Implications of the micromechanical Taylor Factor on work hardening parameters: New perspectives from FFT simulations in DAMASK

Highlights • Classical Taylor model proves inadequate for strain prediction. • Micromechanical Taylor Factor outperforms in capturing local effects. • Work-hardening models improve with Micromechanical Taylor Factor. • Different insights into dislocation mechanisms using refined approach. • Potential to revolutionize materials design with greater precision. This study uses Fast Fourier Transform (FFT) simulations in the Düsseldorf Advanced Material Simulation Kit (DAMASK) to investigate the influence of the micromechanical Taylor Factor on the work hardening parameters. Departing from the assumption of a homogeneous deformation in the classical Taylor model, we use the micromechanical Taylor Factor, which takes better account of local grain interactions and strain distributions. Our comparison of simulations using both classical and micromechanical Taylor factors reveal crucial differences in the predicted dislocation mechanisms, leading to different interpretations of work hardening behavior. Our results question the adequacy of conventional models and suggest a more sophisticated understanding of the deformation of polycrystalline materials. The study underscores the importance of an improved modeling approach to characterize deformation and leads to a re-assessment of existing predictive mechanisms in materials science with possible implications for optimizing of material performance. Graphical abstract Download : Download high-res image (259KB) Download : Download full-size image

Show more

Modulating superdislocation cores and planar faults of Ni3Al through applied stresses

By employing atomic material properties (i.e., elastic moduli and general stacking fault energy (GSFE)) of Ni3Al with L12 structure, we predict a series of core configurations of dislocations with edge and screw characters associated with slip systems of ( 1 1 1 ) 0 1 1 ¯ and ( 0 0 1 ) 1 1 0 under various external applied stresses. For the slip system of ( 1 1 1 ) 0 1 1 ¯ , the dislocation cores are found to consist of one APB and two CSF faults, with a larger core for the edge dislocation than for the screw. Such multi faults core configuration is missing for the ( 0 0 1 ) 1 1 0 slip system, where only a larger APB fault is present due to a lower APB energy on ( 0 0 1 ) as compared with that on ( 1 1 1 ) . The dissociation mechanism for full dislocations into super partials and possible faults under different applied shear stresses are carefully investigated. It is found that the core structures (including APB, CSF and SISF faults) exhibit different degrees of dependence on the direction and magnitude of the applied stresses. The evolution of local displacements exhibits a specific sequence of “full dislocation → SISF → APB”, which can be modulated by the variation of stresses. Graphical abstract Download : Download high-res image (163KB) Download : Download full-size image

Show more

Analyzing the impact of substitution on the temperature-sensitive release of doxorubicin in an imine-based covalent organic framework using molecular dynamics

Highlights • This study analyses the stability of COFs at 37 °C and 42 °C and their impact on the binding and interaction energies with DOX. • vdW interactions contribute most to DOX-COF binding energy, while ES and HB interactions were negligible. • The COFs with small polar or non-polar substitutions were unsuitable for DOX release. • COF-HQ with bulky substitution having the highest binding energy, and placement of DOX between the COF substitution layers impeded the temperature effect to release DOX. • DOX release was observed only in COF-OMe at the higher temperature of 42 °C. Nowadays, drug release through temperature control between healthy and cancer cells is also one of the most critical topics in drug delivery. Covalent organic frameworks (COFs) with specific structural units and functional groups can be optimized for efficient smart drug delivery applications. Hence, in the present study, a detailed systematic study on the release of the anticancer drug doxorubicin (DOX) in a temperature-sensitive method from COFs with structural units of 1,3,5-tris(4-aminophenyl)benzene and terephthalaldehyde substituted with hydrogen (COF-H), ethyl (COF-Et), hydroxyl (COF-OH), methoxy (COF-OMe) and 8-hydroxyquinoline (COF-HQ), by molecular dynamics (MD) simulation method at two temperatures of 37 °C and 42 °C was performed. In addition to the stability of COF systems at 37 °C and 42 °C, the results showed that changing the temperature and substitution effectively changes the binding and interaction energies between the DOX and COFs. It was understood that van der Waals (vdW) interactions, in contrast to electrostatic (ES) interactions, have the major contribution to the binding energy ( Δ G bind ° ). Also, hydrogen bonding (HB) can be effective in binding between the DOX and COFs capable of donating and accepting HBs, such as COF-HQ and COF-OH. It was seen that COFs with completely polar substitution (COF-OH) or completely non-polar substitution (COF-Et and COF-H) were unsuitable, because the DOX establishes strong interactions with these COFs by being placed on the inner surface of the cavities of the COF backbone. Also, COF with bulky substitution, COF-HQ, has the highest Δ G bind ° = −45.9108, but it was observed, due to the gradual placement of the DOX between the COF substitution layers, increasing the temperature was not able to release the DOX. Finally, DOX release was observed among the five COF systems in COF-OMe at 42 °C ( Δ G bind ° = −21.0080 kcal/mol). But at 37 °C, due to the absorption of the DOX inside COF-OMe cavities ( Δ G bind ° = −30.9486 kcal/mol), DOX release was not observed. Graphical abstract Download : Download high-res image (188KB) Download : Download full-size image

