daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Process Design for Copper and Gold Recovery from Electronic and Electrical Waste by Chemical Process AITranslate

Changsha Nonferrous Metallurgical Design Research Institute Co., Ltd.;Changsha Nonferrous Metallurgical Design Research Institute Co., Ltd.;Changsha Nonferrous Metallurgical Design Research Institute Co., Ltd.;Changsha Nonferrous Metallurgical Design Research Institute Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Copper and gold were recovered from electronic and electrical waste.The adopted processes are sulfuric acid stirring leaching-electrolysis and nitric acid treatment of copper leaching residue combined with cyanide plating off the board-zinc replacement-purification with aqua regia,respectively,including the process steps of leaching,replacement,electrodeposition and precipitation.

KeyWords AITranslate

electronic and electrical waste copper and gold recovery by chemical process leaching replacement process design

1郑骥.我国废有色金属拆解利用再生产业发展现状[J].中国环保产业,2010(4):9-12. 被引量:9

2魏金秀,汪永辉,李登新.国内外电子废弃物现状及其资源化技术[J].东华大学学报:自然科学版,2005,31(3):133-138. 被引量:39

3董锁成,范振军.中国电子废弃物循环利用产业化问题及其对策[J].资源科学,2005,27(1):39-45. 被引量:37

4魏家鸿.国外资源再生产业发展现状浅析[J].世界有色金属,2004(4):26-29. 被引量:15

5兰兴华.从再生资源中回收有色金属的进展(续2)[J].世界有色金属,2003(11):64-69. 被引量:2

6柴晓兰,赵跃民,王春彦.电子废弃物机械回收的研究现状与发展[J].污染防治技术,2003,16(3):47-50. 被引量:30

7李莉,张维志.废旧电脑污染问题及其管理对策[J].再生资源研究,2002(6):12-14. 被引量:19

8朱经发,林辉东,王德汉,彭俊杰.电子废物现状评述与资源化初探[J].土壤与环境,2002,11(3):307-310. 被引量:53

9庾晋,白杉.旧家电该如何“处置”[J].中国资源综合利用,2002(6):26-27. 被引量:7

1德国将实施电子电器废弃物处理法[J].福建标准化信息,1996(5):26-26.

2彭绍洪,陈烈强,甘舸.电子电器废弃物的热处置回收技术[J].工业加热,2004,33(6):27-30. 被引量:5

3刘一.中国电子电器废弃物回收利用环境影响与管理研究[J].环境科学与管理,2014,39(7):11-14. 被引量:2

4潘少军.电子垃圾是“环境毒药”吗?[J].今日南国,2011(10):15-16.

5彭绍洪.电子电器废弃物的热处置回收技术[J].有色金属再生与利用,2006(4):21-23. 被引量:4

6赵刚.电器电子废物相关法律制度建设的现状及存在的问题[J].中国电子商务,2010(6):291-291.

7电子垃圾:破解困局[J].中国计算机用户,2004(40):22-24. 被引量:2

8电子垃圾简单的产业链[J].中国科技信息,2004(6):41-42.

9李瑞迪,袁铁锤,范文博,周立波,吴浩波,李健.Removal of tin and extraction of indium from acid-dissolved solution of waste indium-tin targets[J].中南大学学报:英文版,2014,21(5):1741-1746.

10海康威视全面进入前端视频监控产品领域[J].中国公共安全,2008,0(4):139-139.

Basic Information:

DOI:

Chinese Library Classification Number:X705[环境科学与工程—环境工程]

Citation Information:

Copper and gold were recovered from electronic and electrical waste.The adopted processes are sulfuric acid stirring leaching-electrolysis and nitric acid treatment of copper leaching residue combined with cyanide plating off the board-zinc replacement-purification with aqua regia,respectively,including the process steps of leaching,replacement,electrodeposition and precipitation.

quote

GB/T 7714-2015 [1] TAN Rong-he, CHEN Wen-yong, WU Xiao-song, et al. Process Design for Copper and Gold Recovery from Electronic and Electrical Waste by Chemical Process[J]. Rare Metals and Cemented Carbides, 2015(3): 21-24.
MLA [1] TAN Rong-he, et al., "Process Design for Copper and Gold Recovery from Electronic and Electrical Waste by Chemical Process." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 21-24.
APA [1] TAN Rong-he, CHEN Wen-yong, WU Xiao-song, & ZHOU Xiao-yuan. (2015). Process Design for Copper and Gold Recovery from Electronic and Electrical Waste by Chemical Process. Rare Metals and Cemented Carbides(3), 21-24.
IEEE [1] TAN Rong-he, CHEN Wen-yong, WU Xiao-song, and ZHOU Xiao-yuan, "Process Design for Copper and Gold Recovery from Electronic and Electrical Waste by Chemical Process," Rare Metals and Cemented Carbides, no. 3, pp. 21-24, 2015. keywords: {electronic and electrical waste;copper and gold recovery by chemical process;leaching;replacement;process design}