Tensile Properties and Deformation Mechanism of Pure Rhenium at Room Temperature and Ultra-High Temperature AITranslate

1.School of Materials Science and Engineering,Northwestern Polytechnical University,Xi’an 710072,China
2.ATTL Advanced Materials Co.,Ltd.,Beijing 100094,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rhenium has high strain hardening index, tensile strength, elastic modulus and hardness, and has no ductile-brittle transition temperature. It is often used in metal-organic chemical vapor deposition (MOCVD) heaters and key components of engines. In order to meet its application in harsh ultra-high temperature service environments such as MOCVD heaters, this paper studied the tensile properties of pure rhenium (PM-Re) prepared by powder metallurgy at room temperature to 2000 ℃. The deformation mechanism of PM-Re was analyzed using scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), transmission electron microscopy (TEM), etc. The results showed that the room temperature tensile strength of PM-Re was 882 MPa. With the increase of temperature, the tensile strength of PM-Re decreased. At 2000 ℃, the tensile strength decreased to 112 MPa. The elongation after fracture of PM-Re at room temperature was 18%. In the temperature range of 1700–2000 ℃, the elongation after fracture was less than 10%. With the increase of temperature, the non-proportional elongation strength (Rp0.2) of PM-Re continuously decreased. At room temperature, Rp0.2 of PM-Re was 171 MPa, and at 1900 and 2000 ℃, it was only 17 and 6 MPa. The room temperature tensile fracture of PM-Re had both intergranular brittle fracture and transgranular fracture. Symmetrical structures along the fracture surface appeared on the grains where transgranular fracture occurred, and dislocation slip traces were found on the fracture surface. At high temperatures, a large number of lamellar structures, dimple-shaped fractures and "river" pattern characteristics appeared in the PM-Re specimens after tensile testing. It was found by EBSD characterization that the original PM-Re sample was composed of equiaxed grains. A large number of twins were produced after the sample was deformed at room temperature. There was a large local orientation difference inside the rhenium grains. The grain boundaries and twin boundaries showed a high local average misorientation (LAM) value. Dislocations were mainly distributed at the grain boundaries and interacted with the twin boundaries. With the increase of temperature, the degree of deformation of PM-Re increased, and the internal point defects and stress concentration areas increased, resulting in a gradual increase in the LAM value of PM-Re. Through the Schmidt factor map, it was found that the average Schmidt factor values of the cylindrical slip system and the conical slip system were the highest at high temperatures, and the non-basal slip system was the main slip system. The twin deformation traces in different directions on the same slip plane and the phenomenon of dislocation aggregation at the twin boundaries after tensile testing at room temperature were found by TEM, indicating that the twin and dislocation interacted, and the twin boundary would become an obstacle to dislocation movement. After tensile testing at 2000 ℃, subgrain boundaries formed by dislocation movement in the PM-Re body. The formation of subgrain boundaries could further hinder the dislocation slip, increase the deformation resistance of the material, and at the same time, the subgrain boundaries could coordinate the deformation between adjacent grains and effectively improve the uniform deformation ability of PM-Re. The above results showed that during the room temperature deformation process of PM-Re, twin deformation and dislocation slip coexisted. Twin deformation could improve the plasticity of rhenium, and dislocation cells and twin boundaries would hinder dislocation movement and thereby increase the work hardening rate of rhenium. The ultra-high temperature deformation process of PM-Re was dominated by dislocation slip, the non-basal slip system was the main slip system, and the basal slip system gradually opened at 2000 ℃.

KeyWords AITranslate

pure rhenium tensile property twin deformation dislocation motion

[1]Carlen J C, Bryskin B D. Rhenium-a unique rare metal [J].Materials and Manufacturing Processes, 1994, 9: 1087.

[2]Sims C T, Craighead C M, Jaffee R I. Physical and mechanical properties of rhenium [J].Journal of Metals, 1955: 168.

[3]Povarova K B, Tylkina M A. Properties and uses of rhenium [J].Byulleten' Tekhniko-Ekonomicheskoy Informatsii, 1963, 9: 7.

[4](吴王平, 江鹏, 华同曙. 难熔金属铼及其合金的研究进展 [J].金属功能材料, 2015, 22(2): 48.)

W P Wu, P Jiang, T S Hua. Research progress of refractory metalrhenium and its alloy [J].Meatallic Functional Meaterials, 2015, 22(2): 48.

[5](熊宁, 张莹莹, 邱玺, 冯波, 陈福鸽, 王广达. 电子束焊接钼铼合金组织和性能研究 [J].稀有金属, 2022, 46(9): 1172.)

N Xiong, Y Y Zhang, X Qiu, B Feng, F G Cheng, G D Wang. Microstructures and properties research of electron beam welded joints of molybdenum-rhenium alloys [J].Chinese Journal of Rare Metals, 2022, 46(9): 1172.