Show more

Some elements of microstructural mechanics

Microstructural mechanics combines the computational methods of structural mechanics and materials sciences. It is dedicated to the mechanics of heterogeneous materials. On the one hand, it can be used to compute industrial components for which the size of the heterogenities is of the order of magnitude of the size of the structure itself or of holes or notches. On the other hand, the computation of representative volume elements of heterogeneous materials enables one to predict the influence of phase morphology and distribution on the linear or non-linear effective properties, having in view microstructure optimization. Such computations provide the local stress–strain fields that can be used to predict damage or crack initiation. This work focuses on the modern tools available for reconstructing realistic three-dimensional microstructures and for computing them, including parallel computing. The choice of the local non-linear constitutive equations and the difficulty of identification of the corresponding parameters remain the weakest link in the methodology. The main example detailed in this work deals with polycrystalline plasticity and illustrates the tremendous heterogeneity of local stress and strain, and the effect of grain boundary or free surfaces. The computations are finally used to calibrate a simplified homogenization polycrystal model.

Cited: 155
Show more

Mechanical properties of silicene

Highlights • Silicene is a two-dimensional allotrope of silicon, analogous to graphene. • We use full atomistic molecular dynamics (MD) to characterize silicene. • We implement uniaxial tensile tests to determine stiffness and failure states. • We use an energy minimization approach to calculate the monolayer bending rigidity. • Understanding of mechanical performance is necessary for future application. The potential of atomistically two-dimensional (2D) materials has created a new paradigm of materials science. Among the various 2D crystalline structures is silicene – a monolayer allotrope of silicon – similar to the structure of graphene. While this material has been previous investigated for potential in electrical applications, successful implementation in such nanodevices requires full understanding of its mechanical behavior. Here, using full atomistic first-principles-based ReaxFF molecular dynamics (MD) we quantify the elastic stiffness (50.44 N/m for zigzag direction, 62.31 N/m for armchair direction) and limit states (ultimate strength on the order of 5.85 N/m, ultimate strain on the order of 18%) of monolayer silicene. A weak directional dependence is observed. Moreover, we quantify the effective bending stiffness of silicene (38.63 eV per unit width), indicating that its corrugated-like structure increases the bending rigidity compared to the similar system of graphene.

Cited: 114
Show more

Application of highly stretchable and conductive two-dimensional 1T VS2 and VSe2 as anode materials for Li-, Na- and Ca-ion storage

The atomic structure of single layer transition metal-dichalcogenides (TMDs) like two-dimensional Vanadium dichalcogenides (VS2 and VSe2) with octahedral (1T) phase has attracted remarkable interest due to its excellent physical and chemical properties. In this work, we conduct density functional theory (DFT) simulations to study the applicability of 1T VS2 and VSe2 as anode materials for Al-, Mg-, Ca-, Na- or Li-ion batteries. To explore the application of 1T VS2 and VSe2 in rechargeable batteries, charge transfer efficiency, adsorption energy, open circuit voltage profile, stability, electronic conductivity and diffusion energy barrier were evaluated. The results revealed that, both 1T VS2 and VSe2 show highly promising performances as anode material for Li-, Ca- or Na-ions batteries, whereas the Al and Mg atoms are not favourable for the adsorption. Consequently, our first-principles analysis reveals that 1T VS2 and VSe2 have considerable charge capacities of 466 mAh/g and 257 mAh/g for Li-, Ca- or Na-ion storages, which is very promising for stretchable rechargeable batteries. Graphical abstract Download : Download high-res image (148KB) Download : Download full-size image

Cited: 100
Show more

Density functional theory study of dissociative adsorption of O2 on Pd-skin Pd3Cu(1 1 1) surface

