Superplastic dual-phase nanostructure Mg alloy: A molecular dynamics study AITranslate

Northwestern Polytechnical University; Northwestern Polytechnical University; Xi’an Shiyou University; Xi’an Shiyou University; Northwestern Polytechnical University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • The introduction of amorphous phase and ACI can improve the plasticity of Mg alloy. • Two different deformation mechanisms occur depending on d and t. • Reducing d and increasing t is consistent for improving the plastic effect. • The optimal matching relationship between d and t is given. • Some qualitative and quantitative analysis is presented. The introduction of amorphous phase and amorphous-crystalline interfaces is a new approach for enhancing mechanical performance of the Mg-based composite materials. In this work, we use molecular dynamics simulation method to explore the effect of amorphous phase size on the mechanical behavior of dual-phase nanostructure Mg alloy under tensile loading. The results show that two different deformation mechanisms of the dual-phase nanostructure Mg alloy occur depending on crystalline phase size (d) and amorphous thickness (t). There is a critical amorphous thickness (tc) for each sample to achieve nearly perfect plasticity, regardless of d. When t < tc, the plasticity of dual-phase nanostructure Mg alloy is provided by amorphous and crystalline phase. However, the plasticity is provided only by amorphous phase, the crystalline phase hardly participates in plastic deformation when t > tc. The results also indicate that reducing d and increasing t is consistent for improving the plastic effect of the dual-phase nanostructure Mg alloy. The optimal matching relationship between d and t is given. Moreover, some qualitative and quantitative analysis about the plastic deformation behavior of dual-phase nanostructure Mg alloy are also presented. Graphical abstract Download : Download high-res image (137KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2019.01.027

Chinese Library Classification Number:

Citation Information:

Highlights • The introduction of amorphous phase and ACI can improve the plasticity of Mg alloy. • Two different deformation mechanisms occur depending on d and t. • Reducing d and increasing t is consistent for improving the plastic effect. • The optimal matching relationship between d and t is given. • Some qualitative and quantitative analysis is presented. The introduction of amorphous phase and amorphous-crystalline interfaces is a new approach for enhancing mechanical performance of the Mg-based composite materials. In this work, we use molecular dynamics simulation method to explore the effect of amorphous phase size on the mechanical behavior of dual-phase nanostructure Mg alloy under tensile loading. The results show that two different deformation mechanisms of the dual-phase nanostructure Mg alloy occur depending on crystalline phase size (d) and amorphous thickness (t). There is a critical amorphous thickness (tc) for each sample to achieve nearly perfect plasticity, regardless of d. When t < tc, the plasticity of dual-phase nanostructure Mg alloy is provided by amorphous and crystalline phase. However, the plasticity is provided only by amorphous phase, the crystalline phase hardly participates in plastic deformation when t > tc. The results also indicate that reducing d and increasing t is consistent for improving the plastic effect of the dual-phase nanostructure Mg alloy. The optimal matching relationship between d and t is given. Moreover, some qualitative and quantitative analysis about the plastic deformation behavior of dual-phase nanostructure Mg alloy are also presented. Graphical abstract Download : Download high-res image (137KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] H.Y. Song, X.D. Zuo, M.R. An, et al. Computational Materials Science, 2019(160). DOI:10.1016/j.commatsci.2019.01.027.
MLA [1] H.Y. Song, et al., Computational Materials Science, no. 160, 2019, https://doi.org/10.1016/j.commatsci.2019.01.027.
APA [1] H.Y. Song, X.D. Zuo, M.R. An, M.X. Xiao, & Y.L. Li. (2019). Computational Materials Science(160). https://doi.org/10.1016/j.commatsci.2019.01.027
IEEE [1] H.Y. Song, X.D. Zuo, M.R. An, M.X. Xiao, and Y.L. Li, Computational Materials Science, no. 160, 2019, doi: 10.1016/j.commatsci.2019.01.027.