Development of High-quality Mg-Zr Intermediate Alloy AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

K2ZrF6 is reduced with liquid Mg and KCl and NaCl as flux. High-quality Mg-Zr intermediate alloy is produced through control of furnace charge proportion, reduction temperature and time,and by forward and backward mechanical agitation, successfully solving the problem of separation between the slag phase and Mg-Zr intermediate alloy,of somewhat higher impurity in the alloy and alloy constituent segregation from the traditional production process.

KeyWords AITranslate

Mg- Zr intermediate alloy furnace charge proportion mechanical agitation reduction temperature reduction time

1张静,潘复生,郭正,丁培道,汪凌云.含锆镁合金系中的合金相[J].兵器材料科学与工程,2002,25(6):50-56. 被引量:38

2勒斯特曼 B,等.锆[M].北京:中国工业出版社,1965.11.

1李中华,张卫平,刘甲祥.稀土材料在现代军事技术上的应用及发展趋势[J].湖南冶金,2006,34(4):43-48. 被引量:12

1陈珏.我国稀土产业发展现状及其对策建议[J].湖南有色金属,2007,23(3):77-80. 被引量:9

2张卫平,杨庆山,陈建军.高纯稀土金属制备方法与发展趋势[J].金属材料与冶金工程,2007,35(3):61-64. 被引量:8

3钟学明.稀土萃取分离氨皂化废水的处理与消除[J].江西化工,2008,24(1):5-7. 被引量:8

4郭茂林,贾志琦,刘翠玲,董建忠,张纯.中国稀土产业现状及战略安全的几点建议[J].科技情报开发与经济,2009,19(32):95-98. 被引量:18

5徐向超,丁志刚.全球通货膨胀下的世界稀土博弈[J].科技情报开发与经济,2011,21(18):168-169.

6成维,李宗安,陈德宏,庞思明,王志强,王祥生.锂热还原-真空蒸馏联合法制备高纯金属镧工艺研究[J].稀有金属,2011,35(5):781-785. 被引量:8

7吴玉锋,贾平平,王维,王宝磊,章启军.从废弃CRT荧光粉中熔浸稀土元素的研究[J].中国稀土学报,2013,31(6):723-728. 被引量:11

8张兆雪,王瑞祥,熊家春,温功玉,廖根,谢博毅.碱熔预处理对废旧稀土荧光粉中稀土提取的影响[J].有色金属科学与工程,2016,7(6):129-135. 被引量:6

9王晖,王毓明,解文丽.话战略金砖之稀土[J].广东化工,2022,49(14):69-71.

10张生辉,王振涛,李永胜,莫宣学,董庆吉,陈丛林,耿林,王利,张海啟,谭秀民,薛迎喜,周尚国,田郁溟,姚超美,焦森,陈正国,陈军元,王寿成,张浩钰,付水兴,王春连,王永.中国关键矿产清单、应用与全球格局[J].矿产保护与利用,2022,42(5):138-168. 被引量:4

1陈建军,杨庆山.镁热还原K_2ZrF_6制备镁锆中间合金[J].金属材料与冶金工程,2007,35(5):15-17.

2赵鸿金,孔军,陆晟,李涛涛.电磁搅拌方式对Al-Mn合金显微组织的影响[J].铸造技术,2014,35(11):2646-2650. 被引量:1

3张保丰,蔡海勇,李庆奎.利用海绵锆制备低成本ZK60A镁合金的研究[J].铸造,2013,62(1):17-20. 被引量:3

4王庆相,范志康,杨怡.制备方法对W-10%Ti合金组织性能的影响[J].材料研究学报,2009,23(3):293-299. 被引量:6

5操齐高,马光,郑晶.高温合金杂质控制水平国内外对比分析研究[J].科技创新导报,2015,12(30):3-4. 被引量:1

6张黔,李朝志.稀土硼砂型渗硼剂中硅、铝还原剂对渗层组织的影响[J].金属热处理,2000(12):9-10. 被引量:1

7陈淑群,容庆新.用锌柱还原——直接滴定法测定铕[J].稀土,1990,11(6):33-35. 被引量:1

8范景莲,刘涛,田家敏,成会朝,黄伯云.喷雾干燥-氢还原制备W-50Cu纳米复合粉末过程中的相转变[J].稀有金属材料与工程,2008,37(11):1919-1923. 被引量:15

9罗胜联,廖见培,黄杉生.NO_3^-和NO_2^-在有机锡修饰电极上的电化学研究[J].湖南大学学报:自然科学版,2003,30(2):28-31. 被引量:1

10王红霖,苑化军.通泽重工 时代先锋[J].现代工业经济和信息化,2012(1):36-39.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.22[金属学及工艺—金属材料]

Citation Information:

K2ZrF6 is reduced with liquid Mg and KCl and NaCl as flux. High-quality Mg-Zr intermediate alloy is produced through control of furnace charge proportion, reduction temperature and time,and by forward and backward mechanical agitation, successfully solving the problem of separation between the slag phase and Mg-Zr intermediate alloy,of somewhat higher impurity in the alloy and alloy constituent segregation from the traditional production process.

quote

GB/T 7714-2015 [1] LIU Jia-xiang, YANG Qing-shan, LIU Shu-ping, et al. Development of High-quality Mg-Zr Intermediate Alloy[J]. Rare Metals and Cemented Carbides, 2006(1): 30-32.
MLA [1] LIU Jia-xiang, et al., "Development of High-quality Mg-Zr Intermediate Alloy." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 30-32.
APA [1] LIU Jia-xiang, YANG Qing-shan, LIU Shu-ping, CHEN Wei-ping, & HE Bi-ning. (2006). Development of High-quality Mg-Zr Intermediate Alloy. Rare Metals and Cemented Carbides(1), 30-32.
IEEE [1] LIU Jia-xiang, YANG Qing-shan, LIU Shu-ping, CHEN Wei-ping, and HE Bi-ning, "Development of High-quality Mg-Zr Intermediate Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 30-32, 2006. keywords: {Mg- Zr intermediate alloy;furnace charge proportion;mechanical agitation;reduction temperature;reduction time}