The dissociative adsorption of O2 demonstrates a significant correlation with the catalytic efficiency of oxygen reduction catalysts. We have performed density-functional theory calculations to investigate the dissociative adsorption of O2 on the Pd-skin Pd3Cu(1 1 1) surface. The calculated results show that the adsorption configuration denoted as “t-f(h)-b” is energetically favourable on the Pd-skin Pd3Cu(1 1 1) surface. In the context of O2 dissociation, two thermodynamically favourable dissociation pathways have been identified. The first pathway proceeds from the initial state denoted as “t-f-b” to yield two oxygen atoms occupying hcp sites. The second pathway, starting from “t-h-b,” leads to the formation of two oxygen atoms positioned at fcc sites. Furthermore, our analysis demonstrates a decrease in the stability of O2 adsorption and a slight increase in the energy barrier for the dissociation of adsorbed O2 compared to the corresponding process on the Pd(1 1 1) surface. This theoretical investigation offers valuable insights that can inform and guide the practical application of Pd-Cu alloy materials as highly effective catalysts for oxygen reduction reaction. Graphical abstract Download : Download high-res image (224KB) Download : Download full-size image

Download: 0
Show more

Theoretical study of synergistic effect of P and Mg on the cohesive properties of Ni3Al grain boundaries

Highlights • P tends to stay at the interstitial sites while Mg will substitute the host atoms at the Ni-rich Σ5 (2 1 0) Ni3Al GBs. • Synergistic segregation of Mg can improve the detrimental effect of P in the mixed hole on the cohesion properties of the Ni-rich GBs. • The site occupation of Mg can be reversed from the Ni site to the Al site by synergistic alloying of P at the stoichiometric Σ5 (2 1 0) Ni3Al GBs. • GB strengthening of alloying elements can be attributed to the strong P/Mg-Ni interactions across the GBs. The addition of specific alloying elements can effectively control the microstructure of alloys, so as to improve the cohesive properties of the GBs. In this work, the first-principles plane-wave pseudopotential method is used to investigate the segregation behavior of P and Mg doping at the Ni3Al GBs and reveal the physical mechanism. Different 100%Ni Σ5 (2 1 0) [0 1 0] GB systems with and without doping elements are relaxed and larger volume expansions are obtained. The calculated segregation energies show that P or Mg atoms tend to segregate to the GBs relative to the bulk. P atoms tend to stay at the interstitial sites surrounded by 8 Ni atoms in the pure Ni holes of the GBs while Mg atoms tend to substitute Ni atoms. The segregation of P or Mg to the GBs leads to an increase of the Griffith work at the GBs, indicating that the segregation can improve the bonding properties of the GBs. Especially, the synergistic segregation of Mg can improve the detrimental effect of P in the mixed hole on the cohesive properties of the GBs. It is also found that the site occupation of Mg can be reversed from the Ni site to the Al site by the synergistic alloying of P at the 50%Ni Σ5 GBs. P and Mg tend to bond with the host atom Ni regardless of GB structure. The investigation of electronic structure shows that GB strengthening of alloying elements is attributed to the increasing P/Mg-Ni interactions across the GBs. Graphical abstract Download : Download high-res image (80KB) Download : Download full-size image

Download: 0
Show more

Decoupling the effects of geometry and nature of strain in LaMnO 3 : Interplay of dynamic correlations and uniaxial strain driving magnetic phase transitions

Highlights • Uniaxial strain is key to tuning of material properties, including magnetic phases. • Decoupling effect of type of strain from geometrical effects by forming square lattice. • Compressive strain leads to FM insulator by reduction of Jahn–Teller distortion. • Correlation plays strong role; DFT gives metal, DMFT gives insulator. • Tensile strain give AFM insulator; Flavor of strain is more important than geometry. Recent years have seen tremendous progress in experimental techniques to create uniaxial strain. Motivated by these advances we investigate the effect of uniaxial strain on LaMnO 3 employing ab-initio dynamical mean-field theory, and put it in contrast to biaxial strain that occurs in epitaxial systems. Projecting on the low-energy subspace of Mn 3 d states, and solving multi-impurity problems, our approach emphasizes on local dynamic correlations at Mn sites. At ambient pressures, LaMnO 3 crystallizes in an orthorhombic unit cell, with in-plane lattice constants a < b , and shows an A-type antiferromagnetic ground state. If we apply uniaxial compressive strain such that the in-plane lattice becomes square with lattice constant a , we find a ferromagnetic insulating state. This is in sharp contrast to DFT results using various functionals like PBE, PBE+ U , and hybrid functionals like HSE, which all predict a half-metallic ferromagnetic behavior. Interestingly, applying uniaxial tensile strain, such that the in-plane lattice becomes square with the longer lattice constant b , an antiferromagnetic insulating state is observed. We trace back these results to the reduction in Jahn–Teller distortion in the case of compressive strain, favoring a ferromagnetic state. This reduction is absent in the tensile case, and the antiferromagnetic state therefore survives. Our study shows that it is the flavor of the strain (compressive or tensile) which is decisive for the magnitude of Jahn–Teller distortions and, hence, the magnetic state. Graphical abstract Download : Download high-res image (226KB) Download : Download full-size image

Download: 0