daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Solidification Structure Evolution of ZL114A Aluminum Alloy with Surface Pulsed Magnetic Field and Ce Composite Treatment AITranslate

1.School of Materials Science and Engineering,Inner Mongolia University of Science & Technology,Baotou 014010,China
2.Inner Mongolia Key Laboratory of New Metal Material,Baotou 014010,China
3.Inner Mongolia YeKe Electromagnetic Energy Technology Co.,LTD.,Ordos 017010,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

ZL114A aluminum alloy is an Al-Si-Mg series cast aluminum alloy, renowned for its exceptional casting characteristics, comprehensive performance, and low thermal expansion coefficient. It finds extensive applications in producing intricate structural castings within the aerospace, automotive manufacturing, and construction industries. In recent years, the rapid advancement of China's aerospace industry has led to increasing demands for the service life and reliability of aluminum alloy castings. Currently, ZL114A aluminum alloy castings still face challenges such as low comprehensive performance and short service period, necessitating the urgent development of new technologies or processes to enhance the overall mechanical properties of ZL114A aluminum alloy. However, the utilization of various types of magnetic fields, including constant magnetic fields, pulsed magnetic fields, and alternating magnetic fields, to refine the solidification structure of aluminum alloy has emerged as a key area of research focus. Currently, there is limited literature on the enhanced refinement of microstructure and mechanical properties of ZL114A aluminum alloy through the composite interaction of rare earth elements and a magnetic field. This study proposed a composite treatment technology involving the application of surface pulsed magnetic field and Ce. The solidification process of ZL114A aluminum alloy was systematically investigated under the combined influence of surface pulsed magnetic field and varying Ce content. The effects of surface pulsed magnetic field and Ce compound action on the solidification microstructure, crystal structure, and hardness of ZL114A aluminum alloy were investigated by metallurgical microscopy (OM), scanning electron microscope (SEM), X-ray diffraction (XRD), and Vickers hardness tester. The results showed that when Ce content was 0.15% under the action of the surface pulsed magnetic field, the solidification microstructure of ZL114A aluminum alloy had the best refinement effect, and the average grain size of the solidified structure was 95 μm, compared with the sample without composite treatment and only with 0.3%Ce, the average grain of the solidification microstructure was reduced by 39.5% and 24.4%, respectively. The eutectic Si morphology of ZL114A aluminum alloy had also changed from the original slat-shaped to a fine short rod or spherical shape. Compared with the samples with no composite treatment and only 0.3%Ce, the proportion of eutectic Si area and the average size of length diameter decreased by 20.3%, 34.8%, 9.2% and 26.1%, respectively. Compared with the samples without composite treatment, the comparison of the samples with surface pulsed magnetic field and Ce content of 0.15% promoted the accumulation of Al atoms in <111>, <200> and <220> directions, and hindered the growth of Al atoms in <311> direction, and the comparison of the non-composite samples promoted the accumulation of Si atoms in the <200>, <220> and <422>, and hindered the growth of Si atoms in <111> direction. The surface pulsed magnetic field and the composite effect of Ce were more conducive to the refinement of the solidification microstructure of ZL114A aluminum alloy α-Al grain and eutectic Si morphology, which opened up a new way for the composition design and composite process development of ZL114A aluminum alloy.

KeyWords AITranslate

surface pulsed magnetic field rare earth Ce ZL114A aluminum alloy eutectic Si grain refinement

[1]James C W, Edgar A S J. Progress in structural materials for aerospace systems [J].Acta Mater, 2003, 51: 5775.

[2]Xu Y T, Guan T Y, Zhang Z F, Bai Y L, Mao W M. Semi-solid rheological squeeze casting process of ZL114A aluminum alloy thin-wall complex casting [J].Materials Science Forum, 2020, 993: 248.

[3](陈瑞, 许庆彦, 郭会廷, 夏志远, 吴勤芳, 柳百成. Al-7Si-Mg铸造铝合金凝固和热处理过程微观组织模拟和屈服强度预测 [J].稀有金属, 2017, 41(8): 837.)

