daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Microstructure and Properties of JG4247 Alloy with Different Casting Process AITranslate

1.Shenyang Engine Research Institute,Aero Engine Corporation of China Shenyang Engine Research Institute,Shenyang 110000,China
2.High Temperature Materials Research Institute,Central Iron and Steel Research Institute,Beijing 100081,China
3.Gaona Aero Material Co.,Ltd.,Beijing 100081,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The grain structure and dendrite morphology have a significant influence on the mechanical properties of cast Ni-based superalloys. The morphology,size,and distribution of γ' precipitates are also key factors that determine the mechanical properties. The regulation and control of microstructure can be achieved by adjusting the casting process parameters,including the pouring temperature,shell temperature,and cooling rate. The viscosity of the melt decreases with increasing pouring temperature,which enhances the filling ability of the melt. Fine dendrite structures and uniformly distributed precipitates can be easily obtained when the shell temperature is low,which improves the strength,toughness,and fatigue performance of the castings. An increase in cooling rate can significantly refine the dendrites,carbides,borides,and eutectic γ-γ' phase. In addition,solute redistribution occurs during solidification due to its multi-component and non-equilibrium nature of the solidification process. Different casting processes will inevitably alter the distribution of solutes in the solid-liquid phase during the solidification process,thereby affecting the microstructure and properties of the alloy. In this study,a novel Ni-based superalloy JG4247 with high B content was investigated. The test alloy was prepared using vacuum induction melting (VIM). Three variables including pouring temperature,shell temperature,and cooling rate,were set in the pouring test. The pouring temperature was 1430 and 1460 ℃. The shell temperature was 850,950,and 1050 ℃,and the cooling rate was 8,17,and 27 ℃·min−1. Samples from different states of the casting rods were cut by wire-cutting for the observation of the grain morphologies and microstructure by optical microscope (OM)and scanning electron microscope (SEM). The effects of casting parameters on the grain size,dendrite spacing,the morphology of γ' phase,and the size of the eutectic γ-γ' phase were investigated. The relationship between the casting parameters and the microstructure of JG4247 alloy was established. The high-temperature tensile properties and stress-rupture properties of the alloy under different casting conditions were tested at 800 ℃ and 800 ℃/580 MPa,respectively. The results indicated that the size of grains and eutectic γ-γ' phases increased with the increasing pouring temperature and shell temperature,but decreased with higher cooling rate. The volume fraction of eutectic γ-γ' phases increased with the increase of pouring temperature and cooling rate,showed a trend of increasing and then decreasing with the increase of shell temperature,had a peak value when the mold shell temperature was 950 ℃. The volume fraction of borides and dendrite γ' phases increased with the increase of pouring temperature,showed a trend of first increasing and then decreasing with the increase of shell temperature,and decreased with the increase of cooling rate. The evolution of microstructures under different casting parameters was accompanied by significant changes in mechanical properties. The high-temperature mechanical properties of JG4247 alloy at 800 ℃ increased with the increase in pouring temperature and showed a trend of first increasing and then decreasing with the increase of shell temperature. The volume fraction of eutectic γ-γ' phases and the borides were the highest at 950 ℃. JG4247 alloy had the best tensile and stress-rupture properties at 950 ℃. The effect of cooling rate on microstructure was mainly reflected in the eutectic γ-γ' phase and dendriteγ' phase. When the cooling rate was 17 ℃·min−1,the grain size and the volume fraction of eutectic γ-γ' phase and dendritic γ' phase reached a reasonable level,thus JG4247 alloy had the longest stress-rupture life. By summarizing the effect of casting parameters on the microstructure and properties of the JG4247 alloy,the optimum casting parameters were determined to be:pouring temperature was 1460 ℃,shell temperature was 950 ℃,and cooling rate was 17 ℃·min−1. Under these conditions,the volume fraction of eutectic γ-γ' phase and dendritic γ' phase was the highest,the dendritic γ' phase possessed irregular petal-shaped morphology,which made the alloy had the best high-temperature mechanical properties. The study provided significant data for controlling the solidified microstructure of JG4247 alloy.

KeyWords AITranslate

casting process microstructure high-temperature mechanical property JG4247 alloy

[1](丁雨田,闫康,马元俊,高钰璧,陈建军,王兴茂. 一种新型Ni-Cr-Co基变形高温合金的均匀化工艺 [J]. 稀有金属,2023,47(10):1342.)

Y T Ding,K Yan,Y J Ma,Y B Gao,J J Chen,X M Wang. Homogenization of a new-type Ni-Cr-Co based wrought superalloy [J]. Chinese Journal of Rare Metals,2023,47(10):1342.

