Experimental Study on Bioleaching of Low-grade Molybdenum Tailings AITranslate

School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing);School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing);School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing);School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing);School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing);School of Chemistry and Environmental Engineering, China University of Mining and Technology (Beijing)
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Experimental study was carried out on bioleaching of very low-grade molybdenum tailings with acidithiobacillus ferrooxidans and moderately thermophilic sulfobacillus sibiricu,respectively.The influences were investigated of the presence and type of bacteria on molybdenum tailing leaching.Molybdenum concentration in the leaching solution was measured by ICP,and its redox potential was determined by pH meter.The leaching residue was characterized by XRD and SEM.The results show that both the two bacteria bioleaching processes are effective for very low-grade molybdenum tailings of 5%slurry concentration.The presence of bacteria is beneficial to leaching of molybdenum tailings.Sulfobacillus sibiricu has better leaching results of molybdenum tailings,and its molybdenum leaching rate is 18%after 23 dleaching while acidithiobacillus ferrooxidans has only 8% molybdenum leaching rate.

KeyWords AITranslate

molybdenum tailing bioleaching acidithiobacillus ferrooxidans sulfobacillus sibiricu

1张刚,赵中伟,霍广生,曹才放,李江涛,陈爱良,李洪桂.镍钼矿处理工艺的研究现状[J].稀有金属与硬质合金,2008,36(4):37-41. 被引量:31

2Kummer W,Gutknecht W,Olson J G,et al.Recovery of molybdenum from molybdenum bearing sulfide materials by bioleaching in the presence of iron. US Pat:8268037 . 2012

3B. Nasernejad,T. Kaghazchi,M. Edrisi,M. Sohrabi.??Bioleaching of molybdenum from low-grade copper ore(J)Process Biochemistry . 2000 (5)

4Wolfgang Sand,Tilman Gehrke,Peter-Georg Jozsa,Axel Schippers.??(Bio)chemistry of bacterial leaching—direct vs. indirect bioleaching(J)Hydrometallurgy . 2001 (2)

5F.K. Crundwell.??How do bacteria interact with minerals?(J)Hydrometallurgy . 2003 (1)

6张广积,方兆珩.氧化亚铁硫杆菌浸出镍黄铁矿机理的初步分析[J].过程工程学报,2001,1(4):374-377. 被引量:14

7黄海芳.钼精矿焙烧的污染浪费及对策[J].铁合金,2002,33(1):12-16. 被引量:11

8吉兆宁,余斌,刘坚,陈何,薛云新,马公望,赵新峰.金堆城低品位钼矿石可浸性研究[J].有色金属:矿山部分,2002,54(5):15-18. 被引量:11

9Loren C. Bryner,Jay V. Beck,Delmar B. Davis,Dean G. Wilson.Microorganisms in Leaching Sulfide Minerals. Industrial and Engineering Chemistry . 1954

10张鸿彪,牟文宁,宋佩,卢媛嫄,孙雷雷.钼矿冶炼新工艺发展概论[J].材料导报:纳米与新材料专辑,2013,27(2):87-90. 被引量:5

1崔孝炜,狄燕清.磨细钼尾矿粒度分布的分形研究[J].矿业研究与开发,2016,36(11):32-35. 被引量:4

2李建涛,庄肃凯,南宁,李凯斌,朱明明.浸矿菌的选育及对低品位钼矿的浸出试验研究[J].金属矿山,2018,47(5):103-107. 被引量:1

1战佳宇,杨飞华,耿春雷,李万民,杨闯.钼尾矿机械活化处理及对硅酸钙板性能的影响[J].混凝土与水泥制品,2017(6):56-59. 被引量:4

2刘璇,李如燕,崔孝炜,梁卓卓,冷欣燕.机械力活化对钼尾矿胶凝性能的影响研究[J].矿产保护与利用,2018,38(4):108-111. 被引量:4

3崔孝炜,冷欣燕,南宁,刘璇,张梦涛.机械力活化对钢渣粒度分布和胶凝性能的影响[J].硅酸盐通报,2018,37(12):3821-3826. 被引量:9

4董玉凤,佟琳琳,杨洪英,赵前飞,甘露.基于16SrDNA测序技术揭示腐殖酸对浸矿微生物菌群结构变化的影响[J].中国资源综合利用,2021,39(8):4-9.