R Chen, Q Y Xu, H T Guo, Z Y Xia, Q F Wu, B C Liu. Modeling microstructure and yield strength during solidification and heat treatment process in Al-7Si-Mg cast aluminum alloys [J].Chinese Journal of Rare Metals, 2017, 41(8): 837.

[4]Liotti E, Lui A, Vincent R, Kumar S, Guo Z, Connolley T, Dolbnya I P, Hart M, Arnberg L, Mathiesen R H, Grant P S. A synchrotron X-ray radiography study of dendrite fragmentation induced by a pulsed electromagnetic field in an Al-15Cu alloy [J].Acta Mater, 2014, 70: 228.

[5]Liao H C, Ding Y, Sun G X. Effect of strontium on columnar growth of dendritic α phase in near-eutectic Al-11.6%Si alloys [J].Transactions of Nonferrous Metals Society of China, 2004, 14(4): 5.

[6](姜坤, 刘桂亮, 赵凯, 杨化冰, 孙谦谦, 刘相法. 抗Si"中毒"AlTiC-B晶种合金对ZL114铝合金组织和力学性能的影响 [J].材料导报, 2021, 35(16): 16076.)

K Jiang, G L Liu, K Zhao, H B Yang, Q Q Sun, X F Liu. Effect of anti Si 'poisoning' AlTiC-B master alloy on the microstructures and mechanical properties of ZL114 aluminum alloy [J].Material Reports, 2021, 35(16): 16076.

[7](陈义斯, 芦刚, 严青松, 黄普英, 徐翩, 毛蒲, 周泽远. 稀土钇、铈变质真空差压铸造ZL114A合金的力学性能及蠕变机制 [J].机械工程学报, 2023, 59(18): 186.)

Y S Chen, G Lu, Q S Yan, P Y Huang, P Xu, P Mao, Z Y Zhou. Mechanical properties and creep mechanism of yttrium and cerium modified ZL114A alloy via vacuum counter-pressure casting [J].Journal of Mechanical Engineering, 2023, 59(18): 186.

[8](王琳, 牛子帆, 张书维, 张波. 稀土Ce对铝硅合金组织、力学及耐腐蚀性能的影响 [J].轻金属, 2024, 3: 28.)

L Wang, Z F Niu, S W Zhang, B Zhang. Effect of rare earth Ce on the organization, mechanics and corrosion resistance of Al-Si alloy [J].Light Metals, 2024, 3: 28.

[9](宋佳鑫, 郭伟玲, 邢志国, 李志雄, 王海斗, 张磊, 黄艳斐. 磁场类型对金属凝固机理的影响研究综述 [J].中国表面工程, 2023, 36(4): 1.)

J X Song, W L Guo, Z G Xing, Z X Li, H D Wang, L Zhang, Y P Huang. Review of the effect of different magnetic field on metal solidification [J].China Surface Engineering, 2023, 36(4): 1.

[10](朱锐, 王俊杰, 张云虎, 田志超, 苗信成, 翟启杰. 复合磁场对金属熔体流动及凝固组织的影响 [J].金属学报, 2024, 60(2): 231.)

R Zhu, J J Wang, Y H Zhang, Z C Tian, X C Miao, Q J Zhai. Flow and solidification microstructure in metal melts driven by a combined magnetic field [J].Acta Metallurgica Sinica, 2024, 60(2): 231.

[11]Jiang W M, Fan Z T, Dai Y C, Li C. Effects of rare earth elements addition on microstructures, tensile properties and fractography of A357 alloy [J].Materials Science and Engineering: A, 2014, 597: 237.

[12]Gong Y Y, Luo J, Jing J X, Xia Z Q, Zhai Q J. Structure refinement of pure aluminum by pulse magneto-oscillation [J].Materials Science and Engineering: A, 2008, 497(1-2): 147.

[13]Li B, Wang H W, Jie J C, Wei Z J. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al-7.5Si-0.5Mg alloy [J].Materials and Design, 2011, 32(3): 1617.