[2]Long F,Yoo Y S,Jo C Y,S M Seo,Song Y S,Jin T,Hu Z Q. Formation of η and σ phase in three polycrystalline superalloys and their impact on tensile properties [J]. Materials Science and Engineering:A,2009,527(1-2):361.

[3]Sajjadi S A,Zebarjad S M,Guthrie R I L,Isac M. Microstructure evolution of high-performance Ni-base superalloy GTD-111 with heat treatment parameters [J]. Journal of Materials Processing Technology,2006,175(1-3):376.

[4](张家郡,康慧君,李龙健,李仁庚,刘志锋,王同敏. Cu-Cr-Co-Ti合金微观组织和高温性能研究 [J]. 铜业工程,2023,(3):23.)

J J Zhang,H J Kang,L J Li,R G Li,Z F Liu,T M Wang. Microstructure and elevated-temperature properties of Cu-Cr-Co-Ti alloy [J]. Copper Engineering,2023,(3):23.

[5](袁彩霞,李瑞宾,孙元,张金汉,卜宪航,陈振斌. 保温时间对Zn脆化镍基单晶高温合金中组织演变的影响 [J]. 稀有金属,2024,48(11):1529.)

C X Yuan,R B Li,Y Sun,J H Zhang,X H Bu,Z B Chen. Microstructure evolution in Zn embrittlement nickel-based single crystal superalloys with different holding time [J]. Chinese Journal of Rare Metals,2024,48(11):1529.

[6](徐博. 浇注工艺对熔模精铸K417G合金显微组织和持久性能的影响 [D]. 哈尔滨:哈尔滨工业大学,2017. 49.)

B Xu. Effect of Pouring Process on Microstructure and Endurance Mechanical Properties of Investment Casting K417G Alloy [D]. Harbin:Harbin Engineering University,2017. 49.

[7](韦林,曹夕,王振江,孙士杰,柴宏宇,盛乃成,侯桂臣,康涌,王标. 浇注工艺对K416B合金组织和持久性能的影响 [J]. 特种铸造及有色合金,2023,42(8):979.)

L Wei,X Cao,Z J Wang,S J Sun,H Y Chai,N C Sheng,G C Hou,Y Kang,B Wang. Effect of pouring process on microstructure and endurance mechanical properties of investment casting K416B alloy [J]. Special Casting & Nonferrous Alloys,2023,42(8):979.

[8](吴晓娟,冯文刚,倪伟,屠晓林. 一种复杂薄壁件的熔模铸造工艺研究 [J]. 特种铸造及有色合金,2015,35(3):292.)

X J Wu,W G Feng,W Ni,X L Tu. Investment casting a complex thin-walled parts [J]. Special Casting & Nonferrous Alloys,2015,35(3):292.

[9](王春钢,孙长波,夏鹄翔,何金达,焦军红. 浇注工艺对Ni3Al基高温合金组织和性能的影响研究 [J]. 铸造,2023,71(11):1353.)

C G Wang,C B Sun,H X Xia,J D He,J H Jiao. Effect of casting process on microstructure and properties of a Ni3Al based superalloy [J]. China Foundry,2023,71(11):1353.

[10]Czeppe T,Wierzbicka-Miernik A,Sypien A,Garzel G,Goral A,Litynska-Dobrzynska L,Kopyto M,Przybyło W. Effects of Ti and high cooling rate on the phase equilibria and properties of Ni3(Al,V)alloys [J]. Journal of Materials Engineering and Performance,2020,29:1502.

[11]Pan X L,Yu H Y,Tu G F,Sun W R,Hu Z Q. Effect of rare earth metals on solidification behaviour in nickel based superalloy [J]. Materials Science and Technology,2012,28(5):560.

[12](徐继坤,张军,介子奇,黄太文,刘林,傅恒志. 浇注温度和细化剂对K4169高温合金铸态组织的影响 [J]. 热加工工艺,2015,44(3):34.)

J K Xu,J Zhang,Z Q Jie,T W Huang,L Liu,H Z Fu. Effect of pouring temperature and refiners on casting microstructures of superalloy K4169 [J]. Hot Working Technology,2015,44(3):34.

[13](严志,王树森,邹伟,程陆凡,卢厚辰,仉凤江. 工艺参数对大尺寸K465镍基母合金锭中心缩孔的影响 [J]. 特种铸造及有色合金,2023,43(3):410.)

