daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Interactions between displacement cascade and dislocation and their influences on Peierls stress in Fe-20Cr-25Ni alloys AITranslate

University of Tennessee; University of Tennessee; Oak Ridge National Laboratory; Oak Ridge National Laboratory; University of Tennessee
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The interactions between dislocations and displacement cascades are investigated using molecular dynamics simulations. The primary knock-on atoms (PKAs) are placed at different distances to edge and screw dislocation lines. Specifically, an fcc Fe-20Cr-25Ni system is studied; the alloy is the based alloy for Alloy 709. The number of defects is calculated using Wigner-Seitz analysis in order to illustrate the effect of dislocations on cascades. The displacement cascades in systems containing dislocations tend to generate more total defects compared with bulk systems, but eventually lead to less surviving defects in the materials matrix due to interactions with dislocations. The changes in atomic structures of the dislocations after interacting with cascades are analyzed to understand how the primary damage affects dislocations. The displacement cascade potentially causes dislocation climb in edge dislocations and cross-slip in screw dislocations, which could serve as additional mechanisms contributing to the radiation-induced hardening (RIH) compared with conventional RIH models. To reveal this, Peierls stresses are calculated before and after cascades using molecular static simulations. This study provides critical information of how defect production and dislocations are correlated, especially when total dose is high, which needs to be taken into account in upper scale models, such as mean-field rate theory. Graphical abstract Mutual interaction between displacement cascades and dislocations in fcc Fe-20Cr-25Ni alloy. Download : Download high-res image (43KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2018.12.018

Chinese Library Classification Number:

Citation Information:

The interactions between dislocations and displacement cascades are investigated using molecular dynamics simulations. The primary knock-on atoms (PKAs) are placed at different distances to edge and screw dislocation lines. Specifically, an fcc Fe-20Cr-25Ni system is studied; the alloy is the based alloy for Alloy 709. The number of defects is calculated using Wigner-Seitz analysis in order to illustrate the effect of dislocations on cascades. The displacement cascades in systems containing dislocations tend to generate more total defects compared with bulk systems, but eventually lead to less surviving defects in the materials matrix due to interactions with dislocations. The changes in atomic structures of the dislocations after interacting with cascades are analyzed to understand how the primary damage affects dislocations. The displacement cascade potentially causes dislocation climb in edge dislocations and cross-slip in screw dislocations, which could serve as additional mechanisms contributing to the radiation-induced hardening (RIH) compared with conventional RIH models. To reveal this, Peierls stresses are calculated before and after cascades using molecular static simulations. This study provides critical information of how defect production and dislocations are correlated, especially when total dose is high, which needs to be taken into account in upper scale models, such as mean-field rate theory. Graphical abstract Mutual interaction between displacement cascades and dislocations in fcc Fe-20Cr-25Ni alloy. Download : Download high-res image (43KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Zizhe Lu, Liubin Xu, Tianyi Chen, et al. Computational Materials Science, 2019(160). DOI:10.1016/j.commatsci.2018.12.018.
MLA [1] Zizhe Lu, et al., Computational Materials Science, no. 160, 2019, https://doi.org/10.1016/j.commatsci.2018.12.018.
APA [1] Zizhe Lu, Liubin Xu, Tianyi Chen, Lizhen Tan, & Haixuan Xu. (2019). Computational Materials Science(160). https://doi.org/10.1016/j.commatsci.2018.12.018
IEEE [1] Zizhe Lu, Liubin Xu, Tianyi Chen, Lizhen Tan, and Haixuan Xu, Computational Materials Science, no. 160, 2019, doi: 10.1016/j.commatsci.2018.12.018.