[14]Fan T, Ruan Z, Zhong F, Xie C, Li X, Chen D, Tang P, Wu Y. Nucleation and growth of L12-Al3RE particles in aluminum alloys: a first-principles study [J].Journal of Rare Earth, 2023, 41(7): 1116.

[15]Diana A L, Diran A. Relationships between microstructure and fatigue crack propagation paths in Al-Si-Mg cast alloys [J].Engineering Fracture Mechanics, 2008, 75(3-4): 821.

[16]Cheng S J, Zhao Y H, Hou H, Jin Y C, Guo X X. Preparation of semi-solid ZL101 aluminum alloy slurry by serpentine channel [J].Transactions of Nonferrous Metals Society of China, 2016, 26(7): 1820.

[17](甘培原, 韦德仕, 韦世强, 秦文忠, 彭健飞, 曾杰. 稀土元素La, Ce对Al-3Si-0.4Cu-1.0Fe压铸铝合金微观组织, 力学性能及热导率的影响 [J].稀有金属与硬质合金, 2023, 51(5): 50.)

P Y Gan, D S Wei, S Q Wei, W Z Qin, J F Peng, J Zeng. Effect of rare earth element La, Ce on the microstructure, mechanical properties and thermal conductivity of Al-3Si-0.4Cu-1.0Fe die-cast aluminum alloy [J].Rare Metals and Cemente Carbides, 2023, 51(5): 50.

[18]Bai Q W, Ma Y L, Xing S Q, Bao X Y, Feng Y F, Kang X L. Nucleation and grain refinement of 7A04 aluminum alloy under a low-power electromagnetic pulse [J].Journal of Materials Engineering & Performance, 2018, 27(2): 857.

[19]Nourouzi S, Baseri H, Kolahdooz A, Ghavamodini S M. Optimization of semi-solid processing of A356 aluminum alloy [J].Journal of Mechanical Science and Technology, 2013, 27(12): 3869.

[20]Chen Y S, Zhang L, Liu W K, Wu G H, Ding W J. Preparation of Mg-Nd-Zn-(Zr) alloys semisolid slurry by electromagnetic stirring [J].Materials and Design, 2016, 95: 398.

[21](白庆伟, 麻永林, 邢淑清, 冯艳飞, 鲍鑫宇, 于文霞. 铝合金表面脉冲电磁场对半连续铸造晶粒的细化 [J].工程科学学报, 2017, 39(12): 1828.)

Q W Bai, Y L Ma, S Q Xing, Y F Feng, X Y Bao, W X Yu. Refining of a DC-casting aluminum alloy structure using surface electromagnetic pulsing [J].Chinese Journal of Engineering, 2017, 39(12): 1828.

[22]Burke J E, Turnbull D. Recrystallization and grain growth [J].Progress in Metal Physics, 1952, 3: 220.

[23]Li H, Wang G H, Zhao J J, Bian X F. Cluster structure and dynamics of liquid aluminum under cooling conditions [J].Journal of Chemical Physics, 2002, 116(24): 10809.

[24](赵云鹏, 沈利, 冯艳飞, 邢淑清, 麻永林. 表面脉冲磁场作用时间对7A04铝合金凝固过程的影响 [J].热加工工艺, 2021, 50(3): 56.)

Y P Zhao, L Shen, Y F Feng, S Q Xing, Y L Ma. Effect of surface pulsed magnetic field action time on solidification process of 7A04 aluminum alloy [J].Hot Working Technology, 2021, 50(3): 56.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24060015

Chinese Library Classification Number:TG292

Citation Information:

ZL114A aluminum alloy is an Al-Si-Mg series cast aluminum alloy, renowned for its exceptional casting characteristics, comprehensive performance, and low thermal expansion coefficient. It finds extensive applications in producing intricate structural castings within the aerospace, automotive manufacturing, and construction industries. In recent years, the rapid advancement of China's aerospace industry has led to increasing demands for the service life and reliability of aluminum alloy castings. Currently, ZL114A aluminum alloy castings still face challenges such as low comprehensive performance and short service period, necessitating the urgent development of new technologies or processes to enhance the overall mechanical properties of ZL114A aluminum alloy. However, the utilization of various types of magnetic fields, including constant magnetic fields, pulsed magnetic fields, and alternating magnetic fields, to refine the solidification structure of aluminum alloy has emerged as a key area of research focus. Currently, there is limited literature on the enhanced refinement of microstructure and mechanical properties of ZL114A aluminum alloy through the composite interaction of rare earth elements and a magnetic field. This study proposed a composite treatment technology involving the application of surface pulsed magnetic field and Ce. The solidification process of ZL114A aluminum alloy was systematically investigated under the combined influence of surface pulsed magnetic field and varying Ce content. The effects of surface pulsed magnetic field and Ce compound action on the solidification microstructure, crystal structure, and hardness of ZL114A aluminum alloy were investigated by metallurgical microscopy (OM), scanning electron microscope (SEM), X-ray diffraction (XRD), and Vickers hardness tester. The results showed that when Ce content was 0.15% under the action of the surface pulsed magnetic field, the solidification microstructure of ZL114A aluminum alloy had the best refinement effect, and the average grain size of the solidified structure was 95 μm, compared with the sample without composite treatment and only with 0.3%Ce, the average grain of the solidification microstructure was reduced by 39.5% and 24.4%, respectively. The eutectic Si morphology of ZL114A aluminum alloy had also changed from the original slat-shaped to a fine short rod or spherical shape. Compared with the samples with no composite treatment and only 0.3%Ce, the proportion of eutectic Si area and the average size of length diameter decreased by 20.3%, 34.8%, 9.2% and 26.1%, respectively. Compared with the samples without composite treatment, the comparison of the samples with surface pulsed magnetic field and Ce content of 0.15% promoted the accumulation of Al atoms in <111>, <200> and <220> directions, and hindered the growth of Al atoms in <311> direction, and the comparison of the non-composite samples promoted the accumulation of Si atoms in the <200>, <220> and <422>, and hindered the growth of Si atoms in <111> direction. The surface pulsed magnetic field and the composite effect of Ce were more conducive to the refinement of the solidification microstructure of ZL114A aluminum alloy α-Al grain and eutectic Si morphology, which opened up a new way for the composition design and composite process development of ZL114A aluminum alloy.

quote

GB/T 7714-2015 [1] Yanfei Feng, Yonglin Ma, Xinyu Bao, et al. Solidification Structure Evolution of ZL114A Aluminum Alloy with Surface Pulsed Magnetic Field and Ce Composite Treatment[J]. Chinese Journal of Rare Metals, 2025, 49(11): 1669-1679. DOI:10.13373/j.cnki.cjrm.XY24060015.
MLA [1] Yanfei Feng, et al., "Solidification Structure Evolution of ZL114A Aluminum Alloy with Surface Pulsed Magnetic Field and Ce Composite Treatment." Chinese Journal of Rare Metals, vol. 49, no. 11, 2025, pp. 1669-1679, https://doi.org/10.13373/j.cnki.cjrm.XY24060015.
APA [1] Yanfei Feng, Yonglin Ma, Xinyu Bao, Yan Li, Shuqing Xing, & Yongzhen Liu. (2025). Solidification Structure Evolution of ZL114A Aluminum Alloy with Surface Pulsed Magnetic Field and Ce Composite Treatment. Chinese Journal of Rare Metals, 49(11), 1669-1679. https://doi.org/10.13373/j.cnki.cjrm.XY24060015
IEEE [1] Yanfei Feng, Yonglin Ma, Xinyu Bao, Yan Li, Shuqing Xing, and Yongzhen Liu, "Solidification Structure Evolution of ZL114A Aluminum Alloy with Surface Pulsed Magnetic Field and Ce Composite Treatment," Chinese Journal of Rare Metals, vol. 49, no. 11, pp. 1669-1679, 2025, doi: 10.13373/j.cnki.cjrm.XY24060015. keywords: {surface pulsed magnetic field;rare earth Ce;ZL114A aluminum alloy;eutectic Si;grain refinement}