Effects of Alloying on the Microstructure and High Temperature Oxidation Resistance of Nb-Ti-Si-based Alloys AITranslate

National Key Laboratory of Northwestern Polytechnical University Coormination Technology;National Key Laboratory of Northwestern Polytechnical University Coormination Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of multi-element alloying of Nb-Ti-Si-based alloys is described. The effects of alloying on the improvement of microstructure and oxidation resistance of Nb-Ti-Si-based alloys are reviewed.

KeyWords AITranslate

Nb-Ti-Si-based alloy alloying microstructure high temperature oxidation resistance

1Ma C L, Li J G, Tan Y, et al. Microstructual and mechanical properties of Nb/Nb5 Sis in situ composites in Nb-Mo-Si and Nb-W-Si systems[J]. Materials Science and Engineering A, 2004,386 : 375-383.

2Bewlay B P,Jackson M R, Lipsitt H A. The balance of mechanical and environmental properties of a multielement niobium-niobium silicide-based in situ composite [J]. Metallurgical and Materials Transactions A, 1996,27A:3801-3808.

3Bewlay B P,Jackson M R,Zhao J C,et al. A review in very high temperature Nb-silieide-based eomposites[J]. Metall Mater Trans A,2003,34A:2043-2052.

4Kim Won-Yong, Tanaka Hisao, Kasama Akio, et al. Mi crostructual and room temperature fracture and room temperature toughness of Nbss/NbsSi3 in situ composites[J]. Intermetallics, 2001,9 : 872-834.

5Murayama Yonosuke, Hanada Shuji. High temperature strength,fracture toughness and oxidation resistance of Nb-Si-Al-Ti multiphase alloys, [J]. Science and Technology of Andvanced Materials, 2002,3 : 145-156.

6Geng Jie, Tsakiropoulos. A study of microstructure and oxidation of Nb-Si-Cr-Al-Mo in situ composites alloyed with Ti, Hf, Sn[J]. Intermetallics, 2007,15 : 382-395.

7Zelenitas K, Tsakiropoulos P. Study of the role of Al and Cr addition in the microstructure of Nb-Ti-Si in situ composites[J]. Intermetallics ,2005,13 : 1079-1095.

8Zelenitas K,Tsakiropoulos P. Study of the role of Ta and Cr addition in the microstructure of Nb-Ti-Si-Al in situ composites[J]. Intermetallics, 2006,14 : 639-659.

9Geng Jie,Tsakiropoulos Panos, Shao Guosheng. A study of the effect of Hf and Sn addition on the microstructure of Nbss/NbsSi3 based in situ composites[J]. Intermetallics, 2007,15 : 69-76.

10Kim Won-Yong, Yeo In-Dong, Ra Tae-Yeub, et al. Effect of V addition on microstructure and mechanical property in the Nb-Si alloy system[J]. Journal of Alloy and Compounds, 2004,364 : 186-192.

1台元月,姜惠仁,李宁,马文帅,宋旻键.SiO_2增强铌基合金高温抗氧化性的相关研究[J].航空制造技术,2010,0(4):76-78. 被引量:2

2程欢欢,郭喜平.铌-硅基超高温合金定向凝固及相组成的热力学研究进展[J].材料导报,2011,25(17):110-115. 被引量:1

3周家蕤,沙江波.Fe元素对Nb-16Si原位复合材料显微组织及室温力学性能的影响[J].复合材料学报,2011,28(6):172-179. 被引量:1

4万松峰,许春耀,吴锦城.基板偏压对溅镀AlCrNbSiTiV高熵合金氮化物薄膜性能的影响[J].电镀与涂饰,2018,37(3):122-128. 被引量:6

5魏文庆,王宏伟,高增新,魏尊杰.Microstructure evolution of as-cast Nb-Ti-C alloys[J].中国有色金属学报:英文版,2009,19(S02):440-443. 被引量:1

1王雁利,杨海丽,吴晔康,徐宏,王心悦,冯策.脉冲频率对铌表面熔盐电沉积渗硅的影响[J].科学技术与工程,2015,35(36):47-51.