[6](程挺宇, 熊宁, 彭楷元, 杨海兵, 殷晶川. 铼及铼合金的应用现状及制造技术 [J].稀有金属材料与工程, 2009, 38(2): 373.)

T Y Cheng, N Xiong, K Y Peng, H B Yang, J C Yin. The application and preparation technology of rhenium and rhenium alloys [J].Rare Metal Materials and Engineering, 2009, 38(2): 373.

[7]Partridge P. The crystallography and deformation modes of hexagonal closepacked metals [J].Metall. Rev., 1967, 12 (1): 169.

[8]Naor A, Eliaz N, Gileadi E. Properties and applications of Re and its alloys [J].The Ammtiac Quarterly, 2010, 5(1): 11.

[9]Dobrzańska-Danikiewicz A D, Wolany W. A rhenium review-from discovery to novel applications [J].Archives of Materials Science and Engineering, 2016, 82: 70.

[10]Bryskin B D. Evaluation of properties and special features for high-temperature applications of rhenium [J].AIP Conference Proceedings, 1992, 246: 278.

[11]Zhang Y M. Electron beam physical vapor deposition method for rhenium components [J].Rare Metals Letters, 2003, 4: 20.

[12]Melvin L C. Materials property test results of rhenium[R]. CA: AIAA, 1995. 1.

[13]Biaglow J A. High temperature rhenium material properties[R].USA: AIAA, 1998. 1.

[14]Biaglow J A. Rhenium material properties[R].CA: AIAA, 1955. 1.

[15]Bryskin B D, Danek F C. Powder processing and the fabrication of rhenium [J].Journal of the Minerals Metals and Materials Society, 1991, 43(7): 24.

[16]Su H, Yan X B, Liu X W, Ai Y, Ma K, Li R, Zhang Z, Sun Y M, Liu S. Research on high-temperature mechanical properties and microstructure of powder [J].International Journal of Refractory Metals and Hard Materials, 2022, 106: 105.

[17]Raisson G. Evolution of PM nickel base superalloy processes and products [J].Powder Metall, 2008, 51 (1): 10.

[18]Schafrik R, Sprague R. Superalloy technology-a perspective on critical innovations for turbine engines [J].Key Engineering Materials, 2008, 380: 113.

[19]Fecht H, Furrer D. Processing of nickel-base superalloys for turbine engine disc applications [J].Advanced Engineering Materials, 2000, 2 (12): 777.

[20]Wei Z C, Zhang L, Li X Y, Long Y, Qu X H. Effect of grain size on deformation behavior of pure rhenium [J].Materials Science and Engineering: A, 2022, 829: 142170.

[21]Sabisch J E C, Minor A M. Microstructural evolution of rhenium Part I: compression [J].Materials Science and Engineering: A, 2018, 732: 251.

[22]Sabisch J E C, Minor A M. Microstructural evolution of rhenium Part II: tension [J].Materials Science and Engineering: A, 2018, 732: 259.

[23]Jeffery R A, Smith E. Deformation twinning in rhenium single crystals [J].Philosophical Magzine, 1966, 13(126): 1163.

[24]Seyda J, Skibicki D, Pejkowski Ł, Skibicki A, Domanowski P, Maćkowiak P. Mechanical properties and microscopic analysis of sintered rhenium subjected to monotonic tension and uniaxial fatigue [J].Materials Science and Engineering: A, 2021, 817: 141343.

[25]Churchman A T. Deformation mechanisms and work hardening in rhenium [J].Metal. Petrol. Engi. Trans, 1960, 218: 262.

[26]Kacher J, Sabisch J E, Minor A M. Statistical analysis of twin/grain boundary interactions in pure rhenium [J].Acta Materialia, 2019, 173: 44.

[27]Josh K, Minor A M. Twin boundary interactions with grain boundaries investigated in pure rhenium [J].Acta Materials, 2014, 81: 1.

[28](肖林. 密排六方金属的塑性变形 [J].稀有金属材料与工程, 1995, (6): 21.)

L Xiao. Plastic deformation of hexagonal close-packed metals [J].Rare Metal Materials and Engineering, 1995, (6): 21.

[29](黄玖龙, 孙威杰, 张岩, 刘帅, 冯运莉. 轧制退火工艺对高碳含量孪晶诱发塑性钢拉伸变形行为的影响 [J].塑性工程学报, 2024, 31(5): 64.)

