Microstructures and Mechanical Properties of TiB/Ti-55531 Composite Material with Hot-Rolling Deformation AITranslate

New Materials Research Department,AVIC Manufacture Technology Institute,Beijing 100024,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Titanium matrix composites,which can effectively combine the good plasticity of titanium alloy matrix with the high strength and high modulus characteristic of reinforcement phase by introducing an appropriate amount of hard reinforcement phase into titanium or titanium alloy,possess so many advantages such as high specific strength,high specific stiffness,excellent plasticity,and good corrosion resistance,demonstrating broad application prospects in aerospace filed. Melt casting method is widely used in the preparation of titanium matrix composites,that can realize the insitu self-generation of reinforcement phase through the chemical reactions between components,and maintain a good interfacial bonding between the reinforcement phase and alloy matrix,avoiding the adverse influence of oxide pollution in interface caused by external addition on its microstructures and mechanical properties. However,the microstructures of titanium matrix composites prepared by in-situ melt casting method is coarse and the distribution of reinforcement phases is uneven. Therefore,it is necessary to optimize the microstructure and morphology by combing thermal mechanical treatment such as forging,rolling and extrusion with heat treatment to achieve favorable matching of comprehensive mechanical properties. The literature indicated that the material was in three-dimensional compressive stress state during hot rolling deformation,which could utilize the good plasticity of alloy matrix and obtain a large amount of deformation. While the reinforcement phases could achieve relatively uniform distribution following the plastic flow of alloy matrix over a large rang. Recently,the researches on titanium matrix composites in the industry were mainly focused on α and α+β titanium alloys,and its microstructures and mechanical properties were mainly controlled by a single thermal mechanical treatment. There were few reports about near β titanium matrix composites,and the influence of hot rolling coupled forging thermal mechanical treatment on reinforcement phase distribution and microstructures and properties of titanium matrix composites was still unclear. Accordingly,the effects of hot-rolling deformation on microstructures,mechanical properties and work hardening rates of insitu 2%TiB/Ti-55531 (volume fraction)composite material forging stocks were investigated,which were obtained by vacuum consumable arc melting and near-isothermal thermal plastic deformation. The results showed that TiB enhanced phases were broken and distributed directly after hot-rolling deformation in α+β phase region and the fine acicular α phases dispersed in β phase matrix re-dissolve mostly,while the spherical and rod-like α phases precipitate,which resulted in the increase of plasticity and the decrease of strength and work hardening rate. After suffering the solute and aging heat treatment,the morphologies of TiB enhanced phases in the rolled TiB/Ti-55531 composite material microstructures changed little,and the spherical and rod-like α phases grewup and connected into mesh along the crystal boundary in the local area while the fine needle-like secondary α phases were precipitated which obviously optimized the strength and plasticity of rolled composite materials. Its tensile strength,yield strength,and elongation after fracture were 1444.3 MPa,1415.8 MPa and 10.3%,respectively,which achieved favorable matching of strength and plasticity. Otherwise,the annihilation of residual dislocations in TiB/Ti-55531 composite material microstructure was promoted by solute and aging heat treatment which resulted the significant reduce of initial work hardening rate and it was slower than Ti-55531 alloy matrix undergoing the same process program gradually and approaching 0 state quickly with the development of plastic deformation. Electron back-scattered diffraction (EBSD)characterization analysis and kernel average misorientation (KAM)statistical distribution of different pre-deformations indicated that the rolled TiB/Ti-55531 titanium composite material after solute and aging heat treatment had a higher geometric dislocation density than Ti-55531 alloy matrix under low plastic deformation,while it gradually decreased with the continuous plastic deformation and lower than Ti-55531 alloy matrix which was consistent with the variation of work hardening of TiB/Ti-55531 titanium composite material with plastic deformation as mentioned above.

KeyWords AITranslate

TiB/Ti-55531 forging stock hot-rolling microstructures mechanical properties work hardening rate

[1](吕维洁,郭相龙,王立强,覃继宁,张荻. 原位自生非连续增强钛基复合材料的研究进展 [J]. 航空材料学报,2014,34(4),139.)

W J Lv,X L Guo,L Q Wang,J N Qin,D Zhang. Progress on in-situ discontinuously reinforced titanium matrix composites [J]. Journal of Aeronautical Materials,2014,34(4):139.

[2](叶想平,李英雷,翁继东,蔡灵仓,刘仓理. 颗粒增强金属基复合材料的强化机理研究现状 [J]. 材料工程,2018,46(12):28.)

X P Ye,Y L Li,J D Weng,L C Cai,C L Liu. Research status on strengthening mechanism of particle-reinforced metal matrix composites [J]. Journal of Materials Engineering,2018,46(12):28.

[3]Jiao Y,Huang L J,Geng L. Progress on discontinuously reinforced titanium matrix composites [J]. Journal of Alloys Compounds,2018,767:1196.

[4](钟亮,付玉,曹召勋,王荫洋,徐永东. (Ti5Si3+TiBw)/TC11复合材料力学性能与摩擦学性能 [J]. 有色金属工程,2023,13(1):22.)

L Zhong,Y Fu,Z X Cao,Y Y Wang,Y D Xu. Mechanical and tribological properties of (Ti5Si3+TiBw)/TC11 composites [J]. Nonferrous Metals Engineering,2023,13(2):22.

[5]Bermingham M J,McDonald S D,Nogita K,John D H,Dargusch M S. Effects of boron on microstructure in cast titanium alloys [J]. Scripta Materialia,2008,59(5):538.

[6]Morsi K,Patel V V. Processing and properties of titanium-titanium boride (TiBw)matrix composites-a review [J]. Journal of Materials Science,2007,42:2037.

[7](苗润,刘兵亮,任思雨,王立强,吕维洁. 颗粒增强钛基复合材料制备方法与组织性能研究进展 [J]. 精密成形工程,2021,13(3):25.)

R Miao,B L Liu,S Y Ren,L Q Wang,W J Lv. Research progress on preparation methods,microstructure and properties of particle reinforced titanium matrix composites [J]. Journal of netshape forming engineering,2021,13(3):25.

[8]Wang B,Zhang H B,Huang L J,He J L,Zhang Y F,Wang W. Evolution of microstructure and high temperature tensile properties of as-extruded TiBw reinforced near-titanium matrix composite subjected to heat treatment [J]. Science China-Technological Sciences,2018,61(9):1340.

[9](郑俊超. TiBw/TA15(Mo,Si)复合材料组织和力学性能研究 [D]. 哈尔滨:哈尔滨工业大学,2019. 1.)

J C Zheng. Microstructure and Mechanical Properties of TiBw/TA15(Mo,Si)Composites [D]. Harbin:Harbin Institute of Technology,2019. 1.

[10]Sun S Y,Lv W J. Effect of reinforcement contents on microstructure and mechanical properties of in-situ synthesized Ti matrix composite [J]. Rare Metal Materials and Engineering,2020,49(2):0398.

[11](黄孝余,唐斌,李金山. 钛基复合材料微观结构设计的研究进展 [J]. 铸造技术,2022,43(7):473.)

X Y Huang,B Tang,J S Li. Research progress on the microstructure design of titanium matrix composites [J]. Foundry Technology,2022,43(7):473.

[12](黄立国,庄伟彬,高志玉. Ti-6Al-4V-0.1B钛合金的热压缩变形行为 [J]. 稀有金属,2023,47(4):512.)

L G Huang,W B Zhuang,Z Y Gao. Compression deformation behavior of Ti-6Al-4V-0.1B titanium alloy at elevated temperature [J]. Chinese Journal of Rare Metals,2023,47(4):512.

[13](周琳,刘运玺,付明杰. 热处理对原位自生TiB/Ti-55531复合材料锻坯的组织性能影响研究 [J]. 热加工工艺,2023. doi:10.14158/j.cnki.1001-3814.20220090.)

L Zhou,Y X Liu,M J Fu. The influence of heat treatment on the microstructure and mechanical property of insitu TiB/Ti-55531 composite forging stocks [J]. Hot Working Technology,2023. doi:10.14158/j.cnki.1001-3814.20220090.

[14](周琳,刘运玺,付明杰. 原位自生TiB增强Ti-55531合金复合材料的组织与力学性能研究 [J]. 钛工业进展,2022,39(2):33.)

L Zhou,Y X Liu,M J Fu. The research on microstructure and mechanical properties of insitu TiB reinforced Ti-55531 alloy composites [J]. Titanium Industry Progress,2022,39(2):33.

