Study on the Behavior of Fe Impurity during Preparation of High Purity Titanium by CVD AITranslate

School of Materials and Metallurgical Engineering, Guizhou University;School of Materials and Metallurgical Engineering, Guizhou University;School of Materials and Metallurgical Engineering, Guizhou University;School of Materials and Metallurgical Engineering, Guizhou University;School of Materials and Metallurgical Engineering, Guizhou University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The behavior of Fe impurity was studied during preparation of high purity titanium by CVD.The conditions of synthesis and decomposition of ferrous halide were analyzed based on thermodynamic calculation.The results show that the optimal halogenation temperature is 800~1 000 K,and the best pyrolysis deposition temperature is 1 400~1 650 K.In the above temperature range,not only can high purity titanium be effectively produced,but also the secondary pollution caused by Fe impurity can be effectively inhibited.

KeyWords AITranslate

high purity titanium Fe impurity CVD low temperature halogenation high temperature deposition thermodynamics

1王睿,陈肖虎,李纪伟,卢大磊,唐晓宁.卤化法制备高纯钛过程中杂质Al的来源分析[J].湿法冶金,2014,33(4):309-312. 被引量:1

2李武斌,陈肖虎,曾英,王舟,韩涛.CVD高纯钛过程中杂质Mn的热力学行为分析[J].轻金属,2010(8):66-69. 被引量:3

3刘正红,陈志强.高纯钛的应用及其生产方法[J].稀有金属快报,2008,27(2):1-8. 被引量:20

4李玲玲.用碘化物精炼高纯钛[J]新疆有色金属,2001(02).

5李哲,郭让民.高纯钛的制备及其发展方向[J].钛工业进展,1997,14(3):8-11. 被引量:19

6吴全兴.高纯钛作为电子材料的应用[J].钛工业进展,1996(6):32-33. 被引量:2

7高晓军.用新的碘化法制造高纯度钛[J].钛工业进展,1995(4):19-20. 被引量:8

8石应江.高纯钛的生产与应用[J].上海金属:有色分册,1993,14(6):26-33. 被引量:6

1古伟良.电弧等离子体CVD法制备微细钽粉[J].国外稀有金属动态,1992(17):6-7.

2吴荣华.用流化床CVD法制造陶瓷微粉[J].国外稀有金属动态,1991(18):2-3.

3阳志洪,刘莉娜,孙克萍,王克功,陈肖虎.CVD法制备高纯钛中锆杂质的热力学分析[J].有色金属:冶炼部分,2012(3):31-34. 被引量:1

4方敏,陈肖虎,宋建敏,韩涛.CVD法制备高纯钛形核过程动力学分析[J].轻金属,2010(2):55-58.

5李汉广,彭志辉.氟化物CVD法直接制取特纯高致密异型钨制品[J].稀有金属材料与工程,1994,23(6):74-77. 被引量:13

6李杰瑞,陈肖虎,李纪伟,王帅帅,李明新,王睿.CVD法制备高纯钛过程中Ni的热力学分析[J].轻金属,2015(7):48-50.

7胡广勇,武保林,王刚,王轶农,左良,C.Esling.CVD法制取Fe-6-5% Si薄板的扩散工艺计算机模拟[J].东北大学学报:自然科学版,1999,20(4):405-407. 被引量:2

8吴荣华.用等离子电弧CVD法制造Al—TiB2复合粉末[J].国外稀有金属动态,1991(4):8-9.

9王睿,唐晓宁,陈肖虎,李纪伟,李明新.CVD法制备高纯钛的工艺优化[J].有色金属:冶炼部分,2014(9):23-25.

10陈肖虎,刘义敏.CVD高纯钛的热力学分析[J].有色金属:冶炼部分,2009(1):10-13. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]

Citation Information:

The behavior of Fe impurity was studied during preparation of high purity titanium by CVD.The conditions of synthesis and decomposition of ferrous halide were analyzed based on thermodynamic calculation.The results show that the optimal halogenation temperature is 800~1 000 K,and the best pyrolysis deposition temperature is 1 400~1 650 K.In the above temperature range,not only can high purity titanium be effectively produced,but also the secondary pollution caused by Fe impurity can be effectively inhibited.

quote

GB/T 7714-2015 [1] LI Ji-wei, CHEN Xiao-hu, WANG Rui, et al. Study on the Behavior of Fe Impurity during Preparation of High Purity Titanium by CVD[J]. Rare Metals and Cemented Carbides, 2015(3): 29-32.
MLA [1] LI Ji-wei, et al., "Study on the Behavior of Fe Impurity during Preparation of High Purity Titanium by CVD." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 29-32.
APA [1] LI Ji-wei, CHEN Xiao-hu, WANG Rui, LI Ming-xin, & WANG Shuai-shuai. (2015). Study on the Behavior of Fe Impurity during Preparation of High Purity Titanium by CVD. Rare Metals and Cemented Carbides(3), 29-32.
IEEE [1] LI Ji-wei, CHEN Xiao-hu, WANG Rui, LI Ming-xin, and WANG Shuai-shuai, "Study on the Behavior of Fe Impurity during Preparation of High Purity Titanium by CVD," Rare Metals and Cemented Carbides, no. 3, pp. 29-32, 2015. keywords: {high purity titanium;Fe impurity;CVD;low temperature halogenation;high temperature deposition;thermodynamics}