云南冶金,2013,42(2):67-80.
2张瑶.还原液位控制对海绵钛生产的影响研究[J].轻金属,2017(8):47-50. 被引量:1
1贺永东,陈德明,孙小涵,刘洪贵,陈艳华,周云英,赵亿坤.13t大型海绵钛反应器内部温度场模拟研究[J].特种铸造及有色合金,2021,41(8):956-960. 被引量:1
1唐德池,高圣勇,李永林.中间包温度场数值模拟研究[J].上海金属,2012,34(6):56-60. 被引量:2
2曹娜,朱苗勇.板坯连铸中间包内控流装置结构的优化[J].材料与冶金学报,2007,6(2):109-112. 被引量:6
3彭琦,沈巧珍,仇东丽,左都伟,王军.八流中间包内控流装置结构的数理研究[J].连铸,2009,34(2):5-8. 被引量:1
4陈伟鹏,任雁秋,魏祥瑞,计云萍,武文斐.非对称五流圆坯连铸中间包水模实验研究[J].炼钢,2007,23(3):41-44. 被引量:1
5连和平,张胜伟,郭永谦,杜亚伟,李安钢,刘国民.安钢LS70/1-R型钢包滑动水口系统的应用实践[J].时代报告:学术版,2011(8):145-145.
6专利[J].中国重型装备,2011(2):53-54.
7程彩霞,孙秀茹.导风装置在小型搅拌机上的应用[J].矿山机械,2005,33(10):130-130.
8岳所平,刘富庭,段建国.邯钢400m^2烧结机系统单辊破碎机BFT柔性传动装置结构分析[J].烧结球团,2005,30(1):17-19. 被引量:1
9张辉宜,徐德君.国内外连铸中间包等离子体加热装置及其应用现状[J].钢铁钒钛,1997,18(4):30-34. 被引量:1
10炉底冷却装置[J].有色冶金节能,2010(6):77-77.
Basic Information:
DOI:
Chinese Library Classification Number:TF111.522[冶金工程—冶金物理化学]
Citation Information:
Domestic and foreign molten-salt electrolysis device structures for preparing titanium and its alloys are introduced,and their latest development is summarized. The advantages and disadvantages of each electrolytic equipment are comparatively reviewed.
quote
| GB/T 7714-2015 | [1] LU Hui, MENG Jun, XIE Gang, et al. The Latest Development of Molten Salt Electrolysis Equipment Structures for Titanium and Ti Alloy Preparation[J]. Rare Metals and Cemented Carbides, 2012(4): 13-19. |
| MLA | [1] LU Hui, et al., "The Latest Development of Molten Salt Electrolysis Equipment Structures for Titanium and Ti Alloy Preparation." Rare Metals and Cemented Carbides, no. 4, 2012, pp. 13-19. |
| APA | [1] LU Hui, MENG Jun, XIE Gang, & XIE Hong-yan. (2012). The Latest Development of Molten Salt Electrolysis Equipment Structures for Titanium and Ti Alloy Preparation. Rare Metals and Cemented Carbides(4), 13-19. |
| IEEE | [1] LU Hui, MENG Jun, XIE Gang, and XIE Hong-yan, "The Latest Development of Molten Salt Electrolysis Equipment Structures for Titanium and Ti Alloy Preparation," Rare Metals and Cemented Carbides, no. 4, pp. 13-19, 2012. keywords: {titanium;titanium alloys;molten salt electrolysis;electrolytic equipment structure;the latest development} |