Technological Study on Rare Earth Recovery from Rare Earth Sulfate Solution AITranslate

College of Chemistry and Chemical Engineering, Hefei University of Technology;College of Chemistry and Chemical Engineering, Hefei University of Technology;College of Chemistry and Chemical Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study was made on the process for recovery of La and Ce rare earth metal elements from rare earth sulfate solution with sodium sulfate double salt method.The effects were investigated of reaction time,reaction temperature,sodium sulfate dosage and solution pH on rare earth recovery.The optimized technological conditions were obtained through single-factor condition experiments and orthogonal experiments as follows:reaction time of 120 s,reaction temperature of 65 ℃,sodium sulfate-rare earth mass ratio of 5.2∶1,and rare earth sulfate solution pH value of 2.0.Under the optimized conditions,the overall recovery of rare earth is more than 95%.The rare earth-sodium sulfate double salt is analyzed by XRD,and the result shows that high-purity lanthanide-sodium sulfate double salt was obtained.

KeyWords AITranslate

spent rare earth polishing powder rare earth sulfate solution rare earth-sodium sulfate double salt lanthanum recovery cerium recovery

1窦宁.我国稀土抛光粉产业现状浅析(下)[J].稀土信息,2011,17(12):18-20. 被引量:3

2窦宁.我国稀土抛光粉产业现状浅析(上)[J].稀土信息,2011,17(11):20-22. 被引量:5

3林河成.我国稀土资源储量在逐年下降[J].稀土信息,2006,12(6):11-12. 被引量:3

4程建忠,车丽萍.中国稀土资源开采现状及发展趋势[J].稀土,2010,31(2):65-69. 被引量:237

5Chong S,Holmstrom D,Li Q R,et al.Preparation and evaluation of a Ce (Ⅳ)-La (Ⅲ)binary hydroxide adsorbent as recovery of waste ceria powder from glass polishing process for effective arsenic removal. Vatten . 2009

6Nan, Junmin,Han, Dongmei,Yang, Minjie,Cui, Ming.Dismantling, recovery, and reuse of spent nickel-metal hydride batteries. Journal of the Electrochemical Society . 2006

7崔凌霄,杨国胜,谢兵,高玮,窦宁.中国稀土抛光粉行业现状与发展[J].稀土信息,2013,19(5):17-20. 被引量:13

8许涛,于亚辉,吕保义,高晓玲,闫晓杰.稀土抛光粉固体废粉资源特性研究[J].中国资源综合利用,2010,28(5):22-25. 被引量:9

9王秀艳,刘杰民,杜健.浓硫酸低温分解废弃稀土抛光粉工艺研究[J].环境工程学报,2011,5(9):2129-2132. 被引量:8

10李学舜.稀土抛光粉的生产及应用[J].中国稀土学报,2002,20(5):392-397. 被引量:48

1左泽军,李正,吕灵灵,高明军,刘晨光.从FCC烟气脱硫污泥中提取稀土试验研究[J].湿法冶金,2016,35(5):436-439. 被引量:2

1卢国俭.用还原—酸浸—沉淀工艺从废FCC催化剂中回收稀土[J].湿法冶金,2018,37(5):398-401. 被引量:4

2佟志芳,温皓,胡晓飞.稀土电解熔盐渣焙烧产物酸浸提取稀土、锂和氟[J].有色金属科学与工程,2022,13(4):141-147.

1乔军,郝先库,张存瑞,姚亦淳.稀土硫酸钠复盐的碳酸盐转化的研究[J].稀土,1996,17(3):57-59. 被引量:4

2杨启山,马长顺,郝福,吴峰.硫酸钠复盐法分离Ce(Ⅳ)和RE(Ⅲ)过程中影响分离效果的因素的研究[J].稀土,1996,17(6):66-69. 被引量:3

3非皂化混合萃取剂萃取分离稀土新工艺研究通过鉴定[J].现代材料动态,2006(8):23-23.

4徐春涛,李平辉,李志锐,林跃华.废弃稀土抛光粉再生利用的研究[J].稀土,2017,38(2):74-79. 被引量:3

5程步升.钆和镧系元素在冶金中的应用(续)[J].稀土进展,1989(2):20-21.

6邓佐国,徐廷华,林秀梅,童长仁,吴小军.由还原渣提取高纯氧化铥和氧化镥新工艺研究[J].江西有色金属,1996,10(2):30-34. 被引量:1

7陈冬英,欧阳红,卢能迪.真空钙热还原炉渣的综合利用研究[J].江西有色金属,2004,18(3):27-30. 被引量:9

8吴巍,张洪林.废镍氢电池中镍、钴和稀土金属回收工艺研究[J].稀有金属,2010,34(1):79-84. 被引量:20

9魏琦峰,曹佐英,张启修.硫酸介质中阴离子交换膜电解氧化铈(Ⅲ)的研究[J].稀土,2004,25(1):28-31. 被引量:1

10唐朝波,唐谟堂,姚维义,杨声海,何静,彭及.脆硫铅锑矿精矿的还原造锍熔炼[J].中南工业大学学报,2003,34(5):502-505. 被引量:13

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

Study was made on the process for recovery of La and Ce rare earth metal elements from rare earth sulfate solution with sodium sulfate double salt method.The effects were investigated of reaction time,reaction temperature,sodium sulfate dosage and solution pH on rare earth recovery.The optimized technological conditions were obtained through single-factor condition experiments and orthogonal experiments as follows:reaction time of 120 s,reaction temperature of 65 ℃,sodium sulfate-rare earth mass ratio of 5.2∶1,and rare earth sulfate solution pH value of 2.0.Under the optimized conditions,the overall recovery of rare earth is more than 95%.The rare earth-sodium sulfate double salt is analyzed by XRD,and the result shows that high-purity lanthanide-sodium sulfate double salt was obtained.

quote

GB/T 7714-2015 [1] LUO Lei, TANG Hua-wei, YANG Bao-jun. Technological Study on Rare Earth Recovery from Rare Earth Sulfate Solution[J]. Rare Metals and Cemented Carbides, 2015(6): 12-15.
MLA [1] LUO Lei, et al., "Technological Study on Rare Earth Recovery from Rare Earth Sulfate Solution." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 12-15.
APA [1] LUO Lei, TANG Hua-wei, & YANG Bao-jun. (2015). Technological Study on Rare Earth Recovery from Rare Earth Sulfate Solution. Rare Metals and Cemented Carbides(6), 12-15.
IEEE [1] LUO Lei, TANG Hua-wei, and YANG Bao-jun, "Technological Study on Rare Earth Recovery from Rare Earth Sulfate Solution," Rare Metals and Cemented Carbides, no. 6, pp. 12-15, 2015. keywords: {spent rare earth polishing powder;rare earth sulfate solution;rare earth-sodium sulfate double salt;lanthanum recovery;cerium recovery}