Thermal Decomposition of Ammonium Paramolybdate and its Thermodynamic Analysis AITranslate

Institute of Physical Chemistry, School of Chemical Science and Technology, Lingnan Normal University, Guangdong University New Materials Engineering Technology Development Center;Institute of Physical Chemistry, School of Chemical Science and Technology, Lingnan Normal University, Guangdong University New Materials Engineering Technology Development Center;Institute of Physical Chemistry, School of Chemical Science and Technology, Lingnan Normal University, Guangdong University New Materials Engineering Technology Development Center;Institute of Physical Chemistry, School of Chemical Science and Technology, Lingnan Normal University, Guangdong University New Materials Engineering Technology Development Center
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermal decomposition of ammonium paramolybdate in 30~600℃air was analyzed by TG-DSC.The results show that there are three stages during weight loss of ammonium paramolybdate at 30~600℃,and weight loss tends to finish when the temperature is higher than 340℃.XRD pattern shows that the end product of thermal decomposition is pure orthorhombic molybdenum trioxide.The mechanism of thermal decomposition of ammonium paramolybdate in the air was proposed and theoretical verification was carried out.It is considered that ammonium paramolybdate only loses four crystal water molecules in the first stage of its thermal decomposition,while NH3 and H2O are lost by the molar ratio of 2∶1in the other three stages.Otherwise,through enthalpy change values of decomposition reaction in the various stages,approximate molar formation enthalpy was estimated of ammonium paramolybdate and the related decomposition products under the experimental conditions.

KeyWords AITranslate

ammonium paramolybdate thermal decomposition thermogravimetric analysis differential scanning calorimetry

1傅小明,杨在志,刘照文.仲钼酸铵热分解过程的研究[J].中国钼业,2011,35(3):30-32. 被引量:3

2傅小明,刘照文.仲钼酸铵热分解过程及其形貌演变的研究[J].稀有金属,2011,35(1):113-117. 被引量:4

3朱爱辉,王快社,张兵.钼在冶金工业中的应用[J].中国钼业,2006,30(5):8-12. 被引量:19

4李兵.钼在钢铁工业中的应用[J].金属世界,2005(1):48-48. 被引量:7

5赵朴.钼在不锈钢中的应用[J].中国钼业,2004,28(5):3-10. 被引量:17

6罗振中.我国钼工业现状及发展对策浅议[J].中国钼业,2000,24(4):3-6. 被引量:8

7朱伯仲,林钰,尚雪亚,刘双月,李新生.钼酸铵的热分解机理研究[J].兰州大学学报:自然科学版,1997,33(3):72-76. 被引量:13

8朱伯仲,尚雪亚,林钰,刘双月.利用热重差热技术研究钼酸铵的热分解[J].郑州大学学报:自然科学版,1997,29(3):71-73. 被引量:9

1田野,林泉,孙大智,李萍.高压扭转制备难熔金属Mo的微观结构及性能分析[J].稀有金属与硬质合金,2016,44(4):38-42. 被引量:2

2张旭,郭军刚,白佩,员汝娜,李冬,李稳宏.七钼酸铵制备工艺优化及热力学分析研究[J].西北大学学报:自然科学版,2017,47(6):852-858. 被引量:2

3章钒,陈颜龙,李涓.稀土掺杂双钙钛矿结构红色荧光粉的制备及其发光性能[J].材料科学与工程学报,2018,36(3):460-464. 被引量:2

4何江山,佀龙祥,刘涛,雷宁宁,李玉涛,李莉.非团聚二钼酸铵热分解机理及热力学分析[J].中国钼业,2022,46(5):38-42.

1韩兆越.稀有难熔金属材料产业的发展研究[J].世界有色金属,2017,42(20):224-225. 被引量:2

2李彦龙,李银丽,李守荣,鲁兴武,陈一博,焦晓斌,牛永胜.用钼精矿制备钼酸铵试验研究[J].湿法冶金,2020,39(1):30-33. 被引量:1

3巩振虎,刘义章,孟飞,王磊.稀土离子掺杂铌酸盐微纳米材料的制备及性能表征[J].黑龙江工业学院学报:综合版,2020,20(5):102-106.