2褚楚,徐严谨,韩宝帅,孟宪宇,骆良顺,侯红亮,苏彦庆,郭景杰,傅恒志.电弧熔炼Nb-16Si-2Fe合金铸态组织及高温压缩行为[J].精密成形工程,2017,9(1):23-28.

3万松峰,许春耀,张钰乾.高熵合金AlCrNbSiTiV氮化物薄膜溅镀参数的优化[J].电镀与涂饰,2018,37(15):677-682. 被引量:2

4刘志伟,吴明昌,林宇璇.氮氩比对大功率脉冲磁控溅镀(AlCrNbSiTiV)N薄膜性能的影响[J].电镀与涂饰,2019,38(12):568-573. 被引量:2

5刘志伟,何靖国,林宇璇,张良超.高功率脉冲磁控溅射沉积(AlCrNbSiTiV)N薄膜提升刀具的切削性能[J].电镀与涂饰,2019,38(13):674-679. 被引量:3

6万松峰,陈永刚,丁佳伟.(AlCrNbSiTiV)N高熵合金氮化薄膜溅镀参数的灰关联分析优化[J].电镀与涂饰,2020,39(1):20-25.

7万松峰,丁佳伟.退火对磁控溅射AlCrNbSiTiV高熵合金氮化薄膜性能的影响[J].电镀与涂饰,2020,39(5):263-268. 被引量:4

8陈瑞润,陈德志,王琪,王墅,周哲丞,丁宏升,傅恒志.Nb-Si基超高温合金及其定向凝固工艺的研究进展[J].金属学报,2021,57(9):1141-1154. 被引量:1

9宋晓毓,王德志,吴壮志,段柏华,毕海莲,刘新利.爆炸焊接Nb/Q345R层状复合材料的热震性能研究[J].材料导报,2021,35(18):18131-18135.

10王东,XU Kai,WEI Boxin,WANG Yujin.Microstructure and Mechanical Properties of ZrC_(x)-NbC_(y)-Cu Composites by Reactive Infiltration at 1300℃[J].武汉理工大学学报:材料科学英文版,2023,38(1):52-58.

1王勇,郭喜平,张超峰,张平.电弧熔炼Nb-Ti-Si合金的组织和室温力学性能[J].特种铸造及有色合金,2010(6):556-561. 被引量:5

2王勇,郭喜平.凝固速率对Nb-Ti-Si基合金整体定向凝固组织及固/液界面形态的影响[J].金属学报,2010,46(4):506-512. 被引量:15

3严俊杰,郭喜平.热处理对定向凝固Nb-Ti-Si基合金组织及力学性能的影响(英文)[J].稀有金属材料与工程,2017,46(1):1-6. 被引量:1

4张平,郭喜平.Al对Nb-Ti-Si基合金表面Si-Al-Y_2O_3共渗层的影响[J].金属学报,2010,46(7):821-831. 被引量:9

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

The latest development of multi-element alloying of Nb-Ti-Si-based alloys is described. The effects of alloying on the improvement of microstructure and oxidation resistance of Nb-Ti-Si-based alloys are reviewed.

quote

GB/T 7714-2015 [1] GUO Jin-ming, GUO Xi-ping. Effects of Alloying on the Microstructure and High Temperature Oxidation Resistance of Nb-Ti-Si-based Alloys[J]. Rare Metals and Cemented Carbides, 2008(2): 39-43.
MLA [1] GUO Jin-ming, and GUO Xi-ping. "Effects of Alloying on the Microstructure and High Temperature Oxidation Resistance of Nb-Ti-Si-based Alloys." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 39-43.
APA [1] GUO Jin-ming, & GUO Xi-ping. (2008). Effects of Alloying on the Microstructure and High Temperature Oxidation Resistance of Nb-Ti-Si-based Alloys. Rare Metals and Cemented Carbides(2), 39-43.
IEEE [1] GUO Jin-ming and GUO Xi-ping, "Effects of Alloying on the Microstructure and High Temperature Oxidation Resistance of Nb-Ti-Si-based Alloys," Rare Metals and Cemented Carbides, no. 2, pp. 39-43, 2008. keywords: {Nb-Ti-Si-based alloy;alloying;microstructure;high temperature oxidation resistance}