J L Huang, W J Sun, Y Zhang, S Liu, Y L Feng. Effect of rolling and annealing process on tensile deformation behavior of high carbon content twin-induced plasticity steel [J].Journal of Plasticity Engineering, 2024, 31(5): 64.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24070010

Chinese Library Classification Number:TG146.4+18

Citation Information:

Rhenium has high strain hardening index, tensile strength, elastic modulus and hardness, and has no ductile-brittle transition temperature. It is often used in metal-organic chemical vapor deposition (MOCVD) heaters and key components of engines. In order to meet its application in harsh ultra-high temperature service environments such as MOCVD heaters, this paper studied the tensile properties of pure rhenium (PM-Re) prepared by powder metallurgy at room temperature to 2000 ℃. The deformation mechanism of PM-Re was analyzed using scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), transmission electron microscopy (TEM), etc. The results showed that the room temperature tensile strength of PM-Re was 882 MPa. With the increase of temperature, the tensile strength of PM-Re decreased. At 2000 ℃, the tensile strength decreased to 112 MPa. The elongation after fracture of PM-Re at room temperature was 18%. In the temperature range of 1700–2000 ℃, the elongation after fracture was less than 10%. With the increase of temperature, the non-proportional elongation strength (Rp0.2) of PM-Re continuously decreased. At room temperature, Rp0.2 of PM-Re was 171 MPa, and at 1900 and 2000 ℃, it was only 17 and 6 MPa. The room temperature tensile fracture of PM-Re had both intergranular brittle fracture and transgranular fracture. Symmetrical structures along the fracture surface appeared on the grains where transgranular fracture occurred, and dislocation slip traces were found on the fracture surface. At high temperatures, a large number of lamellar structures, dimple-shaped fractures and "river" pattern characteristics appeared in the PM-Re specimens after tensile testing. It was found by EBSD characterization that the original PM-Re sample was composed of equiaxed grains. A large number of twins were produced after the sample was deformed at room temperature. There was a large local orientation difference inside the rhenium grains. The grain boundaries and twin boundaries showed a high local average misorientation (LAM) value. Dislocations were mainly distributed at the grain boundaries and interacted with the twin boundaries. With the increase of temperature, the degree of deformation of PM-Re increased, and the internal point defects and stress concentration areas increased, resulting in a gradual increase in the LAM value of PM-Re. Through the Schmidt factor map, it was found that the average Schmidt factor values of the cylindrical slip system and the conical slip system were the highest at high temperatures, and the non-basal slip system was the main slip system. The twin deformation traces in different directions on the same slip plane and the phenomenon of dislocation aggregation at the twin boundaries after tensile testing at room temperature were found by TEM, indicating that the twin and dislocation interacted, and the twin boundary would become an obstacle to dislocation movement. After tensile testing at 2000 ℃, subgrain boundaries formed by dislocation movement in the PM-Re body. The formation of subgrain boundaries could further hinder the dislocation slip, increase the deformation resistance of the material, and at the same time, the subgrain boundaries could coordinate the deformation between adjacent grains and effectively improve the uniform deformation ability of PM-Re. The above results showed that during the room temperature deformation process of PM-Re, twin deformation and dislocation slip coexisted. Twin deformation could improve the plasticity of rhenium, and dislocation cells and twin boundaries would hinder dislocation movement and thereby increase the work hardening rate of rhenium. The ultra-high temperature deformation process of PM-Re was dominated by dislocation slip, the non-basal slip system was the main slip system, and the basal slip system gradually opened at 2000 ℃.

quote

GB/T 7714-2015 [1] Chenghao Yang, Wenqing Ying, Di Dong, et al. Tensile Properties and Deformation Mechanism of Pure Rhenium at Room Temperature and Ultra-High Temperature[J]. Chinese Journal of Rare Metals, 2025, 49(11): 1651-1658. DOI:10.13373/j.cnki.cjrm.XY24070010.
MLA [1] Chenghao Yang, et al., "Tensile Properties and Deformation Mechanism of Pure Rhenium at Room Temperature and Ultra-High Temperature." Chinese Journal of Rare Metals, vol. 49, no. 11, 2025, pp. 1651-1658, https://doi.org/10.13373/j.cnki.cjrm.XY24070010.
APA [1] Chenghao Yang, Wenqing Ying, Di Dong, Fuge Chen, & Chengyu Zhang. (2025). Tensile Properties and Deformation Mechanism of Pure Rhenium at Room Temperature and Ultra-High Temperature. Chinese Journal of Rare Metals, 49(11), 1651-1658. https://doi.org/10.13373/j.cnki.cjrm.XY24070010
IEEE [1] Chenghao Yang, Wenqing Ying, Di Dong, Fuge Chen, and Chengyu Zhang, "Tensile Properties and Deformation Mechanism of Pure Rhenium at Room Temperature and Ultra-High Temperature," Chinese Journal of Rare Metals, vol. 49, no. 11, pp. 1651-1658, 2025, doi: 10.13373/j.cnki.cjrm.XY24070010. keywords: {pure rhenium;tensile property;twin deformation;dislocation motion}