Study on Nano-SiO_2 Surface Modification and Dispersity AITranslate
Abstract AITranslate
Surface lipophilic modification of nano-SiO2 in ITO film with dichlorodimethylsilane is made. The dispersity of the modified nano-SiO2 in acrylic resin and its effect on the dispersion system is investigated. The results show that the modified nano-SiO2 has a uniform particle size distribution. The transmittance of the system with 2%-3% SiO2 ,which is dispersed by high speed first and then ultrasonic wave,is the minimum and its stability is the highest.
KeyWords AITranslate
1单薇,廖明义.纳米SiO_2的表面处理及其在聚合物基纳米复合材料中的应用进展[J].高分子通报,2006(3):1-9. 被引量:44
2Igarashi K, Tajiri K, Tanemura S, et al. Network structure of fine silica particles[J]. Z Phys D, 1997,40 : 562- 565.
3Halfpenny D R, Kane D M, Lamb R N, et al. Surface modification of silica with ultraviolet laser radiation[J]. Appl Phys A,2000,71:147-151.
4陈国新,赵石林.纳米Sio_2/丙烯酸UV屏蔽透明涂料的制备及性能研究[J].涂料工业,2003,33(10):7-9. 被引量:11
5马文有,田秋,曹茂盛,高正娟,陈玉金,朱静.纳米颗粒分散技术研究进展——分散方法与机理(1)[J].中国粉体技术,2002,8(3):28-31. 被引量:77
1郑文芝,陈砺,王红林,陈姚.疏水性二氧化硅气凝胶的合成及表征[J].硅酸盐通报,2008,27(6):1151-1155. 被引量:4
2闫勋栋,何德民,潘娜娜,潘艳秋.陶瓷膜表面接枝改性及其在膜蒸馏过程中的应用[J].功能材料,2015,46(19):19028-19032. 被引量:2
3沈浩,蒋孝杰,周燕,邓诗峰,杜磊,夏红娟,黄发荣.锌粉催化合成含硅芳炔树脂[J].过程工程学报,2014,14(2):329-334. 被引量:7
4郑振荣,顾振亚,霍瑞亭,叶永红,张之秋.化学浴沉积法制备防污自洁聚偏氟乙烯膜[J].高分子材料科学与工程,2010,26(6):126-129. 被引量:4
5陈兴隆,秦积舜,李治平.表面亲油纳米二氧化硅改变岩石表面润湿性的研究[J].油田化学,2005,22(4):328-331. 被引量:14
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
Surface lipophilic modification of nano-SiO2 in ITO film with dichlorodimethylsilane is made. The dispersity of the modified nano-SiO2 in acrylic resin and its effect on the dispersion system is investigated. The results show that the modified nano-SiO2 has a uniform particle size distribution. The transmittance of the system with 2%-3% SiO2 ,which is dispersed by high speed first and then ultrasonic wave,is the minimum and its stability is the highest.
quote
| GB/T 7714-2015 | [1] FU Xin, DUAN Xue-chen. Study on Nano-SiO_2 Surface Modification and Dispersity[J]. Rare Metals and Cemented Carbides, 2008(2): 33-36. |
| MLA | [1] FU Xin, and DUAN Xue-chen. "Study on Nano-SiO_2 Surface Modification and Dispersity." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 33-36. |
| APA | [1] FU Xin, & DUAN Xue-chen. (2008). Study on Nano-SiO_2 Surface Modification and Dispersity. Rare Metals and Cemented Carbides(2), 33-36. |
| IEEE | [1] FU Xin and DUAN Xue-chen, "Study on Nano-SiO_2 Surface Modification and Dispersity," Rare Metals and Cemented Carbides, no. 2, pp. 33-36, 2008. keywords: {nano-SiO2;ITO film;surface modification;hydrophilicity;lipophilicity} |