4陈文静,胡平,邢海瑞,夏雨,李世磊,左烨盖,王快社,冯鹏发,常恬,李来平.热处理工艺对钼金属板材组织和性能影响的研究进展[J].材料导报,2021,35(3):3141-3151. 被引量:5

5李敬远.双钙钛矿结构Rb_(3)GaF_(6)∶Er^(3+),Yb^(3+)的合成及上转换发光特性研究[J].人工晶体学报,2023,52(2):327-333.

6陈超,张贵清,关文娟,武新生,巫圣喜,李青刚,曹佐英.二钼酸铵湿法制备七钼酸铵新工艺研究[J].稀有金属与硬质合金,2023,51(2):13-19.

1林潜德,徐孝德.仲钼酸铵生产线简介[J].中国钼业,1996,20(3):26-28.

2秦文峰,彭金辉,樊希安,肖新志,袁茂强.微波辐射法干燥仲钼酸铵新工艺[J].中国钼业,2002,26(6):28-31. 被引量:12

3李天锁.钾对仲钼酸铵直接还原成二氧化钼的影响[J].中国钼业,1997,21(6):28-32. 被引量:4

4钼盐文摘[J].无机盐技术,2012(3):54-54.

5谢东.重结晶法提纯生产试剂钼酸铵[J].湖北化工,2002,19(2):29-29. 被引量:3

6易永鹏.仲钼酸铵(APM)生产过程质量控制[J].中国钼业,1998,22(5):45-46.

7周朝辉,华东发,丁芝虎,张之洁,赵业松.仲钼酸铵(AHM)生产新工艺研究[J].稀有金属与硬质合金,1998,26(3):1-4. 被引量:6

8祁文博,艾抚宾,徐彤,乔凯,袁毅.焦化干气加氢热力学研究及其工业应用[J].当代石油石化,2016,24(11):20-24. 被引量:3

9赵延霞.水热法合成一维纳米级MoO_3微粉[J].中国钨业,2012,27(3):25-29. 被引量:2

10高纯仲钼酸铵的制备方法[J].中国钼业,2006,30(5):49-49.

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.12[化学工程—无机化工]

Citation Information:

Thermal decomposition of ammonium paramolybdate in 30~600℃air was analyzed by TG-DSC.The results show that there are three stages during weight loss of ammonium paramolybdate at 30~600℃,and weight loss tends to finish when the temperature is higher than 340℃.XRD pattern shows that the end product of thermal decomposition is pure orthorhombic molybdenum trioxide.The mechanism of thermal decomposition of ammonium paramolybdate in the air was proposed and theoretical verification was carried out.It is considered that ammonium paramolybdate only loses four crystal water molecules in the first stage of its thermal decomposition,while NH3 and H2O are lost by the molar ratio of 2∶1in the other three stages.Otherwise,through enthalpy change values of decomposition reaction in the various stages,approximate molar formation enthalpy was estimated of ammonium paramolybdate and the related decomposition products under the experimental conditions.

quote

GB/T 7714-2015 [1] ZHOU Xiao-ping, MA Lin, XU Xu-yao, et al. Thermal Decomposition of Ammonium Paramolybdate and its Thermodynamic Analysis[J]. Rare Metals and Cemented Carbides, 2015(3): 25-28.
MLA [1] ZHOU Xiao-ping, et al., "Thermal Decomposition of Ammonium Paramolybdate and its Thermodynamic Analysis." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 25-28.
APA [1] ZHOU Xiao-ping, MA Lin, XU Xu-yao, & FENG Zong-cai. (2015). Thermal Decomposition of Ammonium Paramolybdate and its Thermodynamic Analysis. Rare Metals and Cemented Carbides(3), 25-28.
IEEE [1] ZHOU Xiao-ping, MA Lin, XU Xu-yao, and FENG Zong-cai, "Thermal Decomposition of Ammonium Paramolybdate and its Thermodynamic Analysis," Rare Metals and Cemented Carbides, no. 3, pp. 25-28, 2015. keywords: {ammonium paramolybdate;thermal decomposition;thermogravimetric analysis;differential scanning calorimetry}