5赵奎,朱梓豪,曾鹏,刘周超,王万银,王金鉴,宋林.三轴压缩条件下尾砂力学行为与破碎机理[J].矿业研究与开发,2021,41(8):114-119.

1廖德华,李晓波.从浮选尾矿中综合回收钼和白钨[J].资源再生,2008(5):60-61. 被引量:1

2赵世勇.西西伯利亚钢铁股份公司高炉炼铁工艺的改进[J].冶金译丛,1995(6):25-27.

3Ю Н Носов,A A Mихалев,A B Mаханъков,Ю В Школа,马芳.西西伯利亚钢铁公司转炉厂350t LF炉的应用[J].世界钢铁,2009(3):16-17.

4Т.Р.Гапиуплин,Ю.Н.Носов,韩丕兰.转炉出钢时钢水脱硫特点[J].本钢技术,2008(5):40-43.

5В.А.多林斯基,Л.Д.尼基京,А.Ф.阿夫齐诺夫,С.Ф.布加耶夫,石春华(校).西西伯利亚钢铁公司提高高炉冶炼效率[J].重钢技术,2006,49(2):5-8.

6Т.Р.加利乌林,Ю.Н.诺索夫,А.А.米哈列夫,Ю.В.什科拉,А.В.马汉科夫,先越蓉(译),廖明(校).转炉出钢时钢水脱硫的特点[J].重钢技术,2009,52(4):17-19.

7欧乐明,何荣权,冯其明.无菌体系下黄铁矿浸出及热力学分析[J].有色金属,2007,59(4):87-90. 被引量:5

8多流槽BRCU无料钟炉顶设备开始在高炉上推广应用[J].涟钢科技与管理,2005(4):61-61.

9杜娟,李媛媛,张广积,杨超.铜砷滤饼废渣的生物浸出[J].过程工程学报,2014,14(3):415-420. 被引量:9

10Ю.А.Эслстухин,武忠荣(译).高炉大量喷煤对焦炭质量的要求[J].现代冶金(内蒙古),2010(2):16-19.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

Experimental study was carried out on bioleaching of very low-grade molybdenum tailings with acidithiobacillus ferrooxidans and moderately thermophilic sulfobacillus sibiricu,respectively.The influences were investigated of the presence and type of bacteria on molybdenum tailing leaching.Molybdenum concentration in the leaching solution was measured by ICP,and its redox potential was determined by pH meter.The leaching residue was characterized by XRD and SEM.The results show that both the two bacteria bioleaching processes are effective for very low-grade molybdenum tailings of 5%slurry concentration.The presence of bacteria is beneficial to leaching of molybdenum tailings.Sulfobacillus sibiricu has better leaching results of molybdenum tailings,and its molybdenum leaching rate is 18%after 23 dleaching while acidithiobacillus ferrooxidans has only 8% molybdenum leaching rate.

quote

GB/T 7714-2015 [1] ZHAO Huan, ZHANG Guang-ji, YANG Qiao-wen, et al. Experimental Study on Bioleaching of Low-grade Molybdenum Tailings[J]. Rare Metals and Cemented Carbides, 2015(6): 7-11.
MLA [1] ZHAO Huan, et al., "Experimental Study on Bioleaching of Low-grade Molybdenum Tailings." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 7-11.
APA [1] ZHAO Huan, ZHANG Guang-ji, YANG Qiao-wen, LI Yuan-yuan, WU Tao, & YANG Chao. (2015). Experimental Study on Bioleaching of Low-grade Molybdenum Tailings. Rare Metals and Cemented Carbides(6), 7-11.
IEEE [1] ZHAO Huan, ZHANG Guang-ji, YANG Qiao-wen, LI Yuan-yuan, WU Tao, and YANG Chao, "Experimental Study on Bioleaching of Low-grade Molybdenum Tailings," Rare Metals and Cemented Carbides, no. 6, pp. 7-11, 2015. keywords: {molybdenum tailing;bioleaching;acidithiobacillus ferrooxidans;sulfobacillus sibiricu}