Abstract AITranslate

In view of abnormality of about 200 ℃ temperature drop in the bottom of the sintering box during pressure sintering (after argon charged into the furnace) with imported pressure sintering furnace, analysis is made of the cause of the fault,and technical upgrading option is given together with a serials of specific measures. The performance of the upgraded equipment indicated that the partial temperature drop can be controlled within 5 ℃ with a great improvement in ultra-temperature safety of the furnace wall.

KeyWords AITranslate

pressure sintering pressure sintering furnace sintering temperature technical upgrading

1胡耀新,娄述琪.硬质合金专业设备开发应用的思考[J].中国钨业,1999,14(5):220-223. 被引量:4

2陈跃辉,郭淳,罗毅.ZYS-50/50/130压力烧结炉设备的研制[J].稀有金属与硬质合金,2008,36(1):42-45. 被引量:5

1彭志坚,邓斌.LTCC专用烧结炉的研制[J].电子工业专用设备,2009,38(10):16-21. 被引量:1

2范昆.硬质合金压力烧结炉H_2脱蜡停电自动充气保护装置设计[J].机械工程师,2018(3):61-62.

1颜秀文,张建国,邓斌,袁云华,潘喜成,杨毓彬.LTCC专用烧结炉的应用及发展趋势[J].电子工业专用设备,2012,41(2):1-4.

1崔佳娜.我国硬质合金烧结设备的发展[J].中国钨业,2009,24(6):47-49. 被引量:3

2陈跃辉,丁文.WinCC组态软件在压力烧结炉监控系统中的应用[J].设备管理与维修,2009(4):33-36. 被引量:3

3陈跃辉,郭淳,罗毅.ZYS-50/50/130压力烧结炉设备的研制[J].稀有金属与硬质合金,2008,36(1):42-45. 被引量:5

4陈祎,刘余庆.基于热平衡原理的硬质合金压力烧结炉最佳加热功率的研究[J].工业加热,2005,34(5):29-32. 被引量:3

5压力烧结炉[J].军民两用技术与产品,2013(11):49-50.

6储鸿文,吴伊凡.杭钢转炉厂1号连铸机改造的技术特点[J].浙江冶金,1999(2):17-19.

7杨迅.硬质合金真空/压力烧结炉差压脱蜡的研究[J].装备制造技术,2013(3):249-251. 被引量:3

8蔡永成.基于炉控片矫顽磁力测量方法评价PVA压力烧结炉温度场均匀性[J].工业加热,2007,36(6):57-59. 被引量:2

9王宏志.走在世界压力烧结炉市场的最前沿——PVA TePla AG公司全球最大的压力烧结炉制造商[J].硬质合金,2008,25(3):198-198.

10徐爱民.传统法炼铅技改方案的探讨[J].有色金属:冶炼部分,1997(1):2-6. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TF806.1[冶金工程—有色金属冶金]

Citation Information:

In view of abnormality of about 200 ℃ temperature drop in the bottom of the sintering box during pressure sintering (after argon charged into the furnace) with imported pressure sintering furnace, analysis is made of the cause of the fault,and technical upgrading option is given together with a serials of specific measures. The performance of the upgraded equipment indicated that the partial temperature drop can be controlled within 5 ℃ with a great improvement in ultra-temperature safety of the furnace wall.

quote

GB/T 7714-2015 [1] CHEN Yue-hui. Technical Upgrading of Imported Pressure Sintering Furnace[J]. Rare Metals and Cemented Carbides, 2008(2): 37-38.
MLA [1] CHEN Yue-hui. "Technical Upgrading of Imported Pressure Sintering Furnace." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 37-38.
APA [1] CHEN Yue-hui. (2008). Technical Upgrading of Imported Pressure Sintering Furnace. Rare Metals and Cemented Carbides(2), 37-38.
IEEE [1] CHEN Yue-hui, "Technical Upgrading of Imported Pressure Sintering Furnace," Rare Metals and Cemented Carbides, no. 2, pp. 37-38, 2008. keywords: {pressure sintering;pressure sintering furnace;sintering temperature;technical upgrading}