Z Yan,S S Wang,W Zou,L F Cheng,H C Lu,F J Zhang. Influence of processing parameters on shrinkage cavities in large-scale K465 nickel-based master alloy ingot [J]. Special Casting & Nonferrous Alloys,2023,43(3):410.

[14](杜旭初. 浇注工艺对 ZL205A 合金大型回转体铸件偏析缺陷的影响研究 [D]. 北京:清华大学,2016. 1.)

X C Du. Research on the Effect of Casting Process on Segregation Defects of ZL205A Alloy Large Axisymmetric Bodycasting [D]. Beijing:Tsinghua University,2016. 1.

[15](郑泽邦,旷野,赵盼娣,宋晓悦. 拉伸变形和热处理对GH4169镍基高温合金应变速率敏感性的影响 [J]. 锻压技术,2024,49(7):48.)

Z B Zheng,Y Kuang,P D Zhao,X Y Song. Effect of tensile deformation and heat treatment on strain rate sensitivity of nickel-based superalloy GH4169 [J]. Forging & Stamping Technology,2024,49(7):48.

[16](王攀智,龚忠兴,张正,孙青,杨明. 航空发动机用Haynes242高温合金热变形行为 [J]. 有色金属工程,2023,13(2):40.)

P Z Wang,Z X Gong,Z Zhang,Q Sun,M Yang. Physical model of thermal deformation behavior of Haynes242 superalloy [J]. Nonferrous Metals Engineering,2023,13(2):40.

[17](赵志伟,李九霄,董安平,王旭彤,王迪,范敏灏,李子怿. 铸态GH4169高温合金的热变形行为及显微硬度变化 [J]. 塑性工程学报,2024,31(10):176.)

Z W Zhao,J X Li,A P Dong,X T Wang,D Wang,M H Fan,Z Y Li. Thermal deformation behavior and microhardness variation of as-cast GH4169 high temperature alloy [J]. Journal of Plasticity Engineering,2024,31(10):176.

[18]Shi X,Duan S C,Yang W S,Guo H J,Guo J. Effect of cooling rate on microsegregation during solidification of superalloy INCONEL 718 under slow-cooled conditions [J]. Metallurgical and Materials Transactions B,2018,49:1883.

[19](刘子禹,仉凤江,荀淑玲,谢君,舒德龙. 精炼及浇注温度对K417G镍基高温合金组织及持久性能的影响 [J]. 铸造,2022,70(12):1417.)

Z Y Liu,F J Zhang,S L Xun,J Xie,D L Shu. Influence of refining and pouring temperature on microstructures and stress rupture properities of K417G nickel-based superalloy [J]. China Foundry,2022,70(12):1417.

[20](熊继春,李嘉荣,韩梅,刘世忠. 浇注温度对DD6单晶高温合金凝固组织的影响 [J]. 材料工程,2009,(2):43.)

J C Xiong,J R Li,M Han,S Z Liu. Effects of pouring temperature on the solidification microstructure of single crystal superalloy DD6 [J]. Materials Engineering,2009,(2):43.

[21](严志,王振江,桑志茹,仉凤江,侯桂臣,谢君,于金江. 浇注温度对K465合金组织与力学性能的影响 [J]. 特种铸造及有色合金,2022,41(8):1001.)

Z Yan,Z J Wang,Z R Sang,F J Zhang,G C Hou,J Xie,J J Yu. Effects of pouring temperature on microstructure and mechanical properties of K465 alloy [J]. Special Casting & Nonferrous Alloys,2022,41(8):1001.

[22](詹洪飞,黄凯,宋伟伟,唐超,安腾,史维生. 冷却速度对GH4710合金凝固过程偏析行为的影响 [J]. 热加工工艺,2020,49(1):37.)

H F Zhan,K Huang,W W Song,C Tang,T An,W S Shi. Effects of cooling rate on element segregation behaviors of GH4710 alloy during solidification process [J]. Hot Working Technology,2022,49(1):37.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23090012

Chinese Library Classification Number:TG444

Citation Information:

The grain structure and dendrite morphology have a significant influence on the mechanical properties of cast Ni-based superalloys. The morphology,size,and distribution of γ' precipitates are also key factors that determine the mechanical properties. The regulation and control of microstructure can be achieved by adjusting the casting process parameters,including the pouring temperature,shell temperature,and cooling rate. The viscosity of the melt decreases with increasing pouring temperature,which enhances the filling ability of the melt. Fine dendrite structures and uniformly distributed precipitates can be easily obtained when the shell temperature is low,which improves the strength,toughness,and fatigue performance of the castings. An increase in cooling rate can significantly refine the dendrites,carbides,borides,and eutectic γ-γ' phase. In addition,solute redistribution occurs during solidification due to its multi-component and non-equilibrium nature of the solidification process. Different casting processes will inevitably alter the distribution of solutes in the solid-liquid phase during the solidification process,thereby affecting the microstructure and properties of the alloy. In this study,a novel Ni-based superalloy JG4247 with high B content was investigated. The test alloy was prepared using vacuum induction melting (VIM). Three variables including pouring temperature,shell temperature,and cooling rate,were set in the pouring test. The pouring temperature was 1430 and 1460 ℃. The shell temperature was 850,950,and 1050 ℃,and the cooling rate was 8,17,and 27 ℃·min−1. Samples from different states of the casting rods were cut by wire-cutting for the observation of the grain morphologies and microstructure by optical microscope (OM)and scanning electron microscope (SEM). The effects of casting parameters on the grain size,dendrite spacing,the morphology of γ' phase,and the size of the eutectic γ-γ' phase were investigated. The relationship between the casting parameters and the microstructure of JG4247 alloy was established. The high-temperature tensile properties and stress-rupture properties of the alloy under different casting conditions were tested at 800 ℃ and 800 ℃/580 MPa,respectively. The results indicated that the size of grains and eutectic γ-γ' phases increased with the increasing pouring temperature and shell temperature,but decreased with higher cooling rate. The volume fraction of eutectic γ-γ' phases increased with the increase of pouring temperature and cooling rate,showed a trend of increasing and then decreasing with the increase of shell temperature,had a peak value when the mold shell temperature was 950 ℃. The volume fraction of borides and dendrite γ' phases increased with the increase of pouring temperature,showed a trend of first increasing and then decreasing with the increase of shell temperature,and decreased with the increase of cooling rate. The evolution of microstructures under different casting parameters was accompanied by significant changes in mechanical properties. The high-temperature mechanical properties of JG4247 alloy at 800 ℃ increased with the increase in pouring temperature and showed a trend of first increasing and then decreasing with the increase of shell temperature. The volume fraction of eutectic γ-γ' phases and the borides were the highest at 950 ℃. JG4247 alloy had the best tensile and stress-rupture properties at 950 ℃. The effect of cooling rate on microstructure was mainly reflected in the eutectic γ-γ' phase and dendriteγ' phase. When the cooling rate was 17 ℃·min−1,the grain size and the volume fraction of eutectic γ-γ' phase and dendritic γ' phase reached a reasonable level,thus JG4247 alloy had the longest stress-rupture life. By summarizing the effect of casting parameters on the microstructure and properties of the JG4247 alloy,the optimum casting parameters were determined to be:pouring temperature was 1460 ℃,shell temperature was 950 ℃,and cooling rate was 17 ℃·min−1. Under these conditions,the volume fraction of eutectic γ-γ' phase and dendritic γ' phase was the highest,the dendritic γ' phase possessed irregular petal-shaped morphology,which made the alloy had the best high-temperature mechanical properties. The study provided significant data for controlling the solidified microstructure of JG4247 alloy.

quote

GB/T 7714-2015 [1] Yuefeng Cui, Shaoli Han, Shangping Li, et al. Microstructure and Properties of JG4247 Alloy with Different Casting Process[J]. Chinese Journal of Rare Metals, 2025, 49(6): 962-970. DOI:10.13373/j.cnki.cjrm.XY23090012.
MLA [1] Yuefeng Cui, et al., "Microstructure and Properties of JG4247 Alloy with Different Casting Process." Chinese Journal of Rare Metals, vol. 49, no. 6, 2025, pp. 962-970, https://doi.org/10.13373/j.cnki.cjrm.XY23090012.
APA [1] Yuefeng Cui, Shaoli Han, Shangping Li, Jie Hou, & Chen Ling. (2025). Microstructure and Properties of JG4247 Alloy with Different Casting Process. Chinese Journal of Rare Metals, 49(6), 962-970. https://doi.org/10.13373/j.cnki.cjrm.XY23090012
IEEE [1] Yuefeng Cui, Shaoli Han, Shangping Li, Jie Hou, and Chen Ling, "Microstructure and Properties of JG4247 Alloy with Different Casting Process," Chinese Journal of Rare Metals, vol. 49, no. 6, pp. 962-970, 2025, doi: 10.13373/j.cnki.cjrm.XY23090012. keywords: {casting process;microstructure;high-temperature mechanical property;JG4247 alloy}