[15]Hu H T,Huang L J,Geng L,Liu C,Wang B. Effects of extrusion on microstructure and tensile properties of 3D network structured TiBw/Ti60 composites fabricated by reaction hot pressing [J]. Journal of Alloys and Compounds,2014,582:569.

[16](项娟,韩远飞,乐建温,陈越,黄光法,来晓君,吕维洁. 颗粒增强钛基复合材料大塑性变形组织演变与性能 [J]. 稀有金属材料与工程,2020,49(3):901.)

J Xiang,Y F Han,J W Le,Y Chen,G F Huang,X J Lai,W J Lv. Microstructural evolution and properties of particle reinforced titanium matrix composites processed by severe plastic deformation [J]. Rare Metal Materials and Engineering,2020,49(3):901.

[17](王美晨,储双杰,梁高飞,张启飞,赵海燕,毛博. TC4钛合金热轧过程中组织演变和性能控制机理研究及展望 [J]. 塑性工程学报,2024,31(9):1.)

M C Wang,S J Chu,G F Liang,Q F Zhang,H Y Zhao,B Mao. Research and prospect on mechanism of tissue evolution and property control of TC4 titanium alloy during hot rolling process [J]. Journal of Plasticity Engineering,2024,31(9):1.

[18](黄陆军,耿林. 非连续增强钛基复合材料研究进展 [J]. 航空材料学报,2014,34(4):126.)

L J Huang,L Geng. Progress on discontinuously reinforced titanium matrix composites [J]. Journal of Aeronautical Materials,2014,34(4):126.

[19](韩远飞,邱培坤,孙相龙,冯家浩,王立强,吕维洁. 非连续颗粒增强钛基复合材料制备技术与研究进展 [J]. 航空制造技术,2016,59(15):62.)

Y F Han,P K Qiu,X L Sun,J H Feng,L Q Wang,W J Lv. Progress and fabrication technology on discontinuously reinforced titanium matrix composites [J]. Aeronautical Manufacturing Technology,2016,59(15):62.

[20](杨雪梅,闫学伟,史晓楠,郭鸿镇. 初始片层组织BT25y合金加工硬化行为研究 [J]. 稀有金属,2023,47(9):1213.)

X M Yang,X W Yan,X N Shi,H Z Guo. Work hardening behavior of BT25y alloy with initial lamellar microstructure [J]. Chinese Journal of Rare Metals, 2023,47(9):1213.

[21](黄朝文,赵永庆,辛社伟,周伟,李倩,曾卫东. 显微组织均匀性对片层Ti-55531合金高周疲劳裂纹萌生行为的影响 [J]. 稀有金属材料与工程,2017,46(3):663.)

C W Huang,Y Q Zhao,S W Xin,W Zhou,Q Li,W D Zeng. Influence of microstructure homogeneity on high-cycle fatigue crack initiation of Ti-55531 alloy with lamellar microstructure [J]. Rare Metal Materials and Engineering,2017,46(3):663.

[22](曾菁,李昌民,高蕾,张鑫,莫安军,栗文强,王晓巍,王德勇. 变形量对Ti-55531钛合金微观组织和力学性能的影响 [J]. 锻压技术,2024,49(6):249.)

J Zeng,C M Li,L Gao,X Zhang,A J Mo,W Q Li,X W Wang,D Y Wang. Influence of deformation amount on microstructure and mechanical properties for Ti-55531 titanium alloy [J]. Forging & Stamping Technology,2024,49(6):249.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23090007

Chinese Library Classification Number:TB333.1+2

Citation Information:

Titanium matrix composites,which can effectively combine the good plasticity of titanium alloy matrix with the high strength and high modulus characteristic of reinforcement phase by introducing an appropriate amount of hard reinforcement phase into titanium or titanium alloy,possess so many advantages such as high specific strength,high specific stiffness,excellent plasticity,and good corrosion resistance,demonstrating broad application prospects in aerospace filed. Melt casting method is widely used in the preparation of titanium matrix composites,that can realize the insitu self-generation of reinforcement phase through the chemical reactions between components,and maintain a good interfacial bonding between the reinforcement phase and alloy matrix,avoiding the adverse influence of oxide pollution in interface caused by external addition on its microstructures and mechanical properties. However,the microstructures of titanium matrix composites prepared by in-situ melt casting method is coarse and the distribution of reinforcement phases is uneven. Therefore,it is necessary to optimize the microstructure and morphology by combing thermal mechanical treatment such as forging,rolling and extrusion with heat treatment to achieve favorable matching of comprehensive mechanical properties. The literature indicated that the material was in three-dimensional compressive stress state during hot rolling deformation,which could utilize the good plasticity of alloy matrix and obtain a large amount of deformation. While the reinforcement phases could achieve relatively uniform distribution following the plastic flow of alloy matrix over a large rang. Recently,the researches on titanium matrix composites in the industry were mainly focused on α and α+β titanium alloys,and its microstructures and mechanical properties were mainly controlled by a single thermal mechanical treatment. There were few reports about near β titanium matrix composites,and the influence of hot rolling coupled forging thermal mechanical treatment on reinforcement phase distribution and microstructures and properties of titanium matrix composites was still unclear. Accordingly,the effects of hot-rolling deformation on microstructures,mechanical properties and work hardening rates of insitu 2%TiB/Ti-55531 (volume fraction)composite material forging stocks were investigated,which were obtained by vacuum consumable arc melting and near-isothermal thermal plastic deformation. The results showed that TiB enhanced phases were broken and distributed directly after hot-rolling deformation in α+β phase region and the fine acicular α phases dispersed in β phase matrix re-dissolve mostly,while the spherical and rod-like α phases precipitate,which resulted in the increase of plasticity and the decrease of strength and work hardening rate. After suffering the solute and aging heat treatment,the morphologies of TiB enhanced phases in the rolled TiB/Ti-55531 composite material microstructures changed little,and the spherical and rod-like α phases grewup and connected into mesh along the crystal boundary in the local area while the fine needle-like secondary α phases were precipitated which obviously optimized the strength and plasticity of rolled composite materials. Its tensile strength,yield strength,and elongation after fracture were 1444.3 MPa,1415.8 MPa and 10.3%,respectively,which achieved favorable matching of strength and plasticity. Otherwise,the annihilation of residual dislocations in TiB/Ti-55531 composite material microstructure was promoted by solute and aging heat treatment which resulted the significant reduce of initial work hardening rate and it was slower than Ti-55531 alloy matrix undergoing the same process program gradually and approaching 0 state quickly with the development of plastic deformation. Electron back-scattered diffraction (EBSD)characterization analysis and kernel average misorientation (KAM)statistical distribution of different pre-deformations indicated that the rolled TiB/Ti-55531 titanium composite material after solute and aging heat treatment had a higher geometric dislocation density than Ti-55531 alloy matrix under low plastic deformation,while it gradually decreased with the continuous plastic deformation and lower than Ti-55531 alloy matrix which was consistent with the variation of work hardening of TiB/Ti-55531 titanium composite material with plastic deformation as mentioned above.

quote

GB/T 7714-2015 [1] Lin Zhou, Yunxi Liu, Mingjie Fu, et al. Microstructures and Mechanical Properties of TiB/Ti-55531 Composite Material with Hot-Rolling Deformation[J]. Chinese Journal of Rare Metals, 2025, 49(6): 828-837. DOI:10.13373/j.cnki.cjrm.XY23090007.
MLA [1] Lin Zhou, et al., "Microstructures and Mechanical Properties of TiB/Ti-55531 Composite Material with Hot-Rolling Deformation." Chinese Journal of Rare Metals, vol. 49, no. 6, 2025, pp. 828-837, https://doi.org/10.13373/j.cnki.cjrm.XY23090007.
APA [1] Lin Zhou, Yunxi Liu, Mingjie Fu, Yanjin Xu, & Yuansong Zeng. (2025). Microstructures and Mechanical Properties of TiB/Ti-55531 Composite Material with Hot-Rolling Deformation. Chinese Journal of Rare Metals, 49(6), 828-837. https://doi.org/10.13373/j.cnki.cjrm.XY23090007
IEEE [1] Lin Zhou, Yunxi Liu, Mingjie Fu, Yanjin Xu, and Yuansong Zeng, "Microstructures and Mechanical Properties of TiB/Ti-55531 Composite Material with Hot-Rolling Deformation," Chinese Journal of Rare Metals, vol. 49, no. 6, pp. 828-837, 2025, doi: 10.13373/j.cnki.cjrm.XY23090007. keywords: {TiB/Ti-55531 forging stock;hot-rolling;microstructures;mechanical properties;